Abstract Fine grained dual phase steel obtained by deformation enhanced transformation (DEFT) was investigated by using hot compressing simulation experiments. The evolution of ferrite grains and M/A islands distribution during deformation were analyzed. The effects of initial austenite grain size、deformation temperature and strain rate on ferrite transformation kinetics were taken into consideration. The experimental results showed that the microstructure of fine grained ferrite(2~3μm)with fine granular M/A islands dispersing in the matrix can be achieved by controlling the initial austenite grain size and DEFT. Fine dual phase structure can be achieved by austenite recrystallization and the subsequent controlled DEFT.
[1]Hong S C,Lee K S.Mater Sci Eng,2002;A323:148 [2]Yu H.Steel Technol,2005;6(6):10(余海.钢铁技术,2005;6(6):10) [3]Erdogan M,Tekeli S.Mater Design,2002;23:597 [4]Bleck W,Phiu-On K.In:Weng Y Q ed,The Joint Int Conf of HSLA Steels 2005 and ISUGS 2005,Hainan:The Chinese Socity for Metals,2005:50 [5]Li S X,Li G Y,Weng Y Q.Z Metallkd,2004;2:115 [6]Adamczyk J,Grajcar A.J Mater Process Technol,2005;162-163:267 [7]Park K T,Lee Y K,Shin D H.ISIJ Int,2005;45:750 [8]Liu S,Li F P.Automob Technol Mater,2001;4(4):20(刘胜,李飞鹏.汽车工艺与材料,2001;4(4):20) [9]Sun Z Q,Yang W Y,Qi J J,Hu A M.Mater Sci Eng,2002;A334:201 [10]Yang W Y,Hu A M,Qi J J,Sun Z Q.Chin J Mater Res,2001;15:171(杨王玥,胡安民,齐俊杰,孙祖庆.材料研究学报,2001;15:171) [11]Ma M T,Wu B R.Dual Phase Steel—Physics & Mechanical Metallurgy.Beijing:Metallurgical Industry Press,1988:156(马鸣图,吴宝榕.双相钢—物理和力学冶金.北京:冶金工业出版社,1988:156) [12]Zhou R F,Yang W Y,Sun Z Q,Zhang Y.Iron Steel,2004;39(8):93(周荣锋,杨王玥,孙祖庆,张艳.钢铁,2004;39(8):93)