| O, N和Ni含量对0Cr25Ni7Mo4N双相不锈钢热轧塑性的影响* |
陈雨来1, 张泰然1, 王一德2, 李静媛2( ) |
1 北京科技大学冶金工程研究院, 北京 100083 2 北京科技大学材料科学与工程学院, 北京 100083 |
|
| EFFECTS OF O, N AND Ni CONTENTS ON HOT PLASTICITY OF 0Cr25Ni7Mo4N DUPLEX STAINLESS STEEL |
CHEN Yulai1, ZHANG Tairan1, WANG Yide2, LI Jingyuan2( ) |
1 Metallurgical Engineering Research Institute, University of Science and Technology Beijing, Beijing 100083 2 School of Materials Science and Engineering, University of Science and Technology Beijing, Beijing 100083 |
引用本文:
陈雨来, 张泰然, 王一德, 李静媛. O, N和Ni含量对0Cr25Ni7Mo4N双相不锈钢热轧塑性的影响*[J]. 金属学报, 2014, 50(8): 905-912.
Yulai CHEN,
Tairan ZHANG,
Yide WANG,
Jingyuan LI.
EFFECTS OF O, N AND Ni CONTENTS ON HOT PLASTICITY OF 0Cr25Ni7Mo4N DUPLEX STAINLESS STEEL[J]. Acta Metall Sin, 2014, 50(8): 905-912.
| [1] |
Wu J. Duplex Stainless Steel. Beijing: Metallurgy Industry Press, 1999: 1
|
| [1] |
(吴 玖. 双相不锈钢. 北京: 冶金工业出版社, 1999: 1)
|
| [2] |
Fang Y L, Liu Z Y, Zhang W N, Wang G D, Song H M, Jiang L Z. Acta Metall Sin, 2010; 46: 641
|
| [2] |
(方轶琉, 刘振宇, 张维娜, 王国栋, 宋红梅, 江来珠. 金属学报, 2010; 46: 641)
|
| [3] |
Fan G W, Liu J, Han P D, Qiao G J. Mater Sci Eng, 2009; A515: 108
|
| [4] |
Han Y, Zou D N, Chen Z Y, Fan G W, Zhang W. Mater Charact, 2011; 62: 198
|
| [5] |
Chen L, Wang L M, Du X J. Acta Metall Sin, 2010; 46: 52
|
| [5] |
(陈 雷, 王龙妹, 杜晓建. 金属学报, 2010; 46: 52)
|
| [6] |
Iza-Mendia A, Pinol-Juez A, Urcola J J. Metall Mater Trans, 1998; 29A: 2975
|
| [7] |
Alvarez-Armas I, Marinelli M C, Herenu S. Acta Mater, 2006; 54: 5041
|
| [8] |
Jia N, Lin P R, Wang Y D. Acta Mater, 2008; 56: 782
|
| [9] |
Weatherly G C, Hamble P, Borland D. Acta Metall, 1979; 27: 1815
|
| [10] |
Dahmen U, Ferguson P, Westmacott K H. Acta Metall, 1984; 32: 803
|
| [11] |
Qiu D, Zhang W Z. Acta Mater, 2007; 55: 6754
|
| [12] |
Song Z, Zheng W, Feng H. J Iron Steel Res Int, 2013; 20: 83
|
| [13] |
Song Z G, Wu J, Lin X J. J Iron Steel Res Int, 2011; 18: 64
|
| [14] |
Fang Y L, Liu Z Y, Song H M. Mater Sci Eng, 2009; A526: 128
|
| [15] |
Jiang Z L, Wu Y, Chen X Y, Bai F M, Liu X Y, Huang T G. J Mater Eng, 2002; (5): 30
|
| [15] |
(姜忠良, 吴 严, 陈秀云, 白飞明, 刘秀赢, 黄铁光. 材料工程, 2002; (5): 30)
|
| [16] |
Chen P D, Wang J H, Ma Z W. Phys Examination Test, 2012; 30(3): 11
|
| [16] |
(陈培敦, 王俊海, 马正伟. 物理测试, 2012; 30(3): 11)
|
| [17] |
Shen P, Yan H T, Yang Z, Yuan H. Hot Working Technol, 2013; 42(4): 50
|
| [17] |
(申 鹏, 颜海涛, 杨 振, 袁 辉. 热加工工艺, 2013; 42(4): 50)
|
| [18] |
Wu Z Z, Song Z G, Zheng W J, Chen B, Lu J S. Spec Steel, 2006; 27(4): 11
|
| [18] |
(吴忠忠, 宋志刚, 郑文杰, 陈 斌, 陆建生. 特殊钢, 2006; 27(4): 11)
|
| [19] |
Yang Q X, Wu J, Zhao H. Trans Mater Heat Treat, 2006; 26: 124
|
| [19] |
(杨庆祥, 吴 晶, 赵 宏. 材料热处理学报, 2006; 26: 124)
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|