Abstract The deformation behaviour of Mg-Y-Nd-Zr alloy at temperatures of 300-500℃ and strain rates of 0.001-1s-1 has been studied by compressive tests. Processing map of this alloy was established on the basis of Dynamic Material Model; it is suggested that, with microstructural observation, the processing map of this alloy could be characterized as the following four domains: First, dynamic recrystallization (DRX) domain at 450-500℃ and about 0.01s-1. Second, boundary cracking domain at temperatures higher than 450℃ and strain rates of about 0.005s-1. Third, flow instability domain probably due to mechanical twinning at temperature lower than 350℃ and strain rate of about 0.01s-1. Last, shearing fracture at about 450℃ and strain rates higher than 0.5s-1.
[1]Pekguleryuz M O,Kaya A A.Adv Eng Mater,2003;5:866 [2]Smola B,Stulikova I,Von Buch F,Mordike B L.Mater Sci Eng,2002;A324:113 [3]Wang J G,Hsiung L M,Nieh T G,Mabuchi M.Mater SciEng,2001;A315:81 [4]Mohri T,Mabuchi M,Saito N,Nakamura M.Mater Sci Eng,1998;A257:287 [51Watanabe H,Mukai T,Ishikawa K,Mohri T,Mabuchi M,Higashi K.Mater Trans,2001;42:157 [6]Sha G Y,Han E H,Yu T,Xu Y B,Liu L,Gao G Z.Acta Metall Sin,2003;39:1025(沙桂英,韩恩厚,于涛,徐永波,刘路,高国忠.金属学报,2003;39:1025) [7]Mordike B L.Mater Sci Eng,2002;A324:103 [8]Polmear I J.Mater Trans JIM,1996;37(1):12 [9]Sivakesavam O,Prasad Y V R K.Mater Sci Eng,2002;A323:270 [10]Sivakesavam O,Prasad Y V R K.Mater Sci Eng,2003;A362:118 [11]Sivakesavam O,Rao I S,Prasad Y V R K.Mater Sci Technol,1993;9:805 [12]Nie J F,Muddle B C.Acta Mater,2000;48:1691 [13]Prasad Y V R K,Seshacharyulu T.Int Mater Rev,1998;43:243 [14]Narauana M S V S,Nageswara R B,Kashyap B P.Int Mater Rev,2000;45:15 [15]Raj R.Metall Trans,1981;12A:1089