| TENSILE PROPERTIES OF ALLOY ZA27 AT ELEVATED TEMPERATURES |
| ZHU Yuefeng (Institute of Metal Research; Chinese Academy of Sciences; Shenyang 110015); ZENG Daben; HUANG Huisong; WU Dehai (Tsinghua University; Beijing 100084) |
|
Cite this article:
ZHU Yuefeng (Institute of Metal Research; Chinese Academy of Sciences; Shenyang 110015); ZENG Daben; HUANG Huisong; WU Dehai (Tsinghua University; Beijing 100084). TENSILE PROPERTIES OF ALLOY ZA27 AT ELEVATED TEMPERATURES. Acta Metall Sin, 1997, 33(5): 499-503.
|
|
|
Abstract The tensile properties of alloy ZA27 at ambient temperature and elevated(from 275℃ through the solidus) temperatures were studied. The tress-strain plots at varies temperatures and the relationship between the mechanical properties of the alloy and temperatures are obtained. The results show that, the strength decreases with increasing temperature, the alloy exhibits high deformation ability at elevated temperatures, and the fracture modes are dependent on temperature. At about 275℃, alloy ZA27 has high plasticity and very small resistance to deformation, so it is suitable for the alloy to be processed by deformation at this temperature range.
|
|
Received: 18 May 1997
|
1 Gervais E,Levert H,Bess M.Trans Am Foundrymen's 1980;88:183 2Barber M J,Jones P E.Foundry Trade J,1980;148:114 3 Birch J.Mater Des,1990;11(2):83 4久保田耕平,二宫隆二,佐藤勉,尾城武司.铸物,1992;64:765 5曾松岩,段守坤,蒋祖龄,李庆春,孙阳.铸造技术,1991;(5):20 6李振镳.特种铸造及有色合金,1985;(2):10 7Walmag G,Lamberigts M,Coutsouradis D,洛阳工学院耐磨材料研究室译.第25届国际冶金年会译文选.北京:机械工业出版社,1992:9b |
| No Suggested Reading articles found! |
|
|