| 基于原位高能X射线衍射定量分析退火温度对中锰钢加工硬化的影响 |
| 季泽1,高宏伟2,张明赫1,冯运莉1,李时磊2,王沿东2 |
1 华北理工大学 冶金与能源学院 唐山 063210
2 北京科技大学 新金属材料国家重点实验室 北京 100083
|
|
| Quantitative Analysis of the Effect of Annealing Temperature on the Work-hardening Behavior of Medium-Mn Seel Based on in-situ High-energy X-ray Diffraction |