Experimental study of the characteristic of grain-boundary P segregation in GH4169
XU Ting-dong
钢铁研究总院 高温材料研究所
Cite this article: 

XU Ting-dong. Experimental study of the characteristic of grain-boundary P segregation in GH4169. Acta Metall Sin, 2007, 43(8): 893-896 .

Download:  PDF(378KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  In virtue of Auger electron spectroscopy, it is found that the level of grain-boundary P segregation in GH4169 superalloy increases with the increase in solution treatment temperature. Based on this, the characteristic of NGS of P in superalloy is confirmed for the first time. The confirmation provides new theoretical and experimental basis for understanding the influence of P on mechanical properties of superalloys.
Key words:  grain-boundary      segregation      superalloy      Inconel 718      
Received:  21 December 2006     
ZTFLH:  TG111.2  

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2007/V43/I8/893

[1]Holt R T,Wallace W.Int Met Rev,1976;21:1
[2]Seah M P.Acta Metall,1980;28:955
[3]Bieber C G,Decker R F.Trans AIME,1961;221:629
[4]Was G S,Kruger R M.Acta Metell,1985;33:841
[5]Was G S,Sung J K,Angeliu T M.Metall Trans,1992; 23A:3343
[6]Ohtani H,Feng H C,McMahon C J Jr,Mulford R A. Metall Trans,1976;7A:87
[7]Ohtani H,Feng H C,McMahon C J Jr.Metall Trans, 1976;7A:1123
[8]Lawrence E D,MacDonald N C,Palmberg P W.Handbook of Auger Electron Spectroscopy.Minneapolis,Minnesota: Physical Electronics Industries Press,1983:310
[9]Huang X,Chaturvedi M C,Richards N L,Jackman J. Acta Mater,1997;45:3095
[10]Guttmann M,Dumoulin P,Tan-Tai N,Fontaine P.Cor- rosion,1981;37:416
[11]McLean D.Grain Boundaries in Metals.Oxford:Oxford University Press,1957:118
[12]Xu T D,Cheng B Y.Prog Mater Sci,2004;49:109
[13]Xu T D,Song S H.Acta Metall,1989;37:2499
[14]Xu T D,Song S H,Shi H Z,Gust W,Yuan Z X.Acta Metall Mater,1991;39:3119
[15]Aust K T,Hanneman R E,Niessen P,Westbrook J H. Acta Metall,1968;16:291
[16]Westbrook J H,Wood D L.Nature,1961;192:1280
[17]Williams T M,Stoneham A M,Harries D R.Metall Sci, 1976;10:14
[18]Karlsson L,Norden H.Acta Metall,1988;36:1
[19]Li Q F,Li L,Zheng L,Liu E B,Jin G,Yang S L.J Mater Sci,2004;39:6551
[20]Shinoda T,Nakamura T.Acta Metall,1981;29:1631
[21]Dong J X,Xie X S,Thompson R G.Metall Mater Trans, 2000;31A:2135
[1] LI Jiarong, DONG Jianmin, HAN Mei, LIU Shizhong. Effects of Sand Blasting on Surface Integrity and High Cycle Fatigue Properties of DD6 Single Crystal Superalloy[J]. 金属学报, 2023, 59(9): 1201-1208.
[2] LU Nannan, GUO Yimo, YANG Shulin, LIANG Jingjing, ZHOU Yizhou, SUN Xiaofeng, LI Jinguo. Formation Mechanisms of Hot Cracks in Laser Additive Repairing Single Crystal Superalloys[J]. 金属学报, 2023, 59(9): 1243-1252.
[3] JIANG He, NAI Qiliang, XU Chao, ZHAO Xiao, YAO Zhihao, DONG Jianxin. Sensitive Temperature and Reason of Rapid Fatigue Crack Propagation in Nickel-Based Superalloy[J]. 金属学报, 2023, 59(9): 1190-1200.
[4] GONG Shengkai, LIU Yuan, GENG Lilun, RU Yi, ZHAO Wenyue, PEI Yanling, LI Shusuo. Advances in the Regulation and Interfacial Behavior of Coatings/Superalloys[J]. 金属学报, 2023, 59(9): 1097-1108.
[5] BI Zhongnan, QIN Hailong, LIU Pei, SHI Songyi, XIE Jinli, ZHANG Ji. Research Progress Regarding Quantitative Characterization and Control Technology of Residual Stress in Superalloy Forgings[J]. 金属学报, 2023, 59(9): 1144-1158.
[6] ZHENG Liang, ZHANG Qiang, LI Zhou, ZHANG Guoqing. Effects of Oxygen Increasing/Decreasing Processes on Surface Characteristics of Superalloy Powders and Properties of Their Bulk Alloy Counterparts: Powders Storage and Degassing[J]. 金属学报, 2023, 59(9): 1265-1278.
[7] ZHANG Jian, WANG Li, XIE Guang, WANG Dong, SHEN Jian, LU Yuzhang, HUANG Yaqi, LI Yawei. Recent Progress in Research and Development of Nickel-Based Single Crystal Superalloys[J]. 金属学报, 2023, 59(9): 1109-1124.
[8] MA Dexin, ZHAO Yunxing, XU Weitai, WANG Fu. Effect of Gravity on Directionally Solidified Structure of Superalloys[J]. 金属学报, 2023, 59(9): 1279-1290.
[9] CHEN Jia, GUO Min, YANG Min, LIU Lin, ZHANG Jun. Effects of W Concentration on Creep Microstructure and Property of Novel Co-Based Superalloys[J]. 金属学报, 2023, 59(9): 1209-1220.
[10] ZHAO Peng, XIE Guang, DUAN Huichao, ZHANG Jian, DU Kui. Recrystallization During Thermo-Mechanical Fatigue of Two High-Generation Ni-Based Single Crystal Superalloys[J]. 金属学报, 2023, 59(9): 1221-1229.
[11] WANG Lei, LIU Mengya, LIU Yang, SONG Xiu, MENG Fanqiang. Research Progress on Surface Impact Strengthening Mechanisms and Application of Nickel-Based Superalloys[J]. 金属学报, 2023, 59(9): 1173-1189.
[12] FENG Qiang, LU Song, LI Wendao, ZHANG Xiaorui, LI Longfei, ZOU Min, ZHUANG Xiaoli. Recent Progress in Alloy Design and Creep Mechanism of γ'-Strengthened Co-Based Superalloys[J]. 金属学报, 2023, 59(9): 1125-1143.
[13] BAI Jiaming, LIU Jiantao, JIA Jian, ZHANG Yiwen. Creep Properties and Solute Atomic Segregation of High-W and High-Ta Type Powder Metallurgy Superalloy[J]. 金属学报, 2023, 59(9): 1230-1242.
[14] CHANG Songtao, ZHANG Fang, SHA Yuhui, ZUO Liang. Recrystallization Texture Competition Mediated by Segregation Element in Body-Centered Cubic Metals[J]. 金属学报, 2023, 59(8): 1065-1074.
[15] MU Yahang, ZHANG Xue, CHEN Ziming, SUN Xiaofeng, LIANG Jingjing, LI Jinguo, ZHOU Yizhou. Modeling of Crack Susceptibility of Ni-Based Superalloy for Additive Manufacturing via Thermodynamic Calculation and Machine Learning[J]. 金属学报, 2023, 59(8): 1075-1086.
No Suggested Reading articles found!