MICROSTRUCTURE AND MAGNETISM OF[Co/Ti] AND [Co/Cu(Ni)] MULTILAYERS
WU Ping;JIANG Enyong; WANG Cunda; BAI Haili; LIU Yuguang; WANG Heying(Tian jin University; Tianjin; 300072)
Cite this article: 

WU Ping;JIANG Enyong; WANG Cunda; BAI Haili; LIU Yuguang; WANG Heying(Tian jin University; Tianjin; 300072). MICROSTRUCTURE AND MAGNETISM OF[Co/Ti] AND [Co/Cu(Ni)] MULTILAYERS. Acta Metall Sin, 1997, 33(6): 625-630.

Download:  PDF(1075KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Two series of the multilayers with the forms of [Co/Ti]30 and[Co / Cu(Ni)]30 prepared by dual facing target sputtering at room temperature, consist ofamorphous Co magnetic layer and exhibit soft magnetic properties. The structural and magnetic properties of [Co/Cu(Ni)] and [Co/Ti] multilayers were examined as a function of thespacer layer thickness (dTi and dCu(Ni)) by XRD, TEM and VSM measurements. The saturation magnetization Ms of the [Co/Ti] multilayer was found to decrease with dTi, but for the[Co/Cu(Ni)] multilayers, the Ms was found to oscillate with dCu(Ni). The Ms approached toa constant value when dTi and dCu(Ni) thickened enough. This is the result of differentinterlayer magnetic coupling effects.
Key words:  [Co/Ti] multilayer      [Co/Cu(Ni)] multilager      saturation magnetization.interlayer magnetic coupling      density of state     
Received:  18 June 1997     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1997/V33/I6/625

1 Parkin S S P,More N,Roche K P.Phys Rev Lett,1990;64:2304
2Barthelemy A,Fert A,Baibich M N,HadjoudjS,Petroff F.J Appl Phys,1990;67:5908
3 Parkin S S P,Bhadra R,Roche K P.Phys Rev Lett,1991;66:2152
4 Inomata K,Yusu K,Saito Y.Mater Sci Eng,1995;B31:41
5Qiu Z Q,Pearson J,Berger A,Bader S D.Phys Rev Lett,1992;68:1398
6 Fub A,Demokritov S,Grunberg P.J Magn Magn Mater,1992:103:L221
7Liu Y H, Zhang Y M,Yan S S, Ma X D. Phys Rev, 1993; B48: 10266
8 Shi Z P and Klein B M.Phys Rev,1995;B52:12516
9Bobo J F,Hennet b,Piecuch M.J Magn Magn Mater,1995;140-144:587
10 Bruno P,Chappert C.Phys Rev Lett.1991;67:1602
11 XU Y B, Lu M, Bie Q S, Zhai Y, Jin Q Y, Zhu X B, Zhai H R. J Magn Magn Mater, 1995;140—144: 581
12 Fabian D T. Band structure spectroscopy ofmetals and alloys.London: Academic Press, 1973: 63,679
13 Leevwen R V,England C D,Dutcher J R,Falco C M.J Appp Phys,1990;67:4910F
[1] Jun SUN, Jinyu ZHANG, Kai WU, Gang LIU. SIZE EFFECTS ON THE DEFORMATION AND DAMAGEOF Cu-BASED METALLIC NANOLAYEREDMICRO-PILLARS[J]. 金属学报, 2016, 52(10): 1249-1258.
[2] ZHANG Jinyu, LIU Gang, SUN Jun. SIZE EFFECTS ON DEFORMATION AND FRACTURE BEHAVIOR OF NANOSTRUCTURED METALLIC MULTILAYERS[J]. 金属学报, 2014, 50(2): 169-182.
[3] CHENG Dong YAN Zhijun YAN Li. MOLECULAR DYNAMICS SIMULATION OF STRENGTHENING MECHANISM OF Cu/Ni MULTILAYERS[J]. 金属学报, 2008, 44(12): 1461-1464.
[4] YU Xiang; WANG Chengbiao; LIU Yang; YU Deyang. TiN/Ti MULTILAYER FILMS SYNTHESIZED BY MID-FREQUENCY DUAL-MAGNETRON SPUTTERING[J]. 金属学报, 2006, 42(6): 662-666 .
[5] WANG Xinhua; WANG Lingling; WANG Huaiyu; DENG Huiqiu; HUANG Weiqing . INFLUENCES OF FLUORINE DOPING TO THE ELECTRONIC STRUCTURE OF THE Y-Ba-Cu-O UPERCONDUCTORS[J]. 金属学报, 2004, 40(12): 1243-1247 .
[6] WU Ping; JIANG Enyong; LIU Yuguang; WANG Cunda(Tianjin University; Tianjin 300072). EVOLUTION OF STRUCTURE AND MAGNETIC PROPERTIES DURING CRYSTALLIZATION OF AMORPHOUS Co/Ti MULTILAYER FILMS[J]. 金属学报, 1996, 32(11): 1209-1214.
[7] JIANG Enyong;BAI Haili;WANG Cunda;U.BOGLI(Tianjin University;Tianjin 300072)(Department of Applied Physics;Tianjin University;Tianjin 300072)(Manuscript received 1995-12-08;in revised form 1996-06-12). STRUCTURAL STABILITY OF Co/C MULTILAYERS[J]. 金属学报, 1996, 32(10): 1068-1074.
[8] WANG Zhenjun; CHANG Xiangrong; PING Jueyun; TIAN Zhongzhuo; XIAO Jimei (University of Science and Technology Beijing; Beijing 100083); WEN Lishi (Institute of Metal Research; Chinese Academy of Sciences; Shenyang 110015)(Manuscript received 1995-03-03; in revised form 1995-07-21 ). STRUCTURE AND MAGNETISM OF DC-MAGNETRON SPUTTERING Fe / Ti PERIODICAL NANO-MULTILAYERS[J]. 金属学报, 1996, 32(1): 85-90.
No Suggested Reading articles found!