Acta Metall Sin  2009, Vol. 45 Issue (11): 1384-1389    DOI:
论文 Current Issue | Archive | Adv Search |
CORROSION BEHAVIORS OF Ni BASE SOLID SOLUTION-TOUGHENED Cr13Ni5Si2 ALLOY IN Cl- CONTAINING SOLUTIONS
YUAN Lei; WANG Huaming
Laboratory of Laser Materials Processing and Manufacturing; School of Materials Science and Engineering; Beihang University; Beijing 100191
Cite this article: 

YUAN Lei WANG Huaming. CORROSION BEHAVIORS OF Ni BASE SOLID SOLUTION-TOUGHENED Cr13Ni5Si2 ALLOY IN Cl- CONTAINING SOLUTIONS. Acta Metall Sin, 2009, 45(11): 1384-1389.

Download:  PDF(1079KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  

From the application point of view, corrosion resistance of materials in corrosive environments, especially in Cl- containing medium, has great significance when used as mechanical components serving in marine and other aggressive environments. The corrosion behavior of a material is largely controlled by the presence or absence of protective surface film, which may act as a protective barrier against corrosion attacks. Therefore, the corrosion resistance of an alloy is closely related to the particular composition of the passive film and the synergistic interaction between the cations of alloy components in the passive film. In the present study, a γ-toughened Cr13Ni5Si2 metal silicide alloy, consisting of Cr13Ni5Si2, Ni base solid solution $\gamma$ and Cr3Ni5Si2 was designed and fabricated by the introduction melting and die-casting prosess. Corrosion behaviors of the alloy in a series of Na2SO4+NaCl solutions were investigated by anodic polarization, Tafel plot and electrochemical impedance spectroscopy (EIS) experiments. Chemical composition of the passive film and the surface of polarized samples were examined by X-ray photoelectron spectroscopy (XPS) and scanning electron microscopy (SEM), respectively. A commercial solution treated single phase austenitic stainless steel 1Cr18Ni9Ti was selected as the reference material for all the electrochemical tests. Results showed that the metal silicide alloy exhibited high corrosion resistance in all testing solutions due to the formation of a compact and protective passive film composed mainly of Cr2O3, as well as the high chemical stability of Cr13Ni5Si2 and Cr3Ni5Si2 phases. No evidence of localized corrosion occurred even after anodic polarization in 0.1 mol/L Na2SO4+1 mol/L NaCl solution. Moreover, the corrosion potential, breakdown potential and anodic current density are almost invariant with increasing Cl- concentration, which means the alloy has excellent corrosion resistance in neutral Cl- containing solutions.

Key words:  metal silicide      corrosion      polarization curve      Cl- concentration      elecrtochemical impedance spectroscopy (EIS)     
Received:  16 April 2009     
ZTFLH: 

TG174.2

 
Fund: 

Supported by National Science Fund for Distinguished Young Scholars (No.50625413), Cheung Kong Scholars and Innovative Research Team Program in University from Ministry of Education (No.IRT0805) and Innovation Foundation of BUAA for PhD Graduates

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2009/V45/I11/1384

[1] Bateni M R, Szpunar J A, Wang X, Li D Y. Wear, 2006; 260: 116
[2] Batchelor A W, Stachowiak G W. Wear, 1988; 123: 281
[3] Wang H M, Duan G. Intermetallics, 2003; 11: 755
[4] Yuan Y, Wang H M. J Alloys Compd, 2008; 459: 148
[5] Xia Y Q, Hu J H, Zhou F, Lin Y M, Qiao Y L, Xu T. Mater Sci Eng, 2005; A402: 135
[6] Villars P, Prince A, Okamoto H. Handbook of Ternary Alloys Phase Diagrams. New York: ASM International, 1995: 9143
[7] Tang H B, Fang Y L, Wang H M. Acta Mater, 2004; 52: 1773
[8] Xu Y W, Wang H M. Acta Metall Sin, 2006; 42: 722
(徐亚伟, 王华明. 金属学报, 2006; 42: 722)
[9] Yeh C L, Chen W H. J Alloys Compd, 2005; 402: 118
[10] Liu Y, Wang H M. Mater Sci Eng, 2005; A396: 240
[11] Fang Y L, Wang H M. Acta Metall Sin, 2006; 42: 181
(方艳丽, 王华明, 金属学报, 2006; 42: 181)
[12] Fang Y L, Wang H M. Rare Metal Mat Eng, 2007; 36: 690
(方艳丽, 王华明, 稀有金属材料与工程, 2007; 36: 690)
[13] Pardo A, Otero E, Merino M C, L´opez M D, V´azquez M, Agudo P. Corros Sci, 2002; 44: 1193
[14] Liu G Q, Zhu Z Y, Ke W. Acta Metall Sin, 2001; 37: 272
(刘国强, 朱自勇, 柯伟. 金属学报, 2001; 37: 272)
[15] Cai L X, Wang H M, Wang C M. Surf Coat Technol, 2004; 182: 294
[16] Zhang Y Q, Jiang Y H, Zhou R. J Funct Mater, 2006; 37: 1891

