| BEHAVIOR AND MECHANISM OF HOT WORK-HARDENING FOR 316L STAINLESS STEEL |
| SONG Renbo1); XIANG Jianying1); HOU Dongpo1); REN Peidong2) |
| 1 School of Materials Science and Engineering; University of Science and Technology Beijing; Beijing 100083
2 Technological Center of Jiuquan Iron $\&$ Steel Co. Ltd.; Jiayuguan 735100 |
|
Cite this article:
SONG Renbo XIANG Jianying HOU Dongpo REN Peidong. BEHAVIOR AND MECHANISM OF HOT WORK-HARDENING FOR 316L STAINLESS STEEL. Acta Metall Sin, 2010, 46(1): 57-61.
|
|
|
Abstract The characteristics of hot work-hardening for 316L stainless steel have been systematically studied through high temperature compression tests on the Gleeble-1500 thermal simulation testing machine. According to Ludwik true stress-strain model, the experimental data has been regressed by using nonlinear fitting method, and the $n$ value in Ludwik model, a comprehensive index which reflects the competitive result between work-hardening and softening, has been calculated with Crussard-Jaoul method. The dynamic recrystallization and twinning were observed by OM and TEM. The experiments reveal that 316L stainless steel is easy to work-hardening during hot deformation, and deformation rate can effect nC-J-ε curves and variation law; There is no peak stress on its true stress-strain curves, but partial dynamic recrystallization has occurred during hot working process. This incomplete softening mechanism can't counteract the effect of hot work-hardening, so the true stress-strain curves still rise with deformation increasing; In addition, twinning occurred during hot working is one of the major mechanisms of hot work-hardening.
|
|
Received: 10 July 2009
|
|
|
| [1] ASM, translated by Ma J R, Chen L M. Metals Handbook. Beijing: Machinery Industry Press, 1994: 7
(ASM, 马九荣, 陈立敏译. 金属手册. 北京: 机械工业出版社, 1994: 7)
[2] Wang S T, Yang K, Shan Y Y, Li L F. Acta Metall Sin, 2007; 43: 171
(王松涛, 杨柯, 单以银, 李来风. 金属学报, 2007; 43: 171)
[3] Soussan A, Degallaix S. Mater Sci Eng, 1991; A142: 169
[4] Ludwigson D C, Berger J A. JISI, 1969; 207: 63
[5] Simmons J W. Acta Mater, 1997; 45: 2467
[6] Lan S H, Lee H J, Lee S H. Mater Des, 2009; 30: 3881
[7] Jha B K, Ram A, Sagar D V. J Mater Sci Lett, 1987; 6: 891
[8] Mejia I, Maldonado C, Benito J A. Mater Sci Forum, 2006; 509: 37
[9] Remy L. Metall Trans, 1981; 12A: 387
[10] Karaman I, Sehitoglu H, Maier H J. Acta Mater, 2001; 49: 3919
[11] Poliak E I, Jonas J J. ISIJ Int, 2003; 43: 684
[12] McQueen H J, Yue S, Ryan N D, Fry E. J Mater Process Technol, 1995; 53: 293
[13] Adler P H, Olson G B, Owen W S. Metall Trans, 1985; 17A: 1725 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|