| HEAT DAMAGE MECHANISMS AND EVALUATION METHOD OF WC PART1CLES IN LASER CLAD WC-Ni COMPOSITE COATING |
| ZENG Xiaoyan; WU Xinwei; TAO Zengyi; ZHU Beidi; CUI Kun (Department of Materials Schoce and Engineering; Huazhong University of Science and Technology; Wuhan 430074) (Manuscript received 1996-07-12; in revised form 1997-03-14) |
|
Cite this article:
ZENG Xiaoyan; WU Xinwei; TAO Zengyi; ZHU Beidi; CUI Kun (Department of Materials Schoce and Engineering; Huazhong University of Science and Technology; Wuhan 430074) (Manuscript received 1996-07-12; in revised form 1997-03-14). HEAT DAMAGE MECHANISMS AND EVALUATION METHOD OF WC PART1CLES IN LASER CLAD WC-Ni COMPOSITE COATING. Acta Metall Sin, 1997, 33(8): 863-868.
|
|
|
Abstract In this paper, the heat damage fashions and mechanisms of the cast WC parti-cles in the laser clad ceramic-metal composite coating have been investigated systematically. It was demonstrated that the main heat damage fashion of the cast WC particles is the disso-lution and diffusion scorification. A half quantitative formula was derived to evaluate theheat damage extent of the WC particles.
|
|
Received: 18 August 1997
|
1曾晓雁,朱蓓蒂,陶曾毅,崔 .材料科学与工程,1995;13(4):8 2 Boas M, BamdergerM. Surf Coat Technol,1990; 42: 175 3陶曾毅,陈新.中国激光,1989;16:629 4 Zeng Xiaoyan, Tao Zengyi, Zhu Beidi, Cui Kun. Surf Coat Technol, 1996; 79: 209 5 Cerri W, Mortinella R, Mor G P, Bianchi P, Angelo D D. Surf Coat Technol,1991; 49: 40 6 Zeng Xiaoyan, Tao Zengyi, Zhu Beidi, Zhou Erhua, Cui Kun. Surf Coat Technol, 1996; 79: 162 7 Abbas G, West D R F, Steen W R. Key Eng Mater, 1990; 46-47: 47 8 Zhu Beidi, Zeng Xiaoyan, Tao Zengyi, Yang Shuguo, Cui Kun. Wear, 1993; 170: 161 9曾晓雁.华中理工大学博士学位论文,1993 10曾晓雁.华中理工大学学报,1995;23(12):76 11曾晓雁.金属学报,1997;33:885 |