(张玉勤, 蒋业华, 周荣. 功能材料, 2006; 37: 1891)

[1] ZHANG Qiliang, WANG Yuchao, LI Guangda, LI Xianjun, HUANG Yi, XU Yunze. Erosion-Corrosion Performance of EH36 Steel Under Sand Impacts of Different Particle Sizes[J]. 金属学报, 2023, 59(7): 893-904.
[2] ZHAO Pingping, SONG Yingwei, DONG Kaihui, HAN En-Hou. Synergistic Effect Mechanism of Different Ions on the Electrochemical Corrosion Behavior of TC4 Titanium Alloy[J]. 金属学报, 2023, 59(7): 939-946.
[3] LI Xiaohan, CAO Gongwang, GUO Mingxiao, PENG Yunchao, MA Kaijun, WANG Zhenyao. Initial Corrosion Behavior of Carbon Steel Q235, Pipeline Steel L415, and Pressure Vessel Steel 16MnNi Under High Humidity and High Irradiation Coastal-Industrial Atmosphere in Zhanjiang[J]. 金属学报, 2023, 59(7): 884-892.
[4] CHEN Runnong, LI Zhaodong, CAO Yanguang, ZHANG Qifu, LI Xiaogang. Initial Corrosion Behavior and Local Corrosion Origin of 9%Cr Alloy Steel in Cl-Containing Environment[J]. 金属学报, 2023, 59(7): 926-938.
[5] SI Yongli, XUE Jintao, WANG Xingfu, LIANG Juhua, SHI Zimu, HAN Fusheng. Effect of Cr Addition on the Corrosion Behavior of Twinning-Induced Plasticity Steel[J]. 金属学报, 2023, 59(7): 905-914.
[6] WANG Zongpu, WANG Weiguo, Rohrer Gregory S, CHEN Song, HONG Lihua, LIN Yan, FENG Xiaozheng, REN Shuai, ZHOU Bangxin. {111}/{111} Near Singular Boundaries in an Al-Zn-Mg-Cu Alloy Recrystallized After Rolling at Different Temperatures[J]. 金属学报, 2023, 59(7): 947-960.
[7] WU Xinqiang, RONG Lijian, TAN Jibo, CHEN Shenghu, HU Xiaofeng, ZHANG Yangpeng, ZHANG Ziyu. Research Advance on Liquid Lead-Bismuth Eutectic Corrosion Resistant Si Enhanced Ferritic/Martensitic and Austenitic Stainless Steels[J]. 金属学报, 2023, 59(4): 502-512.
[8] WANG Jingyang, SUN Luchao, LUO Yixiu, TIAN Zhilin, REN Xiaomin, ZHANG Jie. Rare Earth Silicate Environmental Barrier Coating Material: High-Entropy Design and Resistance to CMAS Corrosion[J]. 金属学报, 2023, 59(4): 523-536.
[9] HAN En-Hou, WANG Jianqiu. Effect of Surface State on Corrosion and Stress Corrosion for Nuclear Materials[J]. 金属学报, 2023, 59(4): 513-522.
[10] XU Linjie, LIU Hui, REN Ling, YANG Ke. Effect of Cu on In-Stent Restenosis and Corrosion Resistance of Ni-Ti Alloy[J]. 金属学报, 2023, 59(4): 577-584.
[11] CHANG Litao. Corrosion and Stress Corrosion Crack Initiation in the Machined Surfaces of Austenitic Stainless Steels in Pressurized Water Reactor Primary Water: Research Progress and Perspective[J]. 金属学报, 2023, 59(2): 191-204.
[12] LIAO Jingjing, ZHANG Wei, ZHANG Junsong, WU Jun, YANG Zhongbo, PENG Qian, QIU Shaoyu. Periodic Densification-Transition Behavior of Zr-Sn-Nb-Fe-V Alloys During Uniform Corrosion in Superheated Steam[J]. 金属学报, 2023, 59(2): 289-296.
[13] XIA Dahai, JI Yuanyuan, MAO Yingchang, DENG Chengman, ZHU Yu, HU Wenbin. Localized Corrosion Mechanism of 2024 Aluminum Alloy in a Simulated Dynamic Seawater/Air Interface[J]. 金属学报, 2023, 59(2): 297-308.
[14] HU Wenbin, ZHANG Xiaowen, SONG Longfei, LIAO Bokai, WAN Shan, KANG Lei, GUO Xingpeng. Corrosion Behavior of AlCoCrFeNi2.1 Eutectic High-Entropy Alloy in Sulfuric Acid Solution[J]. 金属学报, 2023, 59(12): 1644-1654.
[15] SONG Jialiang, JIANG Zixue, YI Pan, CHEN Junhang, LI Zhaoliang, LUO Hong, DONG Chaofang, XIAO Kui. Corrosion Behavior and Product Evolution of Steel for High-Speed Railway Bogie G390NH in Simulated Marine and Industrial Atmospheric Environment[J]. 金属学报, 2023, 59(11): 1487-1498.
No Suggested Reading articles found!