THERMODYNAMIC AND KINETIC ANALYSIS OF IN SITU SYNTHESIS OF MoSi_2-SiC COMPOSITE
ZHANG Laiqi;SUN Zuqing;ZHANG Yue;YANG Wangyue(State Key Laboratory of Advanced Metal Materials; University of Science & Technology Beijing; Beijing 100083)
Cite this article:
ZHANG Laiqi;SUN Zuqing;ZHANG Yue;YANG Wangyue(State Key Laboratory of Advanced Metal Materials; University of Science & Technology Beijing; Beijing 100083). THERMODYNAMIC AND KINETIC ANALYSIS OF IN SITU SYNTHESIS OF MoSi_2-SiC COMPOSITE. Acta Metall Sin, 1998, 34(11): 1205-1209.
Abstract On the basis of the thermodynamic calculation,XRD and DTA measurements, in view of thermodynamics and kinetics, the phase formation involved in the processing of reactively in situ reactive synthesis of MoSi2-SiC composites are systematically analyzed. Proper heating rate, sintering temperature, and sintering time are recommended.
1 Sadananda K, Jones H,Feng J.Ceram Eng Sci Proc,1991;12(9-10):1671 2 David H,Carter G H.Hurley.J Am Geram Soc, 1987;70(4):C79 3 Michael J M,Ralph J H.Mater Sci Eng, 1992;A155:19 4 Gac F D, Petrovic J J. JAm Ceram Soc,1985;68:C200 5 Petrovic J J,Honnel R E.Ceram Eng Sci Proc,1990;11:734 6 Petrovic J J,Honnel R E.J Mater Sci, 1990;25:4453 7 Henager C H,Jr,Brimhall J L,Brush L N.Mater Sci Eng,1995;A155:65 8 Aiken R M,Ceram J R.Eng Sci Proc,1991;12(9-10):1643 9 Alman D E,Stoloff N S.Scri Metall Mater,1993;28:1525 10 Darken L S,Gurry R W.Physical Chemistry of Metals, New York,NY:MC Graw-Hill,1953 11 Seetharama C D.Mater Sci Eng,1992;A149:241H