REACTION MECHANISM AND DISTRIBUTlON RULES OF SULFUR IN MELTING GASIFIER
LU Qing;JIANG Wufeng;LU Changxing;YIN Haisheng(Hebei Institule of Technol ogy; Tangshan 063009)
Cite this article: 

LU Qing;JIANG Wufeng;LU Changxing;YIN Haisheng(Hebei Institule of Technol ogy; Tangshan 063009). REACTION MECHANISM AND DISTRIBUTlON RULES OF SULFUR IN MELTING GASIFIER. Acta Metall Sin, 1997, 33(9): 952-958.

Download:  PDF(1535KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The smelting process in melting gasifier of COREX has been simulated experimentally. Using the way of dissecting the melting gasifier, reaction mechanism and rule of distribution of sulfur have been studied. The changing patterns of sulfur content in DRI, flux,coal, gas, slag and liquid iron, which effect on sulfur content of the metal, were obtained.
Key words:  melting-gasifier      sulfur      distribution      reaction     
Received:  18 September 1997     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1997/V33/I9/952

1桑野 禄郎,奥 隆夫,小野阳一.铁钢,1980;66:1622
2Langhammer N,Hchenck G.Archiv fur das Eisenhuttenwesen,1966; 37:1
3Shumaker C,Schuhmann R Metall Trans,1983;14B:291
4追谷 畅男,大谷正康,冈部 侠 铁钢,1973;59:33
5Rausch H,Saatci A Thumm W,Oeters F Arch Eisenhuttenwes,1975;46:623
6Rausch H,SaatCi A Thumm W,Oeters F,Stahlu Eisen,1975; 95:1266
7Delport H M W.Ironmaking Steelmaking,1992 19(3):183
8吕庆,张瑞祥.钢铁,1995;30(10):8
9Biswas A K著,齐宝铭,王筱留译.高炉炼铁原理──理论与实践.北京:冶金工业出版社,1989:376
10张景智.国外钢铁,1981;68(8):11
11王筱留.钢铁冶金学.北京:冶金工业出版社,1994:123
[1] DU Zonggang, XU Tao, LI Ning, LI Wensheng, XING Gang, JU Lu, ZHAO Lihua, WU Hua, TIAN Yucheng. Preparation of Ni-Ir/Al2O3 Catalyst and Its Application for Hydrogen Generation from Hydrous Hydrazine[J]. 金属学报, 2023, 59(10): 1335-1345.
[2] SHEN Yingying, ZHANG Guoxing, JIA Qing, WANG Yumin, CUI Yuyou, YANG Rui. Interfacial Reaction and Thermal Stability of the SiCf/TiAl Composites[J]. 金属学报, 2022, 58(9): 1150-1158.
[3] SONG Qingzhong, QIAN Kun, SHU Lei, CHEN Bo, MA Yingche, LIU Kui. Interfacial Reaction Between Nickel-Based Superalloy K417G and Oxide Refractories[J]. 金属学报, 2022, 58(7): 868-882.
[4] ZHANG Shihong, HU Kai, LIU Xia, YANG Yang. Corrosion-Erosion Mechanism and Research Prospect of Bare Materials and Protective Coatings for Power Generation Boiler[J]. 金属学报, 2022, 58(3): 272-294.
[5] ZHENG Chun, LIU Jiabin, JIANG Laizhu, YANG Cheng, JIANG Meixue. Effect of Tensile Deformation on Microstructure and Corrosion Resistance of High Nitrogen Austenitic Stainless Steels[J]. 金属学报, 2022, 58(2): 193-205.
[6] CAO Chao, JIANG Chengyang, LU Jintao, CHEN Minghui, GENG Shujiang, WANG Fuhui. Corrosion Behavior of Austenitic Stainless Steel with Different Cr Contents in 700oC Coal Ash/High Sulfur Flue-Gas Environment[J]. 金属学报, 2022, 58(1): 67-74.
[7] ZHAO Naiqin, GUO Siyuan, ZHANG Xiang, HE Chunnian, SHI Chunsheng. Progress on Graphene/Copper Composites Focusing on Reinforcement Configuration Design: A Review[J]. 金属学报, 2021, 57(9): 1087-1106.
[8] WANG Chao, ZHANG Xu, WANG Yumin, YANG Qing, YANG Lina, ZHANG Guoxing, WU Ying, KONG Xu, YANG Rui. Mechanisms of Interfacial Reaction and Matrix Phase Transition in SiCf /Ti65 Composites[J]. 金属学报, 2020, 56(9): 1275-1285.
[9] DING Wen, WANG Xiaojing, LIU Ning, QIN Liang. Diffusion Bonding of Copper and 304 Stainless Steel with an Interlayer of CoCrFeMnNi High-Entropy Alloy[J]. 金属学报, 2020, 56(8): 1084-1090.
[10] SUN Feilong, GENG Ke, YU Feng, LUO Haiwen. Relationship of Inclusions and Rolling Contact Fatigue Life for Ultra-Clean Bearing Steel[J]. 金属学报, 2020, 56(5): 693-703.
[11] LI Yaqiang, LIU Jianhua, DENG Zhenqiang, QIU Shengtao, ZHANG Pei, ZHENG Guiyun. Peritectic Solidification Characteristics and Mechanism of 15CrMoG Steel[J]. 金属学报, 2020, 56(10): 1335-1342.
[12] ZHANG Zhijie, HUANG Mingliang. In Situ Study on Liquid-Solid Electromigration Behavior in Cu/Sn-37Pb/Cu Micro-Interconnect[J]. 金属学报, 2020, 56(10): 1386-1392.
[13] WANG Zumin,ZHANG An,CHEN Yuanyuan,HUANG Yuan,WANG Jiangyong. Research Progress on Fundamentals and Applications of Metal-Induced Crystallization[J]. 金属学报, 2020, 56(1): 66-82.
[14] Hulin DONG,Haiping BAO,Jianhong PENG. Effect of TiC Contents on Mechanical Properties and Wear Resistance of Iron-Based Composites[J]. 金属学报, 2019, 55(8): 1049-1057.
[15] Xin LI,Yuecheng DONG,Zhenhua DAN,Hui CHANG,Zhigang FANG,Yanhua GUO. Corrosion Behavior of Ultrafine Grained Pure Ti Processed by Equal Channel Angular Pressing[J]. 金属学报, 2019, 55(8): 967-975.
No Suggested Reading articles found!