| EFFECT OF COLD ROLLING ON THE KINETICS OF δ PHASE PRECIPITATION IN INCONEL 718 |
| LIU Wenchang; CHEN Zonglin; XIAO Furen; YAO Mei; WANG Shaogang;LIU Runguang(College of Material Engineering; Yanshan University; Qinhuangdao 066004);(Shenyang Liming Engine Manufacturing Company; Shenyang 110043);(School of Materials Engineering; Harbin Institute of Technology; Harbin 150001)Correspondent:LIU Wenchang;associate professor; Tel: (0335)8057047 |
|
Cite this article:
LIU Wenchang; CHEN Zonglin; XIAO Furen; YAO Mei; WANG Shaogang;LIU Runguang(College of Material Engineering; Yanshan University; Qinhuangdao 066004);(Shenyang Liming Engine Manufacturing Company; Shenyang 110043);(School of Materials Engineering; Harbin Institute of Technology; Harbin 150001)Correspondent:LIU Wenchang;associate professor; Tel: (0335)8057047. EFFECT OF COLD ROLLING ON THE KINETICS OF δ PHASE PRECIPITATION IN INCONEL 718. Acta Metall Sin, 1998, 34(10): 1049-1054.
|
|
|
Abstract The mass percentages of δ phase in Inconel 718 cold rolled to different reductionsand then treated at different temperatures for different times were measured by X-ray diffraction,and the effect of cold rolling on the kinetics of δ phase precipitation was investigated. Therelationship between the mass percentage of δ phase and annealing time follows the Avramiequation. At 960℃, cold rolling has a little effect on the time exponent (n) and the rate constantof δ phase (α). Below 910 ℃, as cold rolling reduction and annealing temperature increases, theValue of n decreases, whereas the value of or increases. The relationship between the rate constantof δ phase and temperature follows Arrhenius equation. As cold roiling reduction increases,the apparent activation energy of δ precipitation decreases. Cold rolling promotes the γ" → δtransformation. According to the kinetics of δ precipitation, the precipitation-temperature-time(PTT) curves of δphase were given.It has been found that the C curve shifts left as cold rolling reduction increases.
|
|
Received: 18 October 1998
|
1 Desvallees Y, Bouzidi M, Bois F, Beaude N. In: Loria E A ed., Superallous 718, 706 and Various Derivatives,Warrendale, PA: TMS, 1994: 281 2 Pieraggi B, Uginet J F. In: Loria E A ed., Supenalloys 718, 625, 706 and Various Derivatives, Warrendale,PA: TMS, 1994: 535 3 Kirman I, Warrington D H. Metoll Trans, 1970; 1: 2667 4 Sundararaman M, Mukhopadhya P, Banerjee S. Metall Trans, 1988; 19A: 453 5 Dong J X, Xie X S, Xu Z C, Zhang S H. In: Loria E A ed., Supenalloys 718, 625 and Varions Derivatives,Warrendale, PA: TMS, 1994: 649 6 Burger J L, Biederman R R, Couts W H. In: Loria E A ed., Speralloy 718-Metallurgy and Applications,Warrendale, PA: TMS, 1989: 207 7 Singh R P, Hyzak J M, Howon T E, Biederman R R. In: Loria E A ed., Sweralloys 718, 625 and VariousDerivatives, Warrendale, PA: TMS, 1991: 205 8 Liu W C, Xiao P R, Yao M, Chen Z L. Scr Mater, 1997; 37: 53 9 刘文昌,姚枚,肖福仁, 陈宗霖.钢铁, 1997; 32(5): 55(Liu W C, Yao M, Xiao F R, Chen Z L. Iron Steel, 1997; 32(5): 55) 10 Liu W C, Xiao F R, Yao M, Chen Z L. J Mater Sci Lett, 1997; 16: 769 11 草开 清志,早川到,大 耕之.铁钢, 1993; 79: 1210(Kusabiraki K, Hayhawa I, Ooka T. Tetsuo Hagane, 1993; 79: 1210) 12 草开清志,新家伸一,大耕之.铁 钢. 1992; 78: 650(Kusabiraki K, Araie S, Ooka T. Tetsuo Hapane, 1992; 78: 650) |
| No Suggested Reading articles found! |
|
|