| EVOLUTION OF δ PHASE IN INCONEL 718 ALLOY DURING DELTA PROCESS |
| ZHANG Haiyan; ZHANG Shihong; CHENG Ming |
| Institute of Metal Research; Chinese Academy of Sciences; Shenyang 110016 |
|
Cite this article:
ZHANG Haiyan ZHANG Shihong CHENG Ming. EVOLUTION OF δ PHASE IN INCONEL 718 ALLOY DURING DELTA PROCESS. Acta Metall Sin, 2009, 45(12): 1451-1455.
|
|
|
Abstract Superalloy Inconel 718 is an important material used for aero–engine high temperature turbine disks. The grain refining of Inconel 718 becomes critical because of the improvement in the quality and reliability of aero–engine. Inconel 718 turbine disks are manufactured by multi–stage hot deformation processes, in which the recrystallized grain grows up in next passes. Therefore, it is difficult to obtain a uniform and refined microstructure by recrystallization refining. The δ phase in Inconel 718 can control grain size through the strong pinning effect. Thus, the Delta process (DP) has been applied for the forging of Inconel 718. In this paper, for the DP of Inconel 718, the evolution of δ phase during isothermal compression deformation at temperature of 950℃ and strain rate of 0.005 s−1, was studied by using optical microscope (OM), scanning electron microscope (SEM) and quantitative X–ray diffraction (XRD) technique. The results show that spherical or rod–shaped δ phase particles in the interior of grains precipitated in the aging treatment disappear during the heating and holding time before deformation, and thcontent of δ phase decreases from 8.14% to 7.05%. Dissolution of δ phase occurs during the deformation, and the content of phase decreases from 7.05% to 5.14%. The spheroidization of plate–like or needl–like δ phase takes place due to the effect of deformation and dissolution breakages, and the plate–like or needle-like δ phase transferrs to sphrical or rod–shaped δ phase. In the centre with the largest strain, the plate–like or needle–like δ phase disappears and spherical or rod–shaped δ hase appears in the interior of grains and grain boundais.
|
|
Received: 02 June 2009
|
|
|
| Fund: Supported by National Nature Science Foundation of China (No.50834008) |
| [1] Hiroaki Y, Takeshi H, Tomohisa H, Sachihiro I, Hideaki S. In: C´esar de S´a J M A, Santos A D eds., Proc 9th Int Conf on Numerical Methods in Industrial Processes, Portugal: Porto, 2007: 987
[2] Zhao Y F. Master Thesis, Beijing Research Institute of Mechanical & Electrical Technology, 1999
(赵耀峰. 机械工业部北京机电研究所硕士学位论文, 1999)
[3] Ruiz C, Obabueki A, Gillespie K. In: Antolovich S D, Stusrud R W, MacKay R A, Anton D L, Khan T, Kissinger R D, Klarstrom D L eds, Superalloys 1992, Warrendale, PA: TMS, 1992: 33
[4] Dix AW, Hyzak J M, Singh R . In: Antolovich S D, Stusrud R W, MacKay R A, Anton D L, Khan T, Kissinger R D, Klarstrom D L eds, Superalloys 1992, Warrendale, PA: TMS, 1992: 23
[5] Bhowal P R, Schirra J J. In: Loria E A ed, Superalloys 718, 625, 706 and Various Derivatives, Warrendale, PA: TMS, 2001: 193
[6] Lu H J, Yao C G, Zhang K F, Jia X C. Mater Mechanical Eng, 2003; 27(1): 15
(吕宏军, 姚草根, 张凯峰, 贾新朝. 机械工程材料, 2003; 27(1): 15)
[7] Yuan H, Liu W C. Mater Sci Eng, 2005; A408: 281
[8] Wang Y, Zhen L, Shao W Z, Yang L, Zhang X M. J Alloys Compd, 2009; 44: 341
[9] Schafrik R E, Ward D D, Groh J R. In: Loria E A ed, Superalloys 718, 625, 706 and Various Derivatives, Warrendale, PA: TMS, 2001: 1
[10] Hu J P. PhD Dissertation, Steel Research Institute, Beijing, 1999
(胡建平. 钢铁研究总院博士学位论文, 北京, 1999)
[11] Zhao D, Chaudhury P K. In: Loria E A ed, Superalloys 718, 625, 706 and Various Derivatives, Warrendale, PA: TMS, 1994: 303
[12] Thomas A, El–Wahabi M, Cabrera J M, Prado J M. J Mater Process Technol, 2006; 177: 469
[13] Sundararaman M, Mukhopadhyay P, Banerjee S. In: Loria E A ed, Superalloys 718, 625, 706 and Various Derivatives , Warrendale, PA: TMS, 1994: 419
[14] Desvall´ees Y, Bouzidi M, Bois F, Beaude N. In: Loria E A ed, Superalloys 718, 625, 706 and Various Derivatives, Warrendale, PA: TMS, 1994: 281
[15] Cai D Y, Zhang W H, Liu W C, Yao M, Sun G D, Chen Z L, Wang S G, Gao Y K. J Iron Steel Res, 2002; 14(6):61
(蔡大勇, 张伟红, 刘文昌, 姚枚, 孙贵东, 陈宗霖, 王少刚, 高玉魁. 钢铁研究学报, 2002, 14(6): 61)
[16] Pan J S, Tong J M, Tian J M. Fundamentals of Material Science. Beijing: Tsinghua University Press, 2002: 473
(潘金生, 仝健民, 田健民. 材料科学基础. 北京: 清华大学出版社, 2002: 473) |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|