Acta Metall Sin  2013, Vol. 49 Issue (5): 513-522    DOI: 10.3724/SP.J.1037.2012.00760
Current Issue | Archive | Adv Search |
LARGE EDDY SIMULATION OF UNSTEADY ARGON/STEEL TWO PHASE TURBULENT FLOW IN A CONTINUOUS CASTING MOLD
LIU Zhongqiu1), LI Baokuan1), JIANG Maofa1), ZHANG Li2), XU Guodong2)
1)Department of Materials and Metallurgy, Northeastern University, Shenyang 110819
2)Baoshan Iron and Steel Limited Company, Shanghai 201900
Cite this article: 

LIU Zhongqiu1, LI Baokuan1, JIANG Maofa1, ZHANG Li2, XU Guodong2. LARGE EDDY SIMULATION OF UNSTEADY ARGON/STEEL TWO PHASE TURBULENT FLOW IN A CONTINUOUS CASTING MOLD. Acta Metall Sin, 2013, 49(5): 513-522.

Download:  PDF(7358KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  

A large eddy simulation of unsteady argon/steel two phase flow in a continuous casting mold is presented in this work. The inhomogeneous Euler-Euler approach is used to describe the equations of motion of the two phase flow. Large eddy simulation model is used to solve the turbulent viscosity force. The drag force, lift force and virtual mass force are incorporated in the model. And this model has been validated with a water model experiment and the measurements of the ultrasonic flaw detection. The predicted unsteady two phase turbulent flow characteristics were validated, indirectly, by the measurements of ultrasonic flaw detection. The predicted asymmetric flow was validated by the water model experiment. The simulation results show that the distribution of the bubble diameter is seen to depend on the argon gas and molten steel flow rates. The mean bubble diameter decreases with increasing the molten steel flow rate, but increases with increasing the argon gas flow rate. The asymmetric flow inside the mold was not stationary; the time intervals for changeover appeared to be vary random. It can be concluded that the shape of the bending part of the secondary cooling zone of mold is important to the asymmetric flow. The asymmetric flow occurrs near the bending section.

Key words:  continuous casting mold      two phase flow      large eddy simulation      Euler-Euler approach     
Received:  21 December 2012     

URL: 

https://www.ams.org.cn/EN/10.3724/SP.J.1037.2012.00760     OR     https://www.ams.org.cn/EN/Y2013/V49/I5/513

[1] Bai H, Thomas B G. Metall Mater Trans, 2001; 32B: 253


[2] Bai H, Thomas B G. Metall Mater Trans, 2001; 32B: 269

[3] Zhang L F, Yang S B, Cai K K, Li J Y, Wang X G, Thomas B G. Metall Mater Trans, 2007; 38B: 63

[4] Yoshida J, Iguchi M, Yokoya S.  Tetsu Hagane, 2001; 87: 529

(吉田进, 井口学, 横谷真一郎. 铁と钢, 2001; 87: 529)

[5] Bessho N, Yoda R, Yamasaki H. Iron Steelmaker, 1991; 18: 39

[6] Thomas B G, Huang X, Sussman R C. Metall Mater Trans, 1994; 25B: 527

[7] Sanchez-Perez R, Morales R D, Palafox-Ramos J, Diaz-Cruz M. Metall Mater Trans, 2004; 35B: 85

[8] Sanchez-Perez R, Morales R D. ISIJ Int, 2003; 43: 637

[9] Bai H, Thomas B G. Metall Mater Trans, 2001; 32B: 1143

[10] Lee G G, Thomas B G, Kim S H. Met Mater Int, 2010; 16: 501

[11] Kubo N, Ishii T, Kubota J. ISIJ Int, 2002; 42: 1251

[12] Li B K, Okane T, Umeda T. Metall Mater Trans, 2000; 31B: 1491

[13] Li B K, Okane T, Umeda T. Metall Mater Trans, 2001; 32B: 1053

[14] Yu H Q, Zhu M Y. Acta Metall Sin, 2008; 44: 619

(于海歧, 朱苗勇. 金属学报, 2008; 44: 619)

[15] Wang Y F, Zhang L F. Metall Mater Trans, 2011; 42B: 1319

[16] Liu Z Q, Qi F S, Li B K, Tsukihashi F. J Iron Steel Res Int, 2011; 18: 243

[17] Hershey D E, Thomas B G, Najjar F M. Int J Numer Methods Fluids, 1993; 17: 23

[18] Moser R D, Kim J, Mansour NN. Phys Fluids, 1999; 4: 943

[19] Yuan Q, Sivaramakrishnan S, Vanka S P, Thomas B G. Metall Mater Trans, 2004; 35B: 967

