| HARDNESS CHANGES OF Al-Zn-Mg ALLOY DURING RETROGRESSION AND REAGING |
| MENG Zhaofu;ZHENG Yong;LONG Houwen (Materials Science Institute; Jilin University; Changchun 130023); LIU Yuhui (State Key Laboratory for Corrosion and Protection; Institute of Corrsion and Protection of Metals; Chinese Academy of Sciences;Shenyang 110015) |
|
Cite this article:
MENG Zhaofu;ZHENG Yong;LONG Houwen (Materials Science Institute; Jilin University; Changchun 130023); LIU Yuhui (State Key Laboratory for Corrosion and Protection; Institute of Corrsion and Protection of Metals; Chinese Academy of Sciences;Shenyang 110015). HARDNESS CHANGES OF Al-Zn-Mg ALLOY DURING RETROGRESSION AND REAGING. Acta Metall Sin, 1997, 33(5): 479-484.
|
|
|
Abstract In this paper the hardness change of Al-Zn-Mg alloy during aging-retrogression-reaging treatments was studied. The microstructure change and the mechanism of the change in hardness were studied by small-angle X-ray scattering.
|
|
Received: 18 May 1997
|
1Cina B,U S Pat 3 856 584,1974 2Danh N C,Rajan K,Wallace W.Metall Trans 1983:14A:1843 3Part J K,Ardell A J.Matall Trans,1983;14A:1957 4 Park J K,Ardell A J.Metall Trans 1984;15A:1531 5Danh N C,Rajan K, Wallace W. Metall Trans,1985;16A:2068 6Park J K.Mater Sci Eng,1988;103:223 7Guinier A,Fournet G.Small Angle Scattering of X-rays.New York:Wiley,1955:17 8Meng C,Wang Y.Scr Matall Mater,1990;24:1521 9Meng C.J Non-Cryst Solids,1991;130:107 10孟昭富,王煜明.中国科学,1990;A(11):1224 11孟昭富.中国科学,1994;A(7):761e |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|