| ANISOTROPIC CREEP IN A Ni-BASED SINGLE CRYSTAL SUPERALLOY |
| JIA Yuxian1;2); JIN Tao1); LIU Jinlai1); SUN Xiaofeng1); HU Zhuangqi1); |
1) Institute of Metal Research; Chinese Academy of Sciences; Shenyang 110016
2) School of Materials Science and Engineering; Shenyang Ligong University; Shenyang 110168 |
|
Cite this article:
JIA Yuxian JIN Tao LIU Jinlai SUN Xiaofeng HU Zhuangqi. ANISOTROPIC CREEP IN A Ni-BASED SINGLE CRYSTAL SUPERALLOY. Acta Metall Sin, 2009, 45(11): 1364-1369.
|
|
|
Abstract Constant load creep tests were performed on the [001] and [011] oriented Ni-Co-Cr-Mo-W-Al-Ti-Ta single crystal superalloys. The [001] oriented alloy has much longer creep life than that of [011] oriented alloy, but the elongation of [011] oriented alloy is slightly higher under the condition of 750 ℃/750 MPa. The average creep life and elongation of [001] oriented alloy are both higher than that of [011] oriented alloy at 982 ℃/248 MPa, and the anisotropy occurs mainly during the accelerating creep stage, but anisotropic degree decreases obviously. The SEM analysis revealsγ ´phases are rafted in the two directions, which blocks the glide/climb of dislocations and causes creep hardening, the rafting of γ´ phase is the dominant reason to decrease of creep anisotropy at higher temperature. The TEM observation indicates deformation twins formed in [011] oriented alloy, which lowers the plasticity of the sample and induces the sample to fracture rapidly.
|
|
Received: 18 March 2009
|
|
|
| Fund: Supported by National Natural Science Foundation of China (No.50931004) |
| [1] Leverant G R, Kear B H. Metall Trans, 1970; 1: 491
[2] Caron P, Ohta Y, Nakagawa Y G, Khan T. In: Duhl D N, Maurer G, Antolovich S, Lund C, Reichman S, eds., Superalloys 1988, Warrendale: The Metallurgical Society, 1988: 215
[3] Peng Z F, Yan Y H. Acta Metall Sin, 1997; 33: 1147
(彭志方, 严演辉. 金属学报, 1997; 33: 1147)
[4] Sass V, Feller–Kniepmeier M. Mater Sci Eng, 1998; A245: 19
[5] MacKay R A, Maier R D. Matall Trans, 1982; 13: 1747
[6] Liu J L, Jin T, Sun X F, Zhang J H, Guan H R, Hu Z Q. Mater Sci Eng, 2008; A479: 277
[7] Kakehi K. Metall Mater Trans, 1999; 30A: 1249
[8] Knowles D M, Chen Q Z. Mater Sci Eng, 2003; A340: 88
[9] Ardakain M G, McLean M, Shollock B A. Acta Mater, 1999; 47: 2593
[10] Matan N, Cox D C, Rist M A, Rae C M F, Reed R C. Acta Mater, 1999; 47: 1549
[11] Knowles D M, Gunturi S. Mater Sci Eng, 2002; A328: 223
[12] Fredholm A, Strudel J L. In: Gell M, Kortovich C S, Bricknell R H, Kent W B, Radavich J F, eds., Superalloys 1984, Warrendale: AIME, 1984: 211
[13] Feller–Kniepmeier M, Kuttner T. Acta Metall Mater, 1994; 42: 3167
[14] Shui L. PhD Thesis, Shenyang University of Technology, 2006
(水丽. 沈阳工业大学博士学位论文, 2006)
[15] Chen Q Z, Knowles D M. Mater Sci Eng, 2003; A356: 352 |