MICROSTRUCTURES AND MECHANICAL PROPERTIES OF Mg-(2, 3, 4)Y-1Zn ALLOYS WITH LONG PERIOD STACKING ORDERED STRUCTURE
LIU Huan, XUE Feng, BAI Jing, ZHOU Jian, SUN Yangshan
Jiangsu Key Lab for Advanced Metallic Materials, College of Materials Science and Engineering, Southeast University,Nanjing 211189
Cite this article: 

LIU Huan, XUE Feng, BAI Jing, ZHOU Jian, SUN Yangshan. MICROSTRUCTURES AND MECHANICAL PROPERTIES OF Mg-(2, 3, 4)Y-1Zn ALLOYS WITH LONG PERIOD STACKING ORDERED STRUCTURE. Acta Metall Sin, 2013, 49(2): 236-242.

Download:  PDF(3188KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  

 

Recently, the Mg-Y-Zn alloy systems have received great attention due to their unique microstructures and excellent mechanical properties. Three kinds of ternary equilibrium Mg-Y-Zn phases have been reported in the systems: the W phase (Mg3Y2Zn3), the I phase (Mg3YZn6) and the X phase (Mg12YZn, long period stacking ordered (LPSO)structure). To further study the evolutions of LPSO structures in Mg-Y-Zn alloys, three Mg-(2, 3, 4)Y-1Zn (atomic fraction, %) ternary alloys were prepared by casting and extrusion. Based on the OM, SEM and TEM observations, the microstructures of the as-cast WZ21 and WZ31 alloys are mainly composed ofα-Mg and Mg12YZn duplex microstructures, while that of the as-cast WZ41 alloy consists of α-Mg,Mg12YZn and Mg24Y5 phases. The Mg12YZn phase which forms a network is a kind of 18R-LPSO structures and the Mg24Y5 phase is inclined to be located within 18R phases. During homogenization treatment, part of 18R phase dissolves and 14H lamellas are precipitated in the matrix of the WZ21 and WZ31 alloys. After extrusion, the 18R phases are aligned along the extrusion direction, whereas the 14H lamellas in the matrix are still parallel to each other. During solution treatment (T4), the 18R structures continue to dissolve and 14H lamellas further develop. With increase of the Y/Zn atomic ratio, the volume fraction of 14H-LPSO phase increases after T4 treatment. The mechanical properties for the extruded alloys are better than alloys in as-cast, as-annealed and T4-treated stages. With increasing Y content, the strength of the alloys increases, but the ductility decreases. Tensile strength of the extruded WZ41 alloy reaches 350 MPa at room temperature.
Key words:  Mg-Y-Zn alloy      long period stacking ordered structure      annealing      extrusion      solution treatment     
Received:  14 September 2012     

URL: 

https://www.ams.org.cn/EN/10.3724/SP.J.1037.2012.00548     OR     https://www.ams.org.cn/EN/Y2013/V49/I2/236

[1] Zhang J H, Leng Z, Liu S J, Li J Q, Zhang M L, Wu R Z. J Alloys Compd, 2011; 509: 7717


[2] Kawamura Y, Hayashi K, Inoue A, Masumoto T. Mater Trans, 2001; 42: 1172

[3] Luo S Q, Tang A T, Pan F S, Song K, Wang W Q. Trans Nonferrous Met Soc China, 2011; 21: 795

[4] Wang J F, Song P F, Gao S, Huang X F, Shi Z Z, Pan F S. Mater Sci Eng, 2011; A528: 5914

[5] Liu K, Zhang J H, Lu H Y, Tang D X, Rokhlin L L, Elkin F M, Meng J. Mater Des, 2010; 31: 210

[6] Zhang S, Yuan G Y, Lu C, Ding W J. J Alloys Compd, 2011; 509: 3515

[7] Yin D D, Wang Q D, Gao Y, Chen C J, Zheng J. J Alloys Compd, 2011; 509: 1696

[8] Abe E, Kawamura Y, Hayashi K, Inoue A. Acta Mater, 2002; 50: 3845

[9] Zheng L, Liu C M, Wan Y C, Yang P W, Shu X. J Alloys Compd, 2011; 509: 8832

[10] Kawamura Y, Kasahara T, Izumi S, Yamasaki M. Scr Mater, 2006; 55: 453

[11] Itoi T, Seimiya T, Kawamura Y, Hirohashi M. Scr Mater, 2004; 51: 107

[12] Li R G, Fang D Q, An J, Lu Y, Cao Z Y, Liu Y B. Mater Charact, 2009; 60: 470

[13] Yamasaki M, Anan T, Yoshimoto S, Kawamura Y. Scr Mater, 2005; 53: 799

[14] Su Z G, Li R G, An J, Lu Y. J Mater Eng Perform, 2010; 19: 70

[15] Chen B, Lin D L, Zeng X Q, Lu C. J Alloys Compd, 2007; 440: 94

[16] Yoshimoto S, Yamasaki M, Kawamura Y. Mater Trans, 2006; 47: 959

[17] Wang J F, Gao S, Song P F, Huang X F, Shi Z Z, Pan F S. J Alloys Compd, 2011; 509: 8567

[18] Chen B, Lin D L, Zeng X Q, Lu C. J Mater Sci, 2010; 45: 2510

[19] Yamasaki M, Sasaki M, Nishijima M, Hiraga K, Kawamura Y. Acta Mater, 2007; 55: 6798

[20] Zhu Y M, Weyland M, Morton A J, Oh-ishi K, Hono K, Nie J F. Scr Mater, 2009; 60: 980

[21] Zhu Y M, Morton A J, Nie J F. Acta Mater, 2010; 58: 2936

[22] Li D J, Zeng X Q, Dong J, Zhai C Q. Trans Nonferrous Met Soc China, 2008; 18: 117

