| FATIGUE LIVES OF GRAIN BOUNDARY AND COMPONENT CRYSTALS IN A COPPER BICRYSTAL |
| ZHANG Zhefeng; LI Guangyi; WANG Zhongguang; LI Shouxin (State Key Laboratory of Fatigue and Fracture of Materials; Institute of Metal Research; The Chinese Academy of Sciences; Shenyang 110015) |
|
Cite this article:
ZHANG Zhefeng; LI Guangyi; WANG Zhongguang; LI Shouxin (State Key Laboratory of Fatigue and Fracture of Materials; Institute of Metal Research; The Chinese Academy of Sciences; Shenyang 110015). FATIGUE LIVES OF GRAIN BOUNDARY AND COMPONENT CRYSTALS IN A COPPER BICRYSTAL. Acta Metall Sin, 1998, 34(1): 51-56.
|
|
|
Abstract Cyclic tension-tension deformation was carried out on a copper bicrystal which consists of a single and a double slip oriented component crystal. The grain boundary of the bicrystal is nearly perpendicular to the stress axis during cyclic deformation. The S-N curves of grain boundary and component crystals were respectively determined. By comparison of fatigue lives between component crystals and grain boundary, it was found that the fatigue lives of grain boundary were lower than those of component crystals, however, the fatigue lives of two component crystals showed no obvious difference under the same cyclic stress. Surface observation by SEM indicated that the probability of initiating fatigue cracks in copper bicrystal increased in the order of double, single slip oriented component crystals and grain boundary under the same cyclic load amplitude.
|
|
Received: 18 January 1998
|
1 Wood W A.Philos Mag,1958;3:692 2 Cottrell A H, Hull D. Proc R Soc London,1957;A242:211 3 Tanaka K,Mura T J Appl Mech.1981; 48:97 4 Gueroa J C,Laird C.Mater Sci Eng,1983;60A:45 5 Kim W H,Laird C Acta Metall,1978; 26:777 6 Lim L C Acta Metall,1987;35:1653 7 Mughrabi Herz K,Stark X.Int J Fract,1981;17:193 8 Boettner R C,McEvily A J,Liu Y C Philos Mag, 1964;10:95 9 Essmann U,Gosele U,Mughrabi H.Philos Mag,1981,44:406 10 Ma B-T,Laird C. Acta Metall;1989;37:325 11 Hunsche A, Neumenn P Acta Metall.1986;34:207 12 Laird C.MaLer Sci Eng.1976 22:231 13 Kettunen P,Philos Mag,1966;14: 421] |