Acta Metall Sin  1998, Vol. 34 Issue (1): 19-23    DOI:
Current Issue | Archive | Adv Search |
DIFFUSION-CONTROLLED PHASE TRANSFORMATIONS OF Al_(65)Cu_(20)Cr_(15) QUASICRYSTALLINE PARTICLES/AI MATRIX COMPOSITES
QI Yuhong;ZHANG Zhanping;HEI Zukun (Institute of Metal and Technology; Dalian Maritime University; Dalian 116026)QUAN Mingliu (Institute of Metal Research; The Chinese Academy of Sciences; Shenyang 110015)DONG Chuang (Dalian University of Technology; 116024)
Cite this article: 

QI Yuhong;ZHANG Zhanping;HEI Zukun (Institute of Metal and Technology; Dalian Maritime University; Dalian 116026)QUAN Mingliu (Institute of Metal Research; The Chinese Academy of Sciences; Shenyang 110015)DONG Chuang (Dalian University of Technology; 116024). DIFFUSION-CONTROLLED PHASE TRANSFORMATIONS OF Al_(65)Cu_(20)Cr_(15) QUASICRYSTALLINE PARTICLES/AI MATRIX COMPOSITES. Acta Metall Sin, 1998, 34(1): 19-23.

Download:  PDF(1621KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Diffuse phase transformations of A165Cu20Cr15 quasicrystalline particles/AI composite were studied by TEM for the first time. It shows that SIQC quasicrystalline particles transform into FIQC, (DQC+DA)+θand θ phases respectively at the different hot press temperatures of 600, 650 and 700 ℃. During diffusion-controlled phase transformation, SIQC phase transforms through the transitional FIQC, DQC, DA phase to the stable θ phase.
Key words:  quasicrystal      composite      phase transformation     
Received:  18 January 1998     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1998/V34/I1/19

1 Shechtman D, Blech I,Cahn J W.Phys Rev Lett;1984;53:1951
2 Kang S S,Dubois J M J Mater Res,1993; 8:2471
3 Tsai A P, Aoki K;Inove A.Masumoto T J Mater Res.1993;8:5
4 齐育红.张占平.黑祖昆,严立.摩擦学学报,1997;待发表(Qi Yuhong,Zhang Zhanping;Hei Zukun,Yan Li.Tribology;1997,to be published)
5 Bondersky L.Phys Rev Lett,1985; 54: 2422
6 Selke H; Ryder P L Mater Sci Eng, 1993; A165: 81
[1] BAI Jiaming, LIU Jiantao, JIA Jian, ZHANG Yiwen. Creep Properties and Solute Atomic Segregation of High-W and High-Ta Type Powder Metallurgy Superalloy[J]. 金属学报, 2023, 59(9): 1230-1242.
[2] ZHANG Deyin, HAO Xu, JIA Baorui, WU Haoyang, QIN Mingli, QU Xuanhui. Effects of Y2O3 Content on Properties of Fe-Y2O3 Nanocomposite Powders Synthesized by a Combustion-Based Route[J]. 金属学报, 2023, 59(6): 757-766.
[3] FENG Aihan, CHEN Qiang, WANG Jian, WANG Hao, QU Shoujiang, CHEN Daolun. Thermal Stability of Microstructures in Low-Density Ti2AlNb-Based Alloy Hot Rolled Plate[J]. 金属学报, 2023, 59(6): 777-786.
[4] MA Zongyi, XIAO Bolv, ZHANG Junfan, ZHU Shize, WANG Dong. Overview of Research and Development for Aluminum Matrix Composites Driven by Aerospace Equipment Demand[J]. 金属学报, 2023, 59(4): 457-466.
[5] WANG Chongyang, HAN Shiwei, XIE Feng, HU Long, DENG Dean. Influence of Solid-State Phase Transformation and Softening Effect on Welding Residual Stress of Ultra-High Strength Steel[J]. 金属学报, 2023, 59(12): 1613-1623.
[6] ZHANG Kaiyuan, DONG Wenchao, ZHAO Dong, LI Shijian, LU Shanping. Effect of Solid-State Phase Transformation on Stress and Distortion for Fe-Co-Ni Ultra-High Strength Steel Components During Welding and Vacuum Gas Quenching Processes[J]. 金属学报, 2023, 59(12): 1633-1643.
[7] MA Guonan, ZHU Shize, WANG Dong, XIAO Bolv, MA Zongyi. Aging Behaviors and Mechanical Properties of SiC/Al-Zn-Mg-Cu Composites[J]. 金属学报, 2023, 59(12): 1655-1664.
[8] JIANG Jiang, HAO Shijie, JIANG Daqiang, GUO Fangmin, REN Yang, CUI Lishan. Quasi-Linear Superelasticity Deformation in an In Situ NiTi-Nb Composite[J]. 金属学报, 2023, 59(11): 1419-1427.
[9] LI Xiaobing, QIAN Kun, SHU Lei, ZHANG Mengshu, ZHANG Jinhu, CHEN Bo, LIU Kui. Effect of W Content on the Phase Transformation Behavior in Ti-42Al-5Mn- xW Alloy[J]. 金属学报, 2023, 59(10): 1401-1410.
[10] LI Sai, YANG Zenan, ZHANG Chi, YANG Zhigang. Phase Field Study of the Diffusional Paths in Pearlite-Austenite Transformation[J]. 金属学报, 2023, 59(10): 1376-1388.
[11] SHEN Yingying, ZHANG Guoxing, JIA Qing, WANG Yumin, CUI Yuyou, YANG Rui. Interfacial Reaction and Thermal Stability of the SiCf/TiAl Composites[J]. 金属学报, 2022, 58(9): 1150-1158.
[12] GU Ruicheng, ZHANG Jian, ZHANG Mingyang, LIU Yanyan, WANG Shaogang, JIAO Da, LIU Zengqian, ZHANG Zhefeng. Fabrication of Mg-Based Composites Reinforced by SiC Whisker Scaffolds with Three-Dimensional Interpenetrating-Phase Architecture and Their Mechanical Properties[J]. 金属学报, 2022, 58(7): 857-867.
[13] ZHENG Shijian, YAN Zhe, KONG Xiangfei, ZHANG Ruifeng. Interface Modifications on Strength and Plasticity of Nanolayered Metallic Composites[J]. 金属学报, 2022, 58(6): 709-725.
[14] PAN Chengcheng, ZHANG Xiang, YANG Fan, XIA Dahai, HE Chunnian, HU Wenbin. Corrosion and Cavitation Erosion Behavior of GLNN/Cu Composite in Simulated Seawater[J]. 金属学报, 2022, 58(5): 599-609.
[15] WANG Haowei, ZHAO Dechao, WANG Mingliang. A Review of the Corrosion Protection Technology on In SituTiB2/Al Composites[J]. 金属学报, 2022, 58(4): 428-443.
No Suggested Reading articles found!