Abstract [Co(1.2nm) / Cu(tCu)](tCu= 1.0 nm, 3.4 nm) nano-multilayers were preparedby dual-facing target sputtering method. The multilayers were then annealed in silu by TEMand TG methods to investigate the changes of the microstructure and magnetism. Twoferromagnetic phases, hop Co and Co-Cu solid solution with lattice parameter of around0.358 nm, existed in tCu= 1.0 nm multilayer and were related to two magnetictransformations.
|
|
Received: 18 June 1997
|
1朱勇,谭铭,储昭琴,张立德.科学通报,1995:40:213 2 Huang L J, Liu B X. Appl Phys Lett, 1990; 57:1401 3 Nishizawa T, Ishida K. Bulletin of Alloy Phase Diagrams, 1984; 5: 161 4 Mosca D H,Petroff F,Fert A.J Magn Magn Mater,1991:94:L1 5 Gleiter H、 Prog Mater Sci, 1989: 33: 223 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|