Export:  BibTeX | EndNote (RIS)      
Abstract  Recent developments in multiphase intermetallics are reviewed in this paper.The emphasis is placed upon the role various interfaces play in influencing the deformationprocess and mechanical behaviour of the multiphase alloys. The examples are taken fromTiAl based and (Ni,Fe,Co)Al based materials. It is shown that the operation of interface-related dislocation sources can improve the deformability of the brittle phases. A better balanceof mechanical properties can be obtained when the beneficial effects of the interfaces are manifested by a proper choice of constituent phases and conditions of material preparation andprocessing.
Key words:  interface      deformation      mechanical behaviour      TiAl      NiAl     
Received:  18 January 1997     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1997/V33/I1/107

1Cahn R W.Phil Trans R Soc Lond A,1995;351:497
2Nabarro F R N.Mater Sci Eng A,1994:184;167
3Noebe R D Bowman R R, Kim J T, Larsen M Gibala R.In:Whang S H,Liu C T,Pope D P,Stiegler J O eds,High Temperature Alumidides Intermetallic,Warrendale:TMS 1990:271
4Kim Y-W, Dimiduk D M JOM,1991(8);43:40
5Fujiwara T,Nakamura A,Hosomi M,Nishitani S R,Shirai Y,Yamaguchi M.Philos Mag A,1990;61:591
6Inui H,Oh M H,Nakamura A Yamaguchi M.Acta Metall Mater,1992;40:30954
7Reviere R D,Oliver B F,Bruns D D.Mater Manuf Proc,1989;4:103
8Minonishi Y.Philos Mag A,1991; 63:1085
9Kad B K,Hazzledine P M,Fraser H L.Mater Res Soc Symp Proc,1993;288:495
10Kad B K,Hazzledine P M.Philos Mag Lett, 1992; 66: 133
11Appel F,Beaven P A, Wagner R.Acta Metall Mater,1993;41:1721
12Christoph U Sparka U,Appel F, Wagner R. Acta Metall Sin(Eng Lett),1995 8:349
13Russell K C,Edington J W.Met Sci J 1972;6:20
14Moskovic R.J Mater Sci,1978;13:1901
15Noebe R D,Misra A Gibala R.ISIJ Int,1991;31:1172
16Misra A Noebe R D,Gibala R.Mater Res Soc Symp Proc,1993;288:483
17Jung I,Sauthoff G.Z Metallkd 1989:80;484
18Guha S,Munroe P R,Baker I.Mater Sci Eng A,1991; 131:27
19Strutt P R, Polvani R S Ingram J C. Metall Trans A, 1976; 7 23
20Polvani R S,Tzeng W S,Strutt P R.Metall Trans A,1976; 7:33
21Nash P G,Liang W W.Metall Trans A,1985;16:319
22Yang R Saunders N,Leake J A, Cahn R W.Acta Metall Mater,1992;40:1553
23Yang R,Parker S V,Leake J A Cahn R W In Stocks G M,Turchi P eds. Alloy Modelling and Design,Proc of TMS Symp,Pittsburgh:TMS,1994:303
24Yang R,Leake J A Cahn R W.J Mater Res,1991;6:343
25Yang R, Leake J A, Cahn R W.Mater Sci Eng,1992;A152:227
26Yang R.PhD Thesis,University of Cambridge,1992
27Yang R,Leake J A Cahn R W.Mater Res Soc Symp Proc, 1993; 288:489
28Hsiung L C,Bhadeshia H K D H.Metall Trans A,1995;26:1895
29Pank D R,Nathal M V,Koss D A J Mater Res,1990; 5:942
30Ishida K,Kainuma R,Ueno N,Nishizawa T Melall Trans A,1991;22:411
31Mishima Y,Lee E H,Liu C T.Mater Trans JIM,1995;36:1031
32Mishima Y Acta Metall Sin (Eng Lett),1995;8:339
33Misnima Y,Kato M, Kimura Y,Hosoda H,Miura S Intermetallics,1996; 6:in pressi
[1] ZHANG Leilei, CHEN Jingyang, TANG Xin, XIAO Chengbo, ZHANG Mingjun, YANG Qing. Evolution of Microstructures and Mechanical Properties of K439B Superalloy During Long-Term Aging at 800oC[J]. 金属学报, 2023, 59(9): 1253-1264.
