Please wait a minute...
Acta Metall Sin  2007, Vol. 43 Issue (3): 332-326     DOI:
Research Articles Current Issue | Archive | Adv Search |
ANALYSIS OF THREE DIMENSIONAL HEAT TRANSFER OF COOLING COPPER PLATE IN THIN-SLAB CONTINUOUS CASTING MOLD
Cite this article: 

. ANALYSIS OF THREE DIMENSIONAL HEAT TRANSFER OF COOLING COPPER PLATE IN THIN-SLAB CONTINUOUS CASTING MOLD. Acta Metall Sin, 2007, 43(3): 332-326 .

Download:  PDF(789KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  A three-dimensional heat transfer mathematical model has been developed for the cooling copper plate of the thin – slab continuous casting mold. Alternative boundary conditions are applied for the cooling slots and back plate of mold copper plate cold face. The self -developed computer code is used to calculate the temperature field in visual Fortran language. The temperature distribution temperature in heat face of mold copper plate is cloudy –shaped, and cold face is ice columnar. The influence on mold copper plate temperature fields of operational parameters (casting speed、copper plate thickness、cooling water velocity) are analyzed. Calculated typical positions temperature agrees well with the measured temperature. These results are the important theoretical base for the process control and optimization of mold design.
Key words:  thin slab continuous casting      mold      copper plate      
Received:  05 June 2006     
ZTFLH:  TG249  
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2007/V43/I3/332

[1]Samarasekera I V,Brimacombe J K.Trans ISS,1984;5: 79
[2]Zhang H,Tao H B,Liu A Q,Zhang Z B,Wang J B, Zhuang H Z.Iron Steel,2005;40(7):25 (张慧,陶红标,刘爱强,张振彪,王进步,庄汉洲.钢铁, 2005;40(7):25)
[3]Thomas B G,Park J K, Sok Y U.Metall Mater Trans, 2002;33B:425
[4]Lu M J,Kuo Y Y,Ong T H,Lin C H.Steelmaking Conf Proc,1996;241:246
[5]Mahapatra R B,Samarasekera I V,Brimacombe J K.Met- all Trons,1991;22B:861
[6]Samarasekera I V,Brimacombe J K.Steelmaking Conf Proc,1991;189:196
[7]Thomas B G,Li G,Moitra A,Habing D.lronmaking Steelmaking,1998;12:125
[8]Won Y M,Yeo T J,Oh K H,Park J K,Choi J,Yim C H. ISIJ Int,1998;38:53
[9]Na X Z,Zhang H,Gan Y,Zhang X Z.Iron Steel(Suppl), 2000;35:233 (那贤昭,张慧,干勇,张兴中.钢铁(增刊),2000;35: 233)
[10]Thomas B G.Metall Mater Trans,1994;25B:443
[1] PENG Zhiqiang, LIU Qian, GUO Dongwei, ZENG Zihang, CAO Jianghai, HOU Zibing. Independent Change Law of Mold Heat Transfer in Continuous Casting Based on Big Data Mining[J]. 金属学报, 2023, 59(10): 1389-1400.
[2] WANG Chunhui, YANG Guangyu, ALIMASI Aredake, LI Xiaogang, JIE Wanqi. Effect of Printing Parameters of 3DP Sand Mold on the Casting Performance of ZL205A Alloy[J]. 金属学报, 2022, 58(7): 921-931.
[3] LIU Zhongqiu, LI Baokuan, XIAO Lijun, GAN Yong. Modeling Progress of High-Temperature Melt Multiphase Flow in Continuous Casting Mold[J]. 金属学报, 2022, 58(10): 1236-1252.
[4] Ting ZHANG,Yuhong ZHAO,Liwen CHEN,Jianquan LIANG,Muxi LI,Hua HOU. Graphene Nanoplatelets Reinforced Magnesium Matrix Composites Fabricated by Thixomolding[J]. 金属学报, 2019, 55(5): 638-646.
[5] ZHUO Weijia, LIU Yuan, LI Yanxiang. EFFECT OF WITHDRAWING RATE ON PORE MORPHOLOGY OF LOTUS-TYPE POROUS COPPER PRODUCED BY SINGLE-MOLD GASAR TECHNIQUE[J]. 金属学报, 2014, 50(8): 921-929.
[6] LI Dewei, SU Zhijian, CHEN Jin, WANG Qiang, MARUKAWA Katsukiyo, HE Jicheng. NUMERICAL SIMULATION OF SWIRLING FLOW IN DIVERGENT SUBMERGED ENTRY NOZZLE IN ROUND BILLET CONTINUOUS CASTING OF STEEL[J]. 金属学报, 2013, 49(7): 871-880.
[7] LIU Zhongqiu1, LI Baokuan1, JIANG Maofa1, ZHANG Li2, XU Guodong2. LARGE EDDY SIMULATION OF UNSTEADY ARGON/STEEL TWO PHASE TURBULENT FLOW IN A CONTINUOUS CASTING MOLD[J]. 金属学报, 2013, 49(5): 513-522.
[8] JIA Hao ZHANG Zhenqiang YU Zhan DENG Kang LEI Zuosheng REN Zhongming. INFLUENCE OF MAGNETIC FIELD INTENSITY MATCH OF FC MOLD II ON METAL FLOW[J]. 金属学报, 2012, 48(9): 1049-1056.
[9] CHEN Zhihui WANG Engang ZHANG XingwuWANG Yuanhua ZHU Mingwei HE Jicheng. STUDY ON THE BEHAVIOUR OF BUBBLES IN A CONTINUOUS CASTING MOLD WITH Ar INJECTION AND TRAVELING MAGNETIC FIELD[J]. 金属学报, 2012, 48(8): 951-956.
[10] ZOU Shiwen1, LI Xiaogang1,2, DONG Chaofang1,2,LI Huiyan1, XIAO Kui1,2. EFFECT OF MOLD ON CORROSION BEHAVIOR OF PRINTED CIRCUIT BOARD-COPPER AND ENIG FINISHED[J]. 金属学报, 2012, 48(6): 687-695.
[11] LI Baokuan LIU Zhongqiu QI Fengsheng WANG Fang XU Guodong. LARGE EDDY SIMULATION FOR UNSTEADY TURBULENT FLOW IN THIN SLAB CONTINUOUS CASTING MOLD[J]. 金属学报, 2012, 48(1): 23-32.
[12] CAI Zhaozhen ZHU Miaoyong. SIMULATION OF THERMAL BEHAVIOR DURING STEEL SOLIDIFICATION IN SLAB CONTINUOUS CASTING MOLD I. Mathematical Model[J]. 金属学报, 2011, 47(6): 671-677.
[13] CAI Zhaozhen ZHU Miaoyong. SIMULATION OF THERMAL BEHAVIOR DURING STEEL SOLIDIFICATION IN SLAB CONTINUOUS CASTING MOLD II. Model Verification and Results Analysis[J]. 金属学报, 2011, 47(6): 678-687.
[14] WANG Yin ZHANG Zhenqiang YU Zhan JIA Hao DENG Kang LEI Zuosheng REN Zhongming. EXPERIMENTAL STUDY ON FLOWIN SLAB MOLD CONTROLLED BY JET–PATTERN MAGNETIC FIELD[J]. 金属学报, 2011, 47(10): 1285-1291.
[15] YU Zhan ZHANG Zhenqiang REN Zhongming LEI Zuosheng DENG Kang. STUDY ON THE FLUID FLOW IN SLAB CONTINUOUS CASTING MOLD WITH ELECTROMAGNETIC BRAKE[J]. 金属学报, 2010, 46(10): 1275-1280.
No Suggested Reading articles found!