DIFFUSION-CONTROLLED PHASE TRANSFORMATIONS OF Al_(65)Cu_(20)Cr_(15) QUASICRYSTALLINE PARTICLES/AI MATRIX COMPOSITES |
QI Yuhong;ZHANG Zhanping;HEI Zukun (Institute of Metal and Technology; Dalian Maritime University; Dalian 116026)QUAN Mingliu (Institute of Metal Research; The Chinese Academy of Sciences; Shenyang 110015)DONG Chuang (Dalian University of Technology; 116024) |
|
Cite this article:
QI Yuhong;ZHANG Zhanping;HEI Zukun (Institute of Metal and Technology; Dalian Maritime University; Dalian 116026)QUAN Mingliu (Institute of Metal Research; The Chinese Academy of Sciences; Shenyang 110015)DONG Chuang (Dalian University of Technology; 116024). DIFFUSION-CONTROLLED PHASE TRANSFORMATIONS OF Al_(65)Cu_(20)Cr_(15) QUASICRYSTALLINE PARTICLES/AI MATRIX COMPOSITES. Acta Metall Sin, 1998, 34(1): 19-23.
|
Abstract Diffuse phase transformations of A165Cu20Cr15 quasicrystalline particles/AI composite were studied by TEM for the first time. It shows that SIQC quasicrystalline particles transform into FIQC, (DQC+DA)+θand θ phases respectively at the different hot press temperatures of 600, 650 and 700 ℃. During diffusion-controlled phase transformation, SIQC phase transforms through the transitional FIQC, DQC, DA phase to the stable θ phase.
|
Received: 18 January 1998
|
1 Shechtman D, Blech I,Cahn J W.Phys Rev Lett;1984;53:1951 2 Kang S S,Dubois J M J Mater Res,1993; 8:2471 3 Tsai A P, Aoki K;Inove A.Masumoto T J Mater Res.1993;8:5 4 齐育红.张占平.黑祖昆,严立.摩擦学学报,1997;待发表(Qi Yuhong,Zhang Zhanping;Hei Zukun,Yan Li.Tribology;1997,to be published) 5 Bondersky L.Phys Rev Lett,1985; 54: 2422 6 Selke H; Ryder P L Mater Sci Eng, 1993; A165: 81 |