| THE PRODUCTION OF SINGLE CRYSTAL OF BINARY NiAl INTERMETALLIC COMPOUND |
| ZHANG Wanming; HU Zhuangqi; ZHENG Qi; YU Yang; TANG Yajun; GUAN Hengrong (Institute of Metal Research; The Chinese Academy of Sciences; Shenyang 110015) |
|
Cite this article:
ZHANG Wanming; HU Zhuangqi; ZHENG Qi; YU Yang; TANG Yajun; GUAN Hengrong (Institute of Metal Research; The Chinese Academy of Sciences; Shenyang 110015). THE PRODUCTION OF SINGLE CRYSTAL OF BINARY NiAl INTERMETALLIC COMPOUND. Acta Metall Sin, 1998, 34(5): 517-520.
|
|
|
Abstract On a small directionally solidified equipment, the technique of double directional solidification with opposite direction was used to produce Ni52Al48 single crystals and the growth rates are 15, 30 and 60 mm/h respectively.
|
|
Received: 18 May 1998
|
1Darolia R.J Mater Sci Technol, 1994; 10: 157 2Darolia R.J Met, 1991; 43: 44 3Darolia R. Acta Metall Sin(Engl Lett); 1995; 8: 625 4Darolia R, Lahrman P F, Field R P. Scr Metall Matet 1992; 26: 1007 5 Levit V I,Bul I A,Hu J,Kaufman M J.Scr Metall Mater,1996;30:1925 6胡汉起.金属凝固.北京:冶金工业出版社,1985(Hu Hanqi .The Solidification of Metal.Beijing:Metallurgical Industry Press,1985) |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|