Please wait a minute...
Acta Metall Sin  1998, Vol. 34 Issue (6): 603-608    DOI:
Current Issue | Archive | Adv Search |
MECHANISM FOR THE OCCURRENCE OF SERRATED FLOW IN Al-Li SINGLE CRYSTALS
TIAN Boohui(Beliing Institute of Aeronautical Materials; Beijing 100095)LI Huanxi; ZHANG Youggang; CHEN Changqi(Beijing University of Aeronautics and Astronautics; Beijing 100083)Corresponent: TIAN Baohui; Tel: (010)62456622-5021 Fax:(010)62456925
Cite this article: 

TIAN Boohui(Beliing Institute of Aeronautical Materials; Beijing 100095)LI Huanxi; ZHANG Youggang; CHEN Changqi(Beijing University of Aeronautics and Astronautics; Beijing 100083)Corresponent: TIAN Baohui; Tel: (010)62456622-5021 Fax:(010)62456925. MECHANISM FOR THE OCCURRENCE OF SERRATED FLOW IN Al-Li SINGLE CRYSTALS. Acta Metall Sin, 1998, 34(6): 603-608.

Download:  PDF(1406KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Strain rate sensitivity varies in a different mariner in Al-Li single crystalsunder different ageing conditions. Stress drops change irregularly with increasing strain andbear no relation to elapsed time for individual serrations. Stress drops and elapsed time duringserrated flow Primarily distribute within their low values under peak aged condition, comparedwith underaged and overaged states. These behaviors may be explained by sheared σ' particlesinducling serrated flow.
Key words:  strain rate sensitivity      stress drop      elapsed time      serrated flow     
Received:  18 June 1998     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1998/V34/I6/603

1 Behnood N, Evans J T. Acta Metall 1989; 37: 687
2 Kumars,Krol J,Pink E.Scr Mater 1996;35:775
3 Ilic N, Drobnjak Dj, Radmilovic V, Jovanovic M T, Markovic D. Ser Mater 1996; 34: 1123
4 田宝辉,李焕喜,张永刚,陈昌麒.金属学报,1997;33:577 (Tian B H, Li H X, Zhang Y G, Chen C Q. Acta Metall Sin, 1997; 33: 577)
5 Kocks U F ,Cook R E,Mulford R A.Acta Metall 1985;33:623
6 McCormick P G. Acto Metall 1972; 20: 351
7 Hong K T, Nam S W. Acta Metal 1989; 37: 31
8 Diego N,Rio J del ,Segers D,Dorkens-Vapraet L,Dorikens M.Phy Rev 19930;B48:6781
9 Harun H J ,McCormick P G ,Acta Metall ,1979;27:155
10 McCormick P G. Acta Metall, 1971; 19: 463
11 Pink E, Grinberg A. Acta Metal 1982; 30: 2153
12 Fujita H, Tanata T. Acta Metall, 1977; 25: 793
13 Kumar S and Pink E.Acta Mater 1997;45:5205
14 Brechet Y ,Estrin Y.Scr Metall Mater 1994;31:185
[1] Yun CAI,Chaoyang SUN,Li WAN,Daijun YANG,Qingjun ZHOU,Zexing SU. STUDY ON THE DYNAMIC RECRYSTALLIZATION SOFTENING BEHAVIOR OF AZ80 MAGNESIUM ALLOY[J]. 金属学报, 2016, 52(9): 1123-1132.
[2] TIAN Chenggang CUI Chuanyong GU Yuefeng SUN Xiaofeng . EFFECT OF SOLUTION TREATMENT ON THE INVERSE DYNAMIC STRAIN AGING OF A Ni–Co BASE SUPERALLOY[J]. 金属学报, 2012, 48(10): 1223-1228.
[3] ZHAO Shuai LI Xiuyan RONG Lijian. SERRATED FLOW IN A FeNi–BASED AUSTENITIC ALLOY[J]. 金属学报, 2011, 47(8): 1017-1021.
[4] LIU Jiangtao;WANG Zhongguang;SHANG Jianku. DEFORMATION BEHAVIORS OF [110] AND [112] ORIENTED β-Sn SINGLE CRYSTALS[J]. 金属学报, 2008, 44(12): 1409-1414.
[5] Cong Wang. PORTEVIN-LE CHATELIER EFFECT OF LA41 MAGNESIUM ALLOYS[J]. 金属学报, 2006, 42(2): 191-194 .
[6] Tian Baohui (Beijing Institute of Aeronautical Materials; Beijing 100095); Li HuanxiZhang Yonggang;Chen Changqi(Beijing University of Aeronautics and Astronautics;Beijing 100083). INFLUENCING FACTORS OF SERRATED FLOW IN Al-Li SINGLE CRYSTALS[J]. 金属学报, 1997, 33(6): 577-582.
[7] TIAN Baohui; ZHANG Yonggang; CHEN Changqi(Beijing University ofAeronautics and Astronautics; Beijing 100083) (Manuscript received 1 995-05- 1 6; in revised form 1 995-08-25). MORPHOLOGY OF SERRATED FLOW OF AI-Li SINGLE CRYSTALS[J]. 金属学报, 1996, 32(3): 249-253.
[8] WU Min;XU Yuehuang;SHEN Gongtian Wuhan University. INFLUENCE OF AGING ON SERRATED FLOW OF LC9 A1 ALLOY[J]. 金属学报, 1991, 27(5): 33-38.
[9] XU Zhensheng;GONG Bo;ZHANG Caibei;LAI Zuhan Northeast University of Technology; Shenyang. EFFECT OF HYDROGEN ON HIGH TEMPERATUREPLASTICITY OF Ti-6Al-4V ALLOY[J]. 金属学报, 1991, 27(4): 26-29.
[10] CUI Jianzhong;MA Longxiang Northeast University of Technology; ShenyangCUI Jianzhong Lecturer;P.O.Box 317;Northpast Uninersity of Technology;Shenyang. CHARACTERISTIC PARAMETERS IN SUPERPLASTIC DEFORMATION[J]. 金属学报, 1988, 24(1): 92-96.
No Suggested Reading articles found!