| GEOMETRICAL ANALYSIS ON PLASTIC DEFORMATION OF POLYCRYSTALLINE METALS AND THE ROOM TEMPERATURE PLASTICITY OF TOW-PHASE TiAl-BASE ALLOYS |
| LIANG Wei; YANG Dezhuang( Centre of Testing and Measuring; Taiyuan University of Technologyl Taiyuan 030024)( Harbin Institute of Technology; Harbin 150001)Comspondent: LIANG Wei; prodessor Tel: (0351)6010610 Fax: (0351)6041237 |
|
Cite this article:
LIANG Wei; YANG Dezhuang( Centre of Testing and Measuring; Taiyuan University of Technologyl Taiyuan 030024)( Harbin Institute of Technology; Harbin 150001)Comspondent: LIANG Wei; prodessor Tel: (0351)6010610 Fax: (0351)6041237. GEOMETRICAL ANALYSIS ON PLASTIC DEFORMATION OF POLYCRYSTALLINE METALS AND THE ROOM TEMPERATURE PLASTICITY OF TOW-PHASE TiAl-BASE ALLOYS. Acta Metall Sin, 1998, 34(6): 597-602.
|
|
|
Abstract Geometrical analysis on plastic deformation charateristics of polycrystallineaggregates proved that the total length of dislocation lines that cat through a unit volume is ininverse proportion to the grain size under given deformation strains, while the total length ofdislocstion lines emitted per unit area of grain boundary is independent of grain size. Furthermore, the distortion of grain boundaries was proved to be propotion to the grain size. On thisbasis and combined with the analysis on the deformation mechanisms, the relationships betweenroom temperature elongation and grain size of two--phase Toil--base alloys were established asfollows:
|
|
Received: 18 June 1998
|
1 Mises V R. Z Augew Math Mech, 1928; 8: 161 2 Kelly A. Strong Solids . New York: Oxford University Press,1966: 82 3 Huang S C,Hall E L.Metoll Trans,1991;22A:427 4 Kim Y W, Dimiduck D M.J Mine Met Mater Soc, 1991; 43: 40 5 Liangg W,Li Q,Yang D Z.Acta Metall Sin (Engl Lett 1996;9:272 6 Chan K S,Kim Y W.Metall Trans ,1994;25A:1217 7 梁伟,李强,杨德庄 金属学报,1997;33:292 (Liang W, Li Q, Yang D Z. Acta Metall Sin, 1997; 33: 292) 8 陈明伟,林栋梁,陈达,石建东,邹敦叙,仲增墉 金属学报,1994;30:A416 (Chen M W, Lin D L, Chen D, Shi J D, Zou D X, Zhong Z Y. Acta Mentall Sin, 1994; 30: A416) 9 张继,张志宏.邹敦叙,仲增墉.金属学报,1996;32: 1044 (Zhang J, Zhang Z H, Zou D X, Zhong Z Y. Acta Metall Sin, 1996; 32: 1044) 10 Viswanathan G B, Vasuclevan V K. Scr Metall Matet 1995; 32: 1705 11 Li J C M,Chan Y T.Metall Trans .1970 ;1:1145 12 Chan K S, Kim Y W. Metall Trans, 1993; 24A: 113 13 Chan K S .Scr Metall Mater 1990 ;24::1725 14 Kim Y W.J Mine Met Mater Soc, 1994; 46: 30R |