EFFECT OF HOMOGENIZATION TREATMENT ON THE MICROSTRUCTURES OF LOW FREQUENCY ELECTROMAGNETIC CASTING 7050 ALUMINUM ALLOY
Zhihao Zhao;;;
东北大学材料电磁过程教育部重点实验室
Cite this article:
Zhihao Zhao. EFFECT OF HOMOGENIZATION TREATMENT ON THE MICROSTRUCTURES OF LOW FREQUENCY ELECTROMAGNETIC CASTING 7050 ALUMINUM ALLOY. Acta Metall Sin, 2007, 43(9): 956-960 .
Abstract The 7050 aluminum alloy ingot with fine microstructure was cast by low frequency electromagnetic casting (LFEC) process. The homogenization treatment behaviors of LFEC ingot were investigated experimentally. The results show that the ingots cast with low frequency electromagnetic field has a better homogenization effect than conventional DC ingot. Under the same homogenization condition, the LFEC ingot has fewer low melting point phase between grains and more solute elements inside grains. After homogenized for 12 hours the LFEC ingots can reach the average percentage of the alloy elements, but the DC ingots haven’t reach it until for 48 hours.
LI Gang;WANG Zhongguang(State Key Laboratory of Fatigue and Fracture for Materials;Institute of Metal Research; Chinese Academy of Sciences; Shenyang; 110015).GUO Jianting; TAN Minghui;SHI Changxu(Institute of Metal Research; Chinese Academy of Sciences;Shenyang; 110015)(Manuscript received 94-05 -03). ^MECHANICAL PROPERTIES AND MICROSTRUCTURES OF TWO Ni_3Al ALLOYS[J]. 金属学报, 1995, 31(2): 64-68.
[7]
NING Xiuzhen;ZHANG Tianxiang;TONG Yingjie;ZHU Yaoxiao Institute of Metal Research; Academia Sinica; Shenyang. HOMOGENIZATION TREATMENT OF ALLOY GH169[J]. 金属学报, 1989, 25(3): 40-44.