Abstract A three-dimensional heat transfer mathematical model has been developed for the cooling copper plate of the thin – slab continuous casting mold. Alternative boundary conditions are applied for the cooling slots and back plate of mold copper plate cold face. The self -developed computer code is used to calculate the temperature field in visual Fortran language. The temperature distribution temperature in heat face of mold copper plate is cloudy –shaped, and cold face is ice columnar. The influence on mold copper plate temperature fields of operational parameters (casting speed、copper plate thickness、cooling water velocity) are analyzed. Calculated typical positions temperature agrees well with the measured temperature. These results are the important theoretical base for the process control and optimization of mold design.
|
Received: 05 June 2006
|
|
[1]Samarasekera I V,Brimacombe J K.Trans ISS,1984;5: 79 [2]Zhang H,Tao H B,Liu A Q,Zhang Z B,Wang J B, Zhuang H Z.Iron Steel,2005;40(7):25 (张慧,陶红标,刘爱强,张振彪,王进步,庄汉洲.钢铁, 2005;40(7):25) [3]Thomas B G,Park J K, Sok Y U.Metall Mater Trans, 2002;33B:425 [4]Lu M J,Kuo Y Y,Ong T H,Lin C H.Steelmaking Conf Proc,1996;241:246 [5]Mahapatra R B,Samarasekera I V,Brimacombe J K.Met- all Trons,1991;22B:861 [6]Samarasekera I V,Brimacombe J K.Steelmaking Conf Proc,1991;189:196 [7]Thomas B G,Li G,Moitra A,Habing D.lronmaking Steelmaking,1998;12:125 [8]Won Y M,Yeo T J,Oh K H,Park J K,Choi J,Yim C H. ISIJ Int,1998;38:53 [9]Na X Z,Zhang H,Gan Y,Zhang X Z.Iron Steel(Suppl), 2000;35:233 (那贤昭,张慧,干勇,张兴中.钢铁(增刊),2000;35: 233) [10]Thomas B G.Metall Mater Trans,1994;25B:443 |
No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|