[23] Zeng X Q, Wu Y J, Peng L M, Lin D L, Ding W J, Peng Y H. Acta Matell Sin, 2010; 46: 1041

(曾小勤, 吴玉娟, 彭立明, 林栋樑, 丁文江, 彭赢红. 金属学报, 2010; 46: 1041)

[24] Liu K, Zhang J F, Tang D X, Rokhlin L L, Elkin F M, Meng J. Mater Chem Phys, 2009; 117: 107

[25] Hagihara K, Kinoshita A, Sugino Y, Yamasaki M, Kawamura Y, Yasuda H Y, Umakoshi Y. Acta Mater, 2010; 58: 6282

[26] Shao X H, Yang Z Q, Ma X L. Acta Mater, 2010; 58: 4760
[1] CHEN Xueshuang, HUANG Xingmin, LIU Junjie, LV Chao, ZHANG Juan. Microstructure Regulation and Strengthening Mechanisms of a Hot-Rolled & Intercritical Annealed Medium-Mn Steel Containing Mn-Segregation Band[J]. 金属学报, 2023, 59(11): 1448-1456.
[2] JIN Xinyan, CHU Shuangjie, PENG Jun, HU Guangkui. Effect of Dew Point on Selective Oxidation and Decarburization of 0.2%C-1.5%Si-2.5%Mn High Strength Steel Sheet During Continuous Annealing[J]. 金属学报, 2023, 59(10): 1324-1334.
[3] YU Shaoxia, WANG Qi, DENG Xiangtao, WANG Zhaodong. Preparation and Size Effect of GH3600 Nickel-Based Superalloy Ultra-Thin Strips[J]. 金属学报, 2023, 59(10): 1365-1375.
[4] CHEN Run, WANG Shuai, AN Qi, ZHANG Rui, LIU Wenqi, HUANG Lujun, GENG Lin. Effect of Hot Extrusion and Heat Treatment on the Microstructure and Tensile Properties of Network Structured TiBw/TC18 Composites[J]. 金属学报, 2022, 58(11): 1478-1488.
[5] YANG Ping, WANG Jinhua, MA Dandan, PANG Shufang, CUI Feng'e. Influences of Composition on the Transformation-Controlled {100} Textures in High Silicon Electrical Steels Prepared by Mn-Removal Vacuum Annealing[J]. 金属学报, 2022, 58(10): 1261-1270.
[6] WANG Yu, HU Bin, LIU Xingyi, ZHANG Hao, ZHANG Haoyun, GUAN Zhiqiang, LUO Haiwen. Influence of Annealing Temperature on Both Mechanical and Damping Properties of Nb-Alloyed High Mn Steel[J]. 金属学报, 2021, 57(12): 1588-1594.
[7] LI Suo, CHEN Weiqi, HU Long, DENG Dean. Influence of Strain Hardening and Annealing Effect on the Prediction of Welding Residual Stresses in a Thick-Wall 316 Stainless Steel Butt-Welded Pipe Joint[J]. 金属学报, 2021, 57(12): 1653-1666.
[8] MA Dexin, ZHAO Yunxing, XU Weitai, PI Libo, LI Zhongxing. Surface Effect on Eutectic Structure Distribution in Single Crystal Superalloy Castings[J]. 金属学报, 2021, 57(12): 1539-1548.
[9] LIU Xianfeng, LIU Dong, LIU Renci, CUI Yuyou, YANG Rui. Microstructure and Tensile Properties of Ti-43.5Al-4Nb-1Mo-0.1B Alloy Processed by Hot Canned Extrusion[J]. 金属学报, 2020, 56(7): 979-987.
[10] CAO Tieshan, ZHAO Jinyi, CHENG Congqian, MENG Xianming, ZHAO Jie. Effect of Cold Deformation and Solid Solution Temperature on σ-phase Precipitation Behavior in HR3C Heat Resistant Steel[J]. 金属学报, 2020, 56(5): 673-682.
[11] YAO Xiaofei, WEI Jingpeng, LV Yukun, LI Tianye. Precipitation σ Phase Evoluation and Mechanical Properties of (CoCrFeMnNi)97.02Mo2.98 High Entropy Alloy[J]. 金属学报, 2020, 56(5): 769-775.
[12] CAO Yuhan,WANG Lilin,WU Qingfeng,HE Feng,ZHANG Zhongming,WANG Zhijun. Partially Recrystallized Structure and Mechanical Properties of CoCrFeNiMo0.2 High-Entropy Alloy[J]. 金属学报, 2020, 56(3): 333-339.
[13] ZHANG Yong, LI Xinxu, WEI Kang, WAN Zhipeng, JIA Chonglin, WANG Tao, LI Zhao, SUN Yu, LIANG Hongyan. Hot Deformation Characteristics of Novel Wrought Superalloy GH4975 Extruded Rod Used for 850 ℃ Turbine Disc[J]. 金属学报, 2020, 56(10): 1401-1410.
[14] Lin WEI,Zhijun WANG,Qingfeng WU,Xuliang SHANG,Junjie LI,Jincheng WANG. Effect of Mo Element and Heat Treatment on Corrosion Resistance of Ni2CrFeMox High-Entropy Alloyin NaCl Solution[J]. 金属学报, 2019, 55(7): 840-848.
[15] Wentao LI,Zhenyu WANG,Dong ZHANG,Jianguo PAN,Peiling KE,Aiying WANG. Preparation of Ti2AlC Coating by the Combination of a Hybrid Cathode Arc/Magnetron Sputtering with Post-Annealing[J]. 金属学报, 2019, 55(5): 647-656.
No Suggested Reading articles found!