| 稀土Ce对钎具钢中夹杂物的改质机理研究 |
黄宇1, 成国光1( ), 谢有2 |
1 北京科技大学钢铁冶金新技术国家重点实验室 北京 100083 2 中天钢铁集团有限公司 常州 213011 |
|
| Modification Mechanism of Cerium on the Inclusions in Drill Steel |
Yu HUANG1, Guoguang CHENG1( ), You XIE2 |
1 State Key Laboratory of Advanced Metallurgy, University of Science and Technology Beijing, Beijing 100083, China 2 Zenith Steel Group Co., Ltd., Changzhou 213011, China |
引用本文:
黄宇, 成国光, 谢有. 稀土Ce对钎具钢中夹杂物的改质机理研究[J]. 金属学报, 2018, 54(9): 1253-1261.
Yu HUANG,
Guoguang CHENG,
You XIE.
Modification Mechanism of Cerium on the Inclusions in Drill Steel[J]. Acta Metall Sin, 2018, 54(9): 1253-1261.
| [1] | Hu Z G.Research and development of drill steel and drill tools[J]. Rock Drill. Mach. Pneum. Tools, 2011, (4): 6(胡支国. 钎钢钎具产品的研制与开发[J]. 凿岩机械气动工具, 2011, (4): 6) | | [2] | Li B X.Failure analysis and fracture mechanism of whorl drill steel[J]. Rock Drill. Mach. Pneum. Tools, 1999, (2): 55(黎炳雄. 螺纹钎杆的失效分析和断裂机理[J]. 凿岩机械气动工具, 1999, (2): 55) | | [3] | Liang X J.Study on the substitution of domestic materials and manufacturing technology for rock drill[D]. Taiyuan: Taiyuan University of Science & Technology, 2014(梁晓捷. 凿岩钎具国产材料替代及制造工艺的研究[D]. 太原: 太原科技大学, 2014) | | [4] | Zhou F Y, Xu Z H.Failure analysis of the heavy drill rod made in China[J]. Mater. Mech. Eng., 1997, 21(3): 47(周凤云, 徐志宏. 国产重型凿岩钎杆的失效分析[J]. 机械工程材料, 1997, 21(3): 47) | | [5] | Zhu H W, Liu Y Z, Zhou L Y, et al.Failure analysis of 22Si2MnCrNi2MoA drilling rods[J]. J. Univ. Sci. Technol. Beijing, 2013, 35: 613(朱洪武, 刘雅政, 周乐育等. 22Si2MnCrNi2MoA钎杆断裂失效分析[J]. 北京科技大学学报, 2013, 35: 613) | | [6] | Yan Y M, Liu Y Z, Zhou L Y, et al.Influence of heat treatment process on microstructure and properties of 23CrNi3Mo steel[J]. Trans. Mater. Heat Treat., 2014, 35: 110(闫永明, 刘雅政, 周乐育等. 热处理工艺对23CrNi3Mo钎具钢组织及性能的影响[J]. 材料热处理学报, 2014, 35: 110) | | [7] | Hong D L, Gu T H, Xu S G, et al.Drill Steel and Drilling Tools [M]. Beijing: Metallurgical Industry Press, 2000: 24(洪达灵, 顾太和, 徐曙光等. 钎钢与钎具 [M]. 北京: 冶金工业出版社, 2000: 24) | | [8] | Tanaka K, Mura T.A theory of fatigue crack initiation at inclusions[J]. Metall. Trans., 1982, 13A: 117 | | [9] | Wang Q Y, Bathias C, Kawagoishi N, et al.Effect of inclusion on subsurface crack initiation and gigacycle fatigue strength[J]. Int. J. Fatigue, 2002, 24: 1269 | | [10] | Gall K, Horstemeyer M F, Degner B W, et al.On the driving force for fatigue crack formation from inclusions and voids in a cast A356 aluminum alloy[J]. Int. J. Fract., 2001, 108: 207 | | [11] | Melander A.A finite element study of short cracks with different inclusion types under rolling contact fatigue load[J]. Int. J. Fatigue, 1997, 19: 13 | | [12] | Zhang J M, Li S X, Yang Z G, et al.Influence of inclusion size on fatigue behavior of high strength steels in the gigacycle fatigue regime[J]. Int. J. Fatigue, 2007, 29: 765 | | [13] | Monnot J, Heritier B, Cogne J Y.Relationship of melting practice, inclusion