[2] ZHANG Haifeng, YAN Haile, FANG Feng, JIA Nan. Molecular Dynamic Simulations of Deformation Mechanisms for FeMnCoCrNi High-Entropy Alloy Bicrystal Micropillars[J]. 金属学报, 2023, 59(8): 1051-1064.
[3] DING Hua, ZHANG Yu, CAI Minghui, TANG Zhengyou. Research Progress and Prospects of Austenite-Based Fe-Mn-Al-C Lightweight Steels[J]. 金属学报, 2023, 59(8): 1027-1041.
[4] LI Jingren, XIE Dongsheng, ZHANG Dongdong, XIE Hongbo, PAN Hucheng, REN Yuping, QIN Gaowu. Microstructure Evolution Mechanism of New Low-Alloyed High-Strength Mg-0.2Ce-0.2Ca Alloy During Extrusion[J]. 金属学报, 2023, 59(8): 1087-1096.
[5] XU Yongsheng, ZHANG Weigang, XU Lingchao, DAN Wenjiao. Simulation of Deformation Coordination and Hardening Behavior in Ferrite-Ferrite Grain Boundary[J]. 金属学报, 2023, 59(8): 1042-1050.
[6] ZHANG Lu, YU Zhiwei, ZHANG Leicheng, JIANG Rong, SONG Yingdong. Thermo-Mechanical Fatigue Cycle Damage Mechanism and Numerical Simulation of GH4169 Superalloy[J]. 金属学报, 2023, 59(7): 871-883.
[7] LI Fulin, FU Rui, BAI Yunrui, MENG Lingchao, TAN Haibing, ZHONG Yan, TIAN Wei, DU Jinhui, TIAN Zhiling. Effects of Initial Grain Size and Strengthening Phase on Thermal Deformation and Recrystallization Behavior of GH4096 Superalloy[J]. 金属学报, 2023, 59(7): 855-870.
[8] LIU Junpeng, CHEN Hao, ZHANG Chi, YANG Zhigang, ZHANG Yong, DAI Lanhong. Progress of Cryogenic Deformation and Strengthening-Toughening Mechanisms of High-Entropy Alloys[J]. 金属学报, 2023, 59(6): 727-743.
[9] WANG Furong, ZHANG Yongmei, BAI Guoning, GUO Qingwei, ZHAO Yuhong. First Principles Calculation of Al-Doped Mg/Mg2Sn Alloy Interface[J]. 金属学报, 2023, 59(6): 812-820.
[10] WANG Changsheng, FU Huadong, ZHANG Hongtao, XIE Jianxin. Effect of Cold-Rolling Deformation on Microstructure, Properties, and Precipitation Behavior of High-Performance Cu-Ni-Si Alloys[J]. 金属学报, 2023, 59(5): 585-598.
[11] WAN Tao, CHENG Zhao, LU Lei. Effect of Component Proportion on Mechanical Behaviors of Laminated Nanotwinned Cu[J]. 金属学报, 2023, 59(4): 567-576.
[12] LI Min, WANG Jijie, LI Haoze, XING Weiwei, LIU Dezhuang, LI Aodi, MA Yingche. Effect of Y on the Solidification Microstructure, Warm Compression Behavior, and Softening Mechanism of Non-Oriented 6.5%Si Electrical Steel[J]. 金属学报, 2023, 59(3): 399-412.
[13] JI Xiumei, HOU Meiling, WANG Long, LIU Jie, GAO Kewei. Modeling and Application of Deformation Resistance Model for Medium and Heavy Plate Based on Machine Learning[J]. 金属学报, 2023, 59(3): 435-446.
[14] LI Qian, SUN Xuan, LUO Qun, LIU Bin, WU Chengzhang, PAN Fusheng. Regulation of Hydrogen Storage Phase and Its Interface in Magnesium-Based Materials for Hydrogen Storage Performance[J]. 金属学报, 2023, 59(3): 349-370.
[15] XIA Dahai, JI Yuanyuan, MAO Yingchang, DENG Chengman, ZHU Yu, HU Wenbin. Localized Corrosion Mechanism of 2024 Aluminum Alloy in a Simulated Dynamic Seawater/Air Interface[J]. 金属学报, 2023, 59(2): 297-308.
No Suggested Reading articles found!