| INFLUENCING FACTORS OF SERRATED FLOW IN Al-Li SINGLE CRYSTALS |
| Tian Baohui (Beijing Institute of Aeronautical Materials; Beijing 100095); Li HuanxiZhang Yonggang;Chen Changqi(Beijing University of Aeronautics and Astronautics;Beijing 100083) |
|
Cite this article:
Tian Baohui (Beijing Institute of Aeronautical Materials; Beijing 100095); Li HuanxiZhang Yonggang;Chen Changqi(Beijing University of Aeronautics and Astronautics;Beijing 100083). INFLUENCING FACTORS OF SERRATED FLOW IN Al-Li SINGLE CRYSTALS. Acta Metall Sin, 1997, 33(6): 577-582.
|
|
|
Abstract Occurrence of serrated flow in Al-Li single crystals is related to the shearingof δ' particles. Critical strain varies with temperature, strain rate and aging state. The agingconditions and crystal orientations of the loading axes have some effects on the time periodwithin one cycle of serration and stress amplitude of serration.
|
|
Received: 18 June 1997
|
1Wert J A,Wycliffe P A.Scr Metall Mater,1985;19:463 2 Gregson P J.McDarmaid D S,Hunt E.Mater Sci Technol,1988;4:713 3Tamura M, Mori T,Nakamura T. Trans JIM, 1973;14: 355 4 Zambo S J,Wert J A.Scr Melall Mater,1993;29:1523 5 Huang J C,Gray G T.Scr Metall Mater,1990;24:85 6 Deladosse D,Lapasset G,Kubin L P.Scr Metall Mater,1993;28:1379 7 Ilic N,Drobniak Dj,Radmilovic V,Jovanovic M T,Markovic D.Scr Metll Maler,1996;34:1123 8 Diego N, Rio J del, Segers D, Dorikens—Vanpraet L, Dorikens M. Phy Rev(B), 1993; 48: 6781 9King J E, You C Y, Knott J F. Acta Metall, 1981:29: 1553 10 Cottrell A H.Dislocation and Plastic Flow in Crysals,Clarendon,Oxford,1953:136 11 Wood J,McCormick P G.Acta Metall ,1971;19:463 12 Bchnood N, Evans J T Acta Metall, 1989; 37: 687 13 Evans J T.Scr Metall Mater,1987;21:435 14 Miuya Y,Matsui A,Furukawa M,Nemoto M.In:Baker C,Gregson D J, Harris S T,Peel C T eds,Aluminum—Lithium Alloys III, London:Inst of Metals,1986:427 15 Brechet Y,Estrin Y.Scr Metall Mater,1994:31:185 16 Fujita H, Tanata T Acta Metall, 1982; 25: 793= |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|