Abstract  The precipitating morphology of the boron components in the boron slags were in both crystallized and amorphous forms during the solidification of the molten salgs.The efficiency of extracted boron (EEB) from the former slag, crystal form, was obviously higher than that from the later slag. The precipitating behavior and morphology of the boron components in the slags can be artificially controlled. The Suanite(2MgO·B2O3) will exist as main phase by changing chemical composition, temperature of heat-treatment and addition,that is the selective precipitating. SEM in situ observation of the heating sample and the computer simulation combined with fractal description confirmed that the precipitating processes of the molten slags consists of the separation of amorphous phase through spinoda1 decomposition and of the precipitating of Suanite by the model of diffusion limited aggregation.
Key words:  slags bearing boron      selective precipitating      efficiency of extracting boron      computer simulation     
Received:  18 September 1997     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1997/V33/I9/943

1张显鹏.辽宁冶金,1991;4:36
2Zhang Peixin Sui Zhitong Metall Mater Trans,1995;B26:345
3张培新,林红,隋智通.硅酸盐学报,1996;23:555
4Bodsworth C,Bell H B.Physical Chemistry of Iron and Steel Manufacture.London:Longman Group Limited 1972:67
5郭贻诚,王震西.非晶态物理学北京:科学出版社,1984:99
6Turkdogan E T.Physical Chemeistry of Higg Temperature Technology,New York:Academic Press.1980:130
7Zhang Peixin,Zhang Qizhi,Wu Liming,Sui Zhitong. Z Metallk,1996;87(1):76
8Zhang Peixin,Sui Zhitong.Scand J Metall ,1994;23:244
9Kissinger H E J Res Nat Bur Stand ,1956,57(4):217
10彭文世,刘高魁著.矿物红外光谱图集北京:科学出版社,1982:179
11杨南如主编无机非金属材料测试方法.武汉:武汉工业大学出版社,1990:273
[1] ;. STUDY OF 3D QUASI--STATIONARY GRAIN SIZE DISTRIBUTION DERIVED FROM MACPHERSON—SROLOVITZ TOPOLOGY--RELATED GRAIN GROWTH RATE EQUATION[J]. 金属学报, 2008, 44(7): 769-774 .
[2] zhang lin. Modelling structural changes of a molten Cu55 cluster on cooling by molecular dynamics[J]. 金属学报, 2008, 44(10): 1161-1166 .
[3] HOU Hua; ZHAO Yuhong; CHEN Zheng; XU Hong. Prediction for the Early Precipitation Process of Ni75AlxV25-X System with Lower Al Concentration by the Phase-Field Model[J]. 金属学报, 2005, 41(7): 695-702 .
[4] ZHANG Lin; ZHANG Caibei; WANG Yuanming; WANG Shaoqing. Cellular Automaton Modelling Of The Transformation From Austenite to Ferrite In Low Carbon Steels During Continuous Cooling[J]. 金属学报, 2004, 40(1): 8-13 .
[5] CHU Yelong; XIONG Liangyue; SUN Xiaokai (Institute of Metal Research; The Chinese Academy of Sciences; Shenyang 110015). COMPUTER STUDY OF MAGNETIZATION IN NANOCOMPOSITE MAGNETS[J]. 金属学报, 1998, 34(4): 423-430.
[6] YIN Aijun; LI Jing; LI Hinhai; HUANG Kexiong; JIANG Hanying (Central South University of Technology; Changsha 410083) (Manuscript received 1995-06-30; in revised form 1995-12-01). COMPUTER SIMULATION ON MINOR ELEMENT BEHAVIOUR IN COPPER FLASH SMELTING[J]. 金属学报, 1996, 32(4): 387-392.
[7] CAI Xun; ZHOU Pingnan; (Shanghai Jiaotong University ; Shanghai 200030)Bangert H (Technical University of Vienna; Auslria)(Manuscript received 94-07-18). SIMULATION OF INDENTATION MICROHARDNESS TESTING[J]. 金属学报, 1995, 31(13): 44-5.
[8] CAO Zhenning(Shandong Polytechnic Unversity; Jinan);WU Chuansong; WU Lin (Harbin Institute of Technology). COMPUTER SIMULATION OF MIG WELD POOLS WITH DROPLET IMPACT[J]. 金属学报, 1994, 30(24): 537-542.
[9] CHEN Da;LU Min;LIN Dongliang (Lin T L) Shanghai Jiao Tong UniversityDepartment of Materials Science;Shanghai Jiao Tong University; Shanghai 200030. SIMULATIVE STUDY OF INTERACTION BETWEEN GRAIN BOUNDARIES AND DISLOCATIONS IN Ni_3Al[J]. 金属学报, 1993, 29(7): 34-39.
[10] SHAO Jun;XU Hua;CHENG Ailan;KLEIN M. L. University of Pennsylvania; Philadelphia; U. S. A; State University of New York; U. S. A.; University of Pennsylvania; Philadelphia; U. S. A.. CONSTANT PRESSURE MOLECULAR DYNAMICS SIMULATION OF MOLTEN LiF-BeF_2 SYSTEM[J]. 金属学报, 1993, 29(1): 59-64.
[11] YAN Wen Xi'an Institute of Technology Correspondent associate professor;xi'an Institute of Technology. SYMMETRICAL SUPERLATTICE INTRINSJC STACKING FAULTS IN DEFORMEDPOLYCRYSTALLINE Ni_3 Al AND THEIR FORMATION MECHANISM[J]. 金属学报, 1991, 27(5): 8-13.
[12] WANG Xi;ZHOU Jiankun;CHEN Youshan;LIU Xianghuai;ZOU Shichang Ion Beam Laboratory; Shanghai Institute of Metallurgy; Academia Sinica. COMPUTER SIMULATION OF ION BEAM ENHANCED DEPOSITION OF TiN FILMS[J]. 金属学报, 1991, 27(3): 136-141.
[13] WEI Chao;QIAN Rengen;LIN Shi;XIAO Jimei University of Science and Technology Beijing Department of mathematics and mechanics; University of Science and Technology Beijing; Beijing 100083. COMPUTER SIMULATION OF EFFECT OF ORIENTATION DIFFERENCE ON MECHANICAL PROPERTIES OF BICRYSTALLINE SPECIMENS[J]. 金属学报, 1990, 26(4): 18-21.
[14] LIN Dongliang;CHEN Da T. L. Lin Shanghai Jiaotong University professor;Department of Materials Science;Shanghai Jiaotong University;Shanghai 200030. COMPUTER SIMULATION OF GRAIN BOUNDARY STRUCTURES IN Ni_3 Al[J]. 金属学报, 1990, 26(3): 10-17.
[15] XIA Lifang;YAN Mufu Harbin Institute of TechnologyDivision of Metal Materials and Heat treatment; Harbin Institute of Technology; Harbin. MATHEMATICAL MODELS OF NITROGEN CONCENTRATION PROFILE OF ION NITRIDED LAYERS AND COMPUTER SIMULATION[J]. 金属学报, 1988, 24(4): 314-321.
No Suggested Reading articles found!