[20] Li B K, Liu Z Q, Qi F S, Wang F, Xu G D. Acta Metall Sin, 2012; 48: 23

(李宝宽, 刘中秋, 齐凤升, 王芳, 徐国栋. 金属学报, 2012; 48: 23)

[21] Yuan Q, Thomas B G, Vanka S P. Metall Mater Trans, 2004; 35B: 685

[22] Qian Z D, Wu Y L. Acta Metall Sin, 2004; 40: 88

(钱忠东, 吴玉林. 金属学报, 2004; 40: 88)

[23] Real C, Miranda R, Vilchis C, Barron M, Hoyos L, Gonzalez J. ISIJ Int, 2006; 46: 1183

[24] Deen N G, Solberg T, Hjertager B H. Chem Eng Sci, 2011; 56: 6341

[25] Dhotre M T, Niceno B, Smith B L. Chem Eng J, 2008; 136: 337

[26] Jakobsen H A, Sannaes B H, Grevskott S, Svendsen H F. Ind Eng Chem Res, 1997; 36: 4052

[27] Sato Y, Sekoguchi K. Int J Multiphase Flow, 1975; 2: 79

[28] Smagorinsky J. Mon Weather Rev, 1963; 91: 99

[29] Singh V, Dash S K, Sunitha J S, Ajmani S K, Das A K. ISIJ Int, 2006; 46: 210

[30] Gupta D, Lahiri A K. Metall Mater Trans, 1996; 27B: 757

[31] Miki Y, Takeuchi S. ISIJ Int, 2003; 43: 1548
[1] LIU Zhongqiu, LI Baokuan, XIAO Lijun, GAN Yong. Modeling Progress of High-Temperature Melt Multiphase Flow in Continuous Casting Mold[J]. 金属学报, 2022, 58(10): 1236-1252.
[2] Chang LIU, Shusen LI, Lifeng ZHANG. Simulation of Gas-Liquid Two-Phase Flow and Mixing Phenomena During RH Refining Process[J]. 金属学报, 2018, 54(2): 347-356.
[3] CHEN Zhihui WANG Engang ZHANG XingwuWANG Yuanhua ZHU Mingwei HE Jicheng. STUDY ON THE BEHAVIOUR OF BUBBLES IN A CONTINUOUS CASTING MOLD WITH Ar INJECTION AND TRAVELING MAGNETIC FIELD[J]. 金属学报, 2012, 48(8): 951-956.
[4] LI Baokuan LIU Zhongqiu QI Fengsheng WANG Fang XU Guodong. LARGE EDDY SIMULATION FOR UNSTEADY TURBULENT FLOW IN THIN SLAB CONTINUOUS CASTING MOLD[J]. 金属学报, 2012, 48(1): 23-32.
[5] YAO Jun Michael Fairweather LI Ning. DEPOSITION MECHANISM OF PARTICLE-LIKE CORROSION PRODUCT IN TURBULENT DUCT[J]. 金属学报, 2011, 47(7): 804-808.
[6] MENG Xiangning ZHU Miaoyong. ANALYSIS OF LIQUID FLUX CONSUMPTION MECHANISM FOR SLAB CONTINUOUS CASTING MOLD WITH HIGH CASTING SPEED[J]. 金属学报, 2009, 45(4): 485-489.
[7] Xiang-Ning MENG; Miao-Yong ZHU. ANALYSIS OF LIQUID FRICTION MECHANISM FOR SLAB CONTINUOUS CASTING MOLD WITH HIGH CASTING SPEED[J]. 金属学报, 2008, 44(10): 1193-1197 .
[8] Xiang-Ning MENG; Xu-Dong LIU. STUDY ON NON-SINUSOIDAL OSCILLATION FOR SLAB CONTINUOUS CASTING MOLD WITH HIGH CASTING SPEED Ⅰ. Mechanism of Oscillation Marks Formation[J]. 金属学报, 2007, 43(8): 839-846 .
[9] Xiang-Ning MENG. STUDY ON NON-SINUSOIDAL OSCILLATION FACTOR FOR CONTINUOUS CASTING MOLD WITH HIGH CASTING SPEED[J]. 金属学报, 2007, 43(2): 205-210 .
[10] QIAN Zhongdong; WU Yulin. Large Eddy Simulation And Controlling Of Vortexing Flow Of Molten Steel In Continuous Casting Mold[J]. 金属学报, 2004, 40(1): 88-93 .
[11] LI Baokuan;HE Jicheng;JIA Guanglin;GAO Yunyan(Northeastern University; Shenyang 110006). ELECTROMAGNETIC BRAKING ON FLOW FIELD OF MOLTEN STEEL IN THE THIN-SLAB CONTINUOUS CASTING MOLD[J]. 金属学报, 1997, 33(11): 1207-1214.
No Suggested Reading articles found!