| CALCULATION OF THE RELAXED STRUCTURE AND ENERGY OF EDGE DISLOCATION IN BCC METAL BY MODIFIED ANALYTICAL EMBEDDED-ATOM METHOD |
| ; |
| 陕西师范大学 |
|
Cite this article:
;. CALCULATION OF THE RELAXED STRUCTURE AND ENERGY OF EDGE DISLOCATION IN BCC METAL BY MODIFIED ANALYTICAL EMBEDDED-ATOM METHOD. Acta Metall Sin, 2007, 43(2): 182-186 .
|
|
|
Abstract Combining MAEAM with MD simulation method, both the relaxed structure and strain energy of an a[100] edge dislocation in BCC metal Mo have been simulated systematically in atomic scales. The results show that the relaxed structure has a C2V type group symmetry.Calculated strain energy Es per unit length of the dislocation is a linear function of ln(R/2b) while radial distance R≥1.5b=4.72Å, thus the corresponding core radius is determined to be rc=4.72Å. From intercept and slope of linear fitting those data corresponding to the outside of the dislocation core, we further infer the dislocation core energy Ecore=1.6334eV/Å, K=0.10eV/Å3, the latter is in agreement with the elasticity theory prediction (K=μ/4π(1-υ)=0.088eV/Å3).
|
|
Received: 22 May 2006
|
|
|
[1]Gao F.Acta Phys Sin,1990;39:1591(高飞.物理学报,1990;39:1591) [2]Daw M S,Baskes M I.Phys Rev,1984;29B:6443 [3]Foiles S M,Baskes M I,Daw M S.Phys Rev,1986;33B:7983 [4]Adams J B,Foiles S M,Wolfer W G.J Mater Res,1989;4:102 [5]Daw M S,Baskes M I.Phys Rev Left,1983;50:1285 [6]Daw M S,Foiles S M.Phys Rev Lett,1987;59:2756 [7]Dodson B W.Phys Rev,1987;35B:880 [8]Johnson R A.Phys Rev,1988;37B:3924 [9]Baskes M I.Phys Rev,1992;46B:2727 [10]Zhang B W,Ouyang Y F.Phys Rev,1993;48B:3022 [11]Zhang B W,Ouyang Y F,Liao S Z,Jin Z P.Physica,1999;262B:218 [12]Hu W Y,Zhang B W,Huang B Y,Gao F,Bacon D J.J Phys:Condens Matter,2001;13:1193 [13]Hu W Y,Zhang B W,Shu X L,Huang B Y.J Alloy Compd,1999;287:159 [14]Zhang J M,Ma F,Xu K W.Surf Interface Anal,2005;35:662 [15]Zhang J M,Ma F,Xu K W,Xin X T.Surf Interface Anal,2003;35:805 [16]Zhang J M,Wei X M,Xin H.Surf Interface Anal,2004;36:1500 [17]Zhang J M,Wei X M,Xin H.Appl Surf Sci,2005;243:1 [18]Zhang J M,Wei X M,Xin H,Xu K W.Chin Phys,2005;14:1015 [19]Ma F,Zhang J M,Xu K W.Surf Interface Anal,2003;36:355 [20]Zhang J M,Xin H,Wei X M.Appl Surf Sci,2005;246:14 [21]Xin H,Zhang J M,Wei X M,Xu K W.Surf Interface Anal,2005;37:608 [22]Zhang B W,Hu W Y,Shu X L.Theory of Embedded Atom Moethod and Its Application to Materials Science.Changsha:Hunan University Press,2003:249(张邦维,胡望宇,舒小林.嵌入原子方法理论及其在材料科学中的应用.长沙:湖南大学出版社,2003:249) [23]Hirth J P,Lothe J.Theory of Dislocations.New York:Wiley Press,1982:761 |
| No Suggested Reading articles found! |
|
|