| Development of New Cu-Zr-Al-Pd Bulk Metallic Glasses with excellent mechanical and corrosion properties |
| 华中科技大学材料学院 |
|
Cite this article:
. Development of New Cu-Zr-Al-Pd Bulk Metallic Glasses with excellent mechanical and corrosion properties. Acta Metall Sin, 2007, 43(2): 177-181 .
|
|
|
Abstract Cu43Zr43Al7Pd7 bulk metallic glass (BMG) with a diameter up to 5mm was successfully prepared by copper mold casting. The glass-forming ability (GFA) and thermal stability of the BMG obtained were investigated by means of XRD, DSC and DTA. It is shown that Cu43Zr43Al7Pd7 system exhibited an excellent glass forming ability as indicated by high values of Trg (=0.607) and γ (=0.417) as well as supercooled liquid region(Tx= 75K), respectively. Uniaxial compressive test revealed that the BMG obtained possesses pretty good mechanical properties with a fracture strength of 1877 MPa and an overall strain of 4.9%, respectively. Electrochemical measurements were carried out in 1mol/LH2SO4 and 3%NaCl aqueous solutions by potentiadynamic polarization at room temperature. It is shown that Cu43Zr43Al7Pd7 BMG exhibited spontaneous passivation in both solutions with wide passive regions. The passive current densities are about 10-6~10-5 A/cm2, which are much lower than that of Cr18-Ni8 stainless steel, implying a good corrosion resistance.
|
|
Received: 23 May 2006
|
|
|
[1]Lin X H,Johnson W L.J Appl Phys,1995;78:6514 [2]Inoue A,Zhang W,Zhang T,Kurosaka K.J Non-Cryst Solid,2002;304:200 [3]Inoue A,Zhang W,Zhang T,Kurosaka K.Acta Mater,2001;49:2645 [4]Wang D,Li Y.Appl Phys Lett,2004;84:4029 [5]Wang D,Tan H,Li Y.Acta Mater,2005;53:2969 [6]Xu D H,Duan G,Johnson W L.Phys Rev Lett,2004;92:245504 [7]Oh J C,Ohkubo T,Kim Y C,Fleury E,Hono K.Scr Mater,2005;53:165 [8]Sung D S,Kwon O J,Fleury E,Kim K B,Lee J C,Kim D H,Kim Y C.Met Mater Int,2004;10:575 [9]Choi-Yim H,Busch R,Johnson W L.J Appl Phys,1998;83:7993 [10]Yamamoto T,Zhang T,Inoue A.Mater Trans JIM,2003;44:1147 [11]Nishiyama N,Inoue A.Mater Trans JIM,1996;31:1531 [12]Senkov O N,Miracle D B.Mater Res Bull,2001;36:2183 [13]de Boer F R,Boom R,Mattens W C M,Miedema A R,Niessen A K.Cohesion in Metals.Amsterdam:North-Holland,1988:485,375 [14]Park E S,Chang H J,Kim D H,Ohkubo T,Hono K.Scr Mater,2006;54:1569 [15]Park E S,Kim D H.Acta Mater,2006;54:2597 [16]Dai C L,Guo H,Shen Y,Li Y,Ma E,Xu J.Scr Mater,2006;54:1403 [17]Xing L Q,Li Y,Ramesh K T,Li J,Hufnagel T C.Phys Rev,2001;64B:18021 [18]Lee M H,Lee J Y,Bae D H,Kim W T,Sordelet D J,Kim D H.Intermetallics,2004;12:1133 [19]Schroers J,Johnson W L.Phys Rev Lett,2004;93:255506 [20]Kündig A A,Ohnuma M,Ping D H,Ohkubo T,Hono K.Acta Mater,2004;52:2441 [21]Fan C,Imafuku M,Kurokawa H,Inoue A,Haas V.Appl Phys Lett,2001;79:1792 [22]Zhu Z W,Zhang H F,Sun W S,Ding B Z,Hu Z Q.Scr Mater,2006;54:1145 [23]Kim K B,Das J,Baler F,Tang M B,Wang W H,Eckert J.Appl Phys Lett,2006;88:051911 [24]Bei H,Lu Z P,George E P.Phys Rev Lett,2004;93:125504 [25]Bei H,Xie S,George E P.Phys Rev Lett,2004;96:105503 [26]Qin F X,Zhang H F,Deng Y F,Ding B Z,Hu Z Q.J Alloy Compd,2004;375:318 [27]Qin F X,Zhang H F,Chen P,Chen F F,Qiao D C,Hu Z Q.Mater Lett,2004;58:1246 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|