CALCULATION ON ELECTROMAGNETIC FORCE IN ELECTROMAGNETIC STIRRING OF CONTINUOUS CASTING OF STEