EFFECT OF COLD ROLLING ON THE KINETICS OF δ PHASE PRECIPITATION IN INCONEL 718
LIU Wenchang; CHEN Zonglin; XIAO Furen; YAO Mei; WANG Shaogang;LIU Runguang(College of Material Engineering; Yanshan University; Qinhuangdao 066004);(Shenyang Liming Engine Manufacturing Company; Shenyang 110043);(School of Materials Engineering; Harbin Institute of Technology; Harbin 150001)Correspondent:LIU Wenchang;associate professor; Tel: (0335)8057047
Cite this article: 

LIU Wenchang; CHEN Zonglin; XIAO Furen; YAO Mei; WANG Shaogang;LIU Runguang(College of Material Engineering; Yanshan University; Qinhuangdao 066004);(Shenyang Liming Engine Manufacturing Company; Shenyang 110043);(School of Materials Engineering; Harbin Institute of Technology; Harbin 150001)Correspondent:LIU Wenchang;associate professor; Tel: (0335)8057047. EFFECT OF COLD ROLLING ON THE KINETICS OF δ PHASE PRECIPITATION IN INCONEL 718. Acta Metall Sin, 1998, 34(10): 1049-1054.

Download:  PDF(465KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The mass percentages of δ phase in Inconel 718 cold rolled to different reductionsand then treated at different temperatures for different times were measured by X-ray diffraction,and the effect of cold rolling on the kinetics of δ phase precipitation was investigated. Therelationship between the mass percentage of δ phase and annealing time follows the Avramiequation. At 960℃, cold rolling has a little effect on the time exponent (n) and the rate constantof δ phase (α). Below 910 ℃, as cold rolling reduction and annealing temperature increases, theValue of n decreases, whereas the value of or increases. The relationship between the rate constantof δ phase and temperature follows Arrhenius equation. As cold roiling reduction increases,the apparent activation energy of δ precipitation decreases. Cold rolling promotes the γ" → δtransformation. According to the kinetics of δ precipitation, the precipitation-temperature-time(PTT) curves of δphase were given.It has been found that the C curve shifts left as cold rolling reduction increases.
Key words:  Inconel 718      cold rolling      δphase      precipitation kinetics     
Received:  18 October 1998     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1998/V34/I10/1049

1 Desvallees Y, Bouzidi M, Bois F, Beaude N. In: Loria E A ed., Superallous 718, 706 and Various Derivatives,Warrendale, PA: TMS, 1994: 281
2 Pieraggi B, Uginet J F. In: Loria E A ed., Supenalloys 718, 625, 706 and Various Derivatives, Warrendale,PA: TMS, 1994: 535
3 Kirman I, Warrington D H. Metoll Trans, 1970; 1: 2667
4 Sundararaman M, Mukhopadhya P, Banerjee S. Metall Trans, 1988; 19A: 453
5 Dong J X, Xie X S, Xu Z C, Zhang S H. In: Loria E A ed., Supenalloys 718, 625 and Varions Derivatives,Warrendale, PA: TMS, 1994: 649
6 Burger J L, Biederman R R, Couts W H. In: Loria E A ed., Speralloy 718-Metallurgy and Applications,Warrendale, PA: TMS, 1989: 207
7 Singh R P, Hyzak J M, Howon T E, Biederman R R. In: Loria E A ed., Sweralloys 718, 625 and VariousDerivatives, Warrendale, PA: TMS, 1991: 205
8 Liu W C, Xiao P R, Yao M, Chen Z L. Scr Mater, 1997; 37: 53
9 刘文昌,姚枚,肖福仁, 陈宗霖.钢铁, 1997; 32(5): 55(Liu W C, Yao M, Xiao F R, Chen Z L. Iron Steel, 1997; 32(5): 55)
10 Liu W C, Xiao F R, Yao M, Chen Z L. J Mater Sci Lett, 1997; 16: 769
11 草开 清志,早川到,大 耕之.铁钢, 1993; 79: 1210(Kusabiraki K, Hayhawa I, Ooka T. Tetsuo Hagane, 1993; 79: 1210)
12 草开清志,新家伸一,大耕之.铁 钢. 1992; 78: 650(Kusabiraki K, Araie S, Ooka T. Tetsuo Hapane, 1992; 78: 650)
[1] WANG Zhoutou, YUAN Qing, ZHANG Qingxiao, LIU Sheng, XU Guang. Microstructure and Mechanical Properties of a Cold Rolled Gradient Medium-Carbon Martensitic Steel[J]. 金属学报, 2023, 59(6): 821-828.
[2] WANG Changsheng, FU Huadong, ZHANG Hongtao, XIE Jianxin. Effect of Cold-Rolling Deformation on Microstructure, Properties, and Precipitation Behavior of High-Performance Cu-Ni-Si Alloys[J]. 金属学报, 2023, 59(5): 585-598.
[3] XU Lei, TIAN Xiaosheng, WU Jie, LU Zhengguan, YANG Rui. Microstructure and Mechanical Properties of Inconel 718 Powder Alloy Prepared by Hot Isostatic Pressing[J]. 金属学报, 2023, 59(5): 693-702.
[4] YU Shaoxia, WANG Qi, DENG Xiangtao, WANG Zhaodong. Preparation and Size Effect of GH3600 Nickel-Based Superalloy Ultra-Thin Strips[J]. 金属学报, 2023, 59(10): 1365-1375.
[5] REN Ping, CHEN Xingpin, WANG Cunyu, YU Feng, CAO Wenquan. Effects of Pre-Strain and Two-Step Aging on Microstructure and Mechanical Properties of Fe-30Mn-11Al-1.2C Austenitic Low-Density Steel[J]. 金属学报, 2022, 58(6): 771-780.
[6] TANG Yanbing, SHEN Xinwang, LIU Zhihong, QIAO Yanxin, YANG Lanlan, LU Daohua, ZOU Jiasheng, XU Jing. Corrosion Behaviors of Selective Laser Melted Inconel 718 Alloy in NaOH Solution[J]. 金属学报, 2022, 58(3): 324-333.
[7] TANG Shuai, LAN Huifang, DUAN Lei, JIN Jianfeng, LI Jianping, LIU Zhenyu, WANG Guodong. Co-Precipitation Behavior in Ferrite Region During Isothermal Process in Ti-Mo-Cu Microalloyed Steel[J]. 金属学报, 2022, 58(3): 355-364.
[8] LI Yamin, ZHANG Yaoyao, ZHAO Wang, ZHOU Shengrui, LIU Hongjun. First-Principles Study on the Effect of Cu on Nb Segregation in Inconel 718 Alloy[J]. 金属学报, 2022, 58(2): 241-249.
[9] WANG Wenquan, WANG Suyu, CHEN Fei, ZHANG Xinge, XU Yuxin. Microstructure and Mechanical Properties of TiN/Inconel 718 Composites Fabricated by Selective Laser Melting[J]. 金属学报, 2021, 57(8): 1017-1026.
[10] XU Kun, WANG Haichuan, KONG Hui, WU Zhaoyang, ZHANG Zhan. Precipitation Kinetics of Al3Sc in Aluminum Alloys Modeled with a New Grouping Cluster Dynamics Model[J]. 金属学报, 2021, 57(6): 822-830.
[11] Chunbo LAN,Jianeng LIANG,Yuanxia LAO,Dengfeng TAN,Chunyan HUANG,Xianzhong MO,Jinying PANG. Anomalous Thermal Expansion Behavior of Cold-RolledTi-35Nb-2Zr-0.3O Alloy[J]. 金属学报, 2019, 55(6): 701-708.
[12] Houlong LIU,Mingyu MA,Lingling LIU,Liangliang WEI,Liqing CHEN. Effect of Hot Band Annealing Processes on Texture and Formability of 19Cr2Mo1W Ferritic Stainless Steel[J]. 金属学报, 2019, 55(5): 566-574.
[13] Lina WANG, Ping YANG, Kai LI, Feng'e CUI, Weimin MAO. Phase Transformation and Texture Evolution During Cold Rolling and α'-M Reversion in High Manganese TRIP Steel[J]. 金属学报, 2018, 54(12): 1756-1766.
[14] Yongchang LIU, Hongjun ZHANG, Qianying GUO, Xiaosheng ZHOU, Zongqing MA, Yuan HUANG, Huijun LI. Microstructure Evolution of Inconel 718 Superalloy During Hot Working and Its Recent Development Tendency[J]. 金属学报, 2018, 54(11): 1653-1664.
[15] Yutian DING,Yubi GAO,Zhengyi DOU,Xin GAO,Dexue LIU,Zhi JIA. Precipitation Behavior of δ Phase of Deformation Induced GH3625 Superalloy Hot-Extruded Tube[J]. 金属学报, 2017, 53(6): 695-702.
No Suggested Reading articles found!