Progress in Materials Characterization Technique Based on in Situ Neutron Diffraction
XU Pingguang; TOMOTA Yo
Graduate School of Science and Engineering;Ibaraki University; Hitachi 316-8511; Japan
Cite this article:
XU Pingguang; TOMOTA Yo. Progress in Materials Characterization Technique Based on in Situ Neutron Diffraction. Acta Metall Sin, 2006, 42(7): 681-688 .
Abstract Neutron diffraction is an atomic- or molecular-level characterization technique of material structures and microscopic movements because neutron is an electronic neutral subatomic particle with certain magnetic moment, strong penetration, more sensitive to light elements than X-ray and electron. The in situ neutron diffraction as one of materials four-dimensional characterization techniques has been reviewed with much emphasis on its applications to metallic materials science, such as residual stress evaluation, plastic deformation mechanism, solid phase transformation and nanometer clusters.
[1] Bacon G E. Neutron Diffraction.Oxford:Clarendon Press, 1975: 1 [2] Niimura N,Torikai N,Uesaka M,Tomota Y,Sakuma T,Nishihara Y,Nakanishi T,Takatsuma T.Proc Ibaraki Symp on Industrial Applications of Neutron Science (hosted by Ibaraki-ken Govemment).Tsukuba,Japan, 2005: 9 (新村信雄,鸟饲直也,上坂 充,友田 阳,佐久间隆,西原美 一,中西友子,高妻孝光.茨城中性子产业利用ツソホヅヮム讲 演资料集(茨城主催).日本,筑波,2005:9) [3] Chen D F, Gou C, Ye C T. Nucl Tech, 2005; 28(2): 127 (陈东风,勾 成,叶春堂.核技术, 2005;28(2):127) [4] Tomota Y. Ferrum, 2004; 9: 544 (友田阳.ふぇらむ,2004;9:544) [5] Tomota Y.CAMP-ISIJ, 2005; 18: 491 [6] Poulsen H F,Garbe S,Lorentzen T,Juul Jensen D, Poulsen F W,Andersen N H,Frello T,Feidenhans'l R, Graafsma H. J Synchrot Radiat, 1997; 4: 147 [7] Margulies L, Winther G, Poulen H F. Science, 2001; 291:2392 [8] Ohnuma M, Hono K, Linderoth S,Pedersen J S,Yoshizawa Y, Onodera H. Acta Mater, 2000 48: 4783 [9] Nakamura Y. J Magn Magn Mater,1999; 200: 634 [10] Allen D R, Sayers C M. NDT Int, 1981; 14: 263 [11] Hutchings M T,Withers P J,Holden T M, Lorentzen T. Introduction to the Characterization of Residual Stress by Neutron Diffraction.Boca Raton:Taylor and Francis Group, 2005: 1 [12] Jin X J, Shiota Y, Tomota Y,Matsushima,Suzuki H,Moriai A. CAMP-ISIJ, 2005; 18: 497 [13] Webster P J. In:Fitzpatrick M E,Lodini A, eds.,Analysis of Residual Stress by Diffraction Using Neutron and Synchrotron Radiation,London:Taylor and Francis Group, 2003: 209 [14] Shiota Y,Xu P G,Tomota Y,Suzuki H,Holden T M. Unpublished Work [15] Donadille C,Valle R,Dervin P,Penelle R.Acta Metall, 1989; 37: 1547 [16] Sprauel J M. In: Fitzpatrick M E, Lodini A eds., Analysis of Residual Stress by Diffraction Using Neutron and Synchrotron Radiation.London:Taylor and Francis Group, 2003: 78 [17] Tomota Y, Lukas P, Harjo S, Park J H,Tsuchida N, Neov D. Acta Mater, 2003; 51: 819 [18] Tomota Y,Tokuda H,Adachi Y, Wakita M, Minakawa N, Moriai A, Morii Y. Acta Mater, 2004; 52: 5737 [19] Kanie A, Tomota Y,Suzuki T,Torii S,Kamiyama T. CAMP-ISIJ,2003;16:1453 [20] Ikeda K,Tomota Y,Suzuki J.CAMP-ISIJ,2006;19(3): 36 [21] Xu P G, Tomota Y, Lukas P,Muransky O,Adachi Y. Sci Eng A, accepted [22] Xu P G, Tomota Y,Lukas P, Adachi Y.Iron Steel,2005; 40(suppl.): 234