STUDY ON MICROSTRUCTURES AND AGING CHARACTERISTICS OF 7050 ALUMINUM ALLOY PLATE EXTRUDED FROM LOW FREQUENCY ELECTROMAGNETIC CASTING INGOT
Zhihao Zhao;;;
东北大学材料电磁过程教育部重点实验室
Cite this article:
Zhihao Zhao. STUDY ON MICROSTRUCTURES AND AGING CHARACTERISTICS OF 7050 ALUMINUM ALLOY PLATE EXTRUDED FROM LOW FREQUENCY ELECTROMAGNETIC CASTING INGOT. Acta Metall Sin, 2007, 43(9): 949-955 .
Abstract The microstructures and aging characteristics of 7050 aluminum alloy plates extruded from low frequency electromagnetic casting and DC casting ingots have been studied. The results show that the plate extruded from LFEC ingot has a fine microstructure. After a constant extrusion process, the average diameter of grains of the plate extruded from LFEC ingot is about 10μm, and the plate extruded from DC ingot is about 20μm. Comparing with plate extruded from DC ingot, the plate extruded from LFEC ingot has a fast aging rate and much stronger ability of aging strengthening. Aging at 120℃, the plate extruded from LFEC ingot reaches its peak strength in 8 hours, and its longitudinal and the transverse strength are 656MPa and 596MPa respectively. However, the plate extruded from DC ingot reaches its the maximum value in 12 hours and its longitudinal and the transverse strength are 647MPa and 590MPa respectively.
[1]Zhang B J,Cui J Z.Mater Sci Eng,2003;A355:325 [2]Zhang B J,Cui J Z,Lu G M,Zhang Q,Ban C Y.Acta Metall Sin,2002;38:215 (张北江,崔建忠,路贵民,张勤,班春燕.金属学报,2002;38:215) [3]Zhang B J,Cui J Z,Lu G M.Mater Lett,2003;57:1707 [4]Dong J,Cui J Z.Metall Mater Trans,2004;35A:2487 [5]Dong J,Liu X T,Zhao Z H,Bao W P,Cui J Z.Acta Metall Sin,2004;40:215 (董杰,刘晓涛,赵志浩,包卫平,崔建忠.金属学报,2004;40:215) [6]Zuo Y B,Cui J Z,Dong J,Yu F X.J Alloy Compd,2005; 402:149 [7]Zuo Y B,Cui J Z,Dong J.Mater Sci Eng,2005;A408: 176 [8]Vives C.Metall Trans,1989;20B:623 [9]Dong J,Cui J Z,Zeng X Q,Ding W J.Mater Lett,2005; 59:1502 [10]Jia F,Jin J Z.Acta Metall Sin,2002;38:393 (贾非,金俊泽.金属学报,2002;38:393)