type, and size with fatigue resistance of bearing steels [A]. Effect of Steel Manufacturing Processes on the Quality of Bearing Steels[C]. West Conshohocken: ASTM International, 1988: 149 | | [14] | Wang L M, Lin Q, Ji J W, et al. New study concerning development of application of rare earth metals in steels [J]. J. Alloys Compd., 2006, 408-412: 384 | | [15] | Waudby P E.Rare earth additions to steel[J]. Int. Met. Rev., 1978, 23: 74 | | [16] | Yang X H, Wu P F, Cheng G G, et al.Behavior of rare earth on modifying inclusion in special steel[J]. J. Chin. Rare Earth Soc., 2010, 28: 612(杨晓红, 吴鹏飞, 成国光等. 特殊钢中稀土变质夹杂物行为研究[J]. 中国稀土学报, 2010, 28: 612) | | [17] | Wang L J, Liu Y Q, Wang Q, et al.Evolution mechanisms of MgO·Al2O3 inclusions by cerium in spring steel used in fasteners of high-speed railway[J]. ISIJ Int., 2015, 55: 970 | | [18] | Hirata H, Isobe K.Steel having finely dispersed inclusions [P]. U.S. Pat, 20060157162A1, 2004 | | [19] | Liu X, Yang J C, Yang L, et al.Effect of Ce on inclusions and impact property of 2Cr13 stainless steel[J]. J. Iron Steel Res. Int., 2010, 17: 59 | | [20] | Wakoh M, Sawai T, Mizoguchi S.Effect of S content on the MnS precipitation in steel with oxide nuclei[J]. ISIJ Int., 1996, 36: 1014 | | [21] | Verma N, Pistorius P C, Fruehan R J, et al.Calcium modification of spinel inclusions in aluminum-killed steel: Reaction steps[J]. Metall. Mater. Trans., 2012, 43B: 830 | | [22] | Liu H L, Liu C J, Jiang M F.Effect of rare earths on impact toughness of a low-carbon steel[J]. Mater. Des., 2012, 33: 306 | | [23] | Yan N, Yu S F, Chen Y.In situ observation of austenite grain growth and transformation temperature in coarse grain heat affected zone of Ce-alloyed weld metal[J]. J. Rare Earths, 2017, 35: 203 | | [24] | Hao F F, Liao B, Li D, et al.Effects of rare earth oxide on hardfacing metal microstructure of medium carbon steel and its refinement mechanism[J]. J. Rare Earths, 2011, 29: 609 | | [25] | Wang L M.Application of Rare Earth in Low Alloy and Alloy Steel [M]. Beijing: Metallurgical Industry Press, 2016: 16(王龙妹. 稀土在低合金及合金钢中的应用 [M]. 北京: 冶金工业出版社, 2016: 16) | | [26] | Li W C.Thermodynamics of the formation of rare-earth inclusions in steel[J]. Iron Steel, 1986, 21(3): 7(李文超. 钢中稀土夹杂物生成的热力学规律[J]. 钢铁, 1986, 21(3): 7) | | [27] | Adabavazeh Z, Hwang W S, Su Y H.Effect of adding cerium on microstructure and morphology of Ce-based inclusions formed in low-carbon steel[J]. Sci. Rep., 2017, 7: 46503 | | [28] | Ma Q Q, Wu C C, Cheng G G, et al.Characteristic and formation mechanism of inclusions in 2205 duplex stainless steel containing rare earth elements[J]. Mater. Today, 2015, 2: S300 | | [29] | Wilson W G, Kay D, Vahed A.The use of thermodynamics and phase equilibria to predict the behavior of the rare earth elements in steel[J]. JOM, 1974, 26(5): 14 |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|