Fe-Mn-Al轻质高强钢组织和力学性能研究* |
杨富强, 宋仁伯( ), 孙挺, 张磊峰, 赵超, 廖宝鑫 |
北京科技大学材料科学与工程学院, 北京 100083 |
|
MICROSTRUCTURE AND MECHANICAL PROPER- TIES OF Fe-Mn-Al LIGHT-WEIGHT HIGH STRENGTH STEEL |
YANG Fuqiang, SONG Renbo( ), SUN Ting, ZHANG Leifeng, ZHAO Chao, LIAO Baoxin |
School of Materials Science and Engineering, University of Science and Technology Beijing, Beijing 100083 |
引用本文:
杨富强, 宋仁伯, 孙挺, 张磊峰, 赵超, 廖宝鑫. Fe-Mn-Al轻质高强钢组织和力学性能研究*[J]. 金属学报, 2014, 50(8): 897-904.
Fuqiang YANG,
Renbo SONG,
Ting SUN,
Leifeng ZHANG,
Chao ZHAO,
Baoxin LIAO.
MICROSTRUCTURE AND MECHANICAL PROPER- TIES OF Fe-Mn-Al LIGHT-WEIGHT HIGH STRENGTH STEEL[J]. Acta Metall Sin, 2014, 50(8): 897-904.
[1] |
Suh D W, Kim N J. Scr Mater, 2013; 68: 337
|
[2] |
Hwang S W, Ji J H, Park K T. Mater Sci Eng, 2011; A528: 7267
|
[3] |
Sahraoui T, Hadji M, Yahi M. Mater Sci Eng, 2009; A523: 271
|
[4] |
Park K, Kim G, Kim S K, Lee S W, Hwang S W, Lee C S. Met Mater Int, 2010; 16: 1
|
[5] |
Saeed-Akbari A, Imlau J, Prahl U, Bleck W. Metall Mater Trans, 2009; 40A: 3076
|
[6] |
Torabinejad V, Zarei-Hanzaki A, Moemeni S, Imandoust A. Mater Des, 2011; 32: 5015
|
[7] |
Frommeyer G, Brux U. Steel Res Int, 2006; 77: 627
|
[8] |
Yoo J D, Park K. Mater Sci Eng, 2008; A496: 417
|
[9] |
Yoo J D, Hwang S W, Park K. Mater Sci Eng, 2009; A508: 234
|
[10] |
Yoo J D, Hwang S W, Park K T. Metall Mater Trans, 2009; 40A: 1520
|
[11] |
Choi K, Seo C, Lee H, Kim S K, Kwak J H. Scr Mater, 2010; 63: 1028
|
[12] |
Kalashnikov I, Shalkevich A, Acselrad O, Peraira L C. J Mater Eng Perform, 2000; 9: 597
|
[13] |
Ma F C, Liu P, Li W, Feng W J, Wang L. Trans Mater Heat Treat, 2010; 31(9): 64
|
[13] |
(马凤仓, 刘 平, 李 伟, 封为骏, 王 利. 材料热处理学报, 2010; 31(9): 64)
|
[14] |
Bao W P, Zhao Y J, Xu L W, Xiong Z P, Ren X P. Heat Treat Met, 2010; 35(4): 33
|
[14] |
(包卫平, 赵艳君, 许立伟, 熊志平, 任学平. 金属热处理, 2010; 35(4): 33)
|
[15] |
Umino R, Liu X, Sutou Y, Wang C, Ohnuma I, Kainuma R. J Phase Equilib Diff, 2006; 27: 54
|
[16] |
Park K, Jin K G, Han S H, Hwang S W, Choi K, Lee S W. Mater Sci Eng, 2010; A527: 3651
|
[17] |
Ding H, Yang P. J Mater Metall, 2010; 9: 265
|
[17] |
(丁 桦, 杨 平. 材料与冶金学报, 2010; 9: 265)
|
[18] |
Gutierrez I, Raabe D. Acta Metar, 2012; 60: 5791
|
[19] |
Dumay A, Chateau J P, Allain S, Migot S, Bouaziz O. Mater Sci Eng A, 2008; 483-484: 184
|
[20] |
Poy N C. PhD Dissertation, University Ghent, 2004
|
[21] |
Talonen J, Hanninen H. Acta Mater, 2007; 55: 6108
|
[22] |
Paul H, Morawiec A, Driver J H, Bouzy E. Int J Plast, 2009; 25: 1588
|
[23] |
Imandoust A, Zarei-Hanzaki A, Abedi H R. Scr Mater, 2012; 67: 995
|
[24] |
Dong H, Sun X. Curr Opin Solid State Mater Sci, 2005; 9: 269
|
[25] |
Hughes D A. Acta Metall Mater, 1993; 41: 1421
|
[26] |
Park K. Scr Mater, 2013; 68: 375
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|