Ni-CeO2纳米镀层在酸性NaCl溶液中的腐蚀行为及电化学阻抗谱特征 |
周小卫,沈以赴 |
南京航空航天大学材料科学与技术学院, 南京 210016 |
|
CORROSION BEHAVIOR AND EIS STUDY OF NANOCRYSTALLINE Ni-CeO2 COATINGS IN AN ACID NaCl SOLUTION |
ZHOU Xiaowei,SHEN Yifu |
College of Materials Science and Technology, Nanjing University of Aeronautics and Astronautics, Nanjing 210016 |
引用本文:
周小卫,沈以赴. Ni-CeO2纳米镀层在酸性NaCl溶液中的腐蚀行为及电化学阻抗谱特征[J]. 金属学报, 2013, 49(9): 1121-1130.
.
CORROSION BEHAVIOR AND EIS STUDY OF NANOCRYSTALLINE Ni-CeO2 COATINGS IN AN ACID NaCl SOLUTION[J]. Acta Metall Sin, 2013, 49(9): 1121-1130.
[1] Dutta R S, Tewari R, De P K. Corros Sci, 2007; 49: 303
[2] Jin H M, Chen R F, Zhang J F, Felix A C. Mater Mech Eng, 2004; 28: 7
(靳惠明, 陈荣发, 张剑峰, Felix A C. 机械工程材料, 2004; 28: 7)
[3] Qu N S, Zhu D, Chan K C. Scr Mater, 2006; 54: 1421
[4] Sen R, Das S, Das K. Mater Res Bull, 2012; 47: 478
[5] Xue Y J, Liu H B, Lan M M, Ku X C, Li J S. Chin J Nonferrous Met, 2010; 20: 1599
(薛玉君, 刘红彬, 兰明明, 库祥臣, 李济顺. 中国有色金属学报, 2010; 20: 1599)
[6] Sen R, Das S, Das K. Surf Coat Technol, 2011; 205: 3847
[7] Mihalache V, Pasuk I. Acta Mater, 2011; 59: 4875
[8] Arsenault R J. Scr Metall Mater, 1991; 25: 2617
[9] Aruna S T, William Grips V K, Ezhil Selvi V, Rajam K S. J Appl Electrochem, 2007; 37: 991
[10] Dias S A S, Lamak S V, Nogueira C A , Diamantinoa T C, Ferreira M G S.Corros Sci, 2012; 62: 153
[11] Zhou X W, Shen Y F, Gu D D. Acta Metall Sin, 2012; 48: 957
(周小卫, 沈以赴, 顾冬冬. 金属学报, 2012; 48: 957)
[12] Zhou X W, Shen Y F, Zheng Y Y, Jin H M. J Rare Earths, 2011; 29: 883
[13] Yu X W, Cao C N, Lin H C. Chin Rare Earths, 2000; 18: 243
(于兴文, 曹楚南, 林海潮. 稀土学报, 2000; 18: 243)
[14] Simon J, Elizabeth A K, William G F, Matthew J O. Corros Sci, 2012; 60: 290
[15] Stern M, Geary A L. J Electrochem Soc, 1957; 104: 56.
[16] Yong X Y, Liu J J, Lin Y Z. Acta Metall Sin, 2005; 41: 871
(雍兴跃, 刘景军, 林玉珍. 金属学报, 2005; 41: 871)
[17] Aruna S T, Bindu C N, Ezhil Selvi V, William Grips V K, Rajam K S.Surf Coat Technol, 2006; 200: 6871
[18] Conde A, Damborenea J. Corros Sci, 2000; 42: 1363
[19] Gray J J, Orme C A. Electrochimica Acta, 2007; 52: 2370
[20] Wang B, Liu Q Y, Mao X P, Weng Y, Wang X D, Jia S J, Dong H. Acta Metall Sin, 2008; 44: 863
(汪兵, 刘清友, 毛新平, 翁宇, 王向东, 贾书君, 董瀚. 金属学报, 2008; 44: 863)
[21] Czerwinski F, Szpunar J A. Thin Solid Films, 1996; 289: 213
[22] Czerwinski F, Smeltzer W W. Oxid Met, 1993; 40: 503
[23] Hinton B R W, Arnott D R, Ryan N E. Mater Form, 1986; 9: 162
[24] Zamanzad-Ghavidel M R, Raeissi K, Saatchi A. Mater Lett, 2009; 63: 1807
[25] Hasannejad H, Shahrabi T, Jafarian M, Sabour Rouhaghdam A. J Alloys Compd,2011; 509: 1924
[26] Muhamed A P, Shibli S M A. Electrochem Commun, 2007; 9: 443
[27] Thanneeru R, Patil S, Deshpande S, Seal S. Acta Mater, 2007; 55: 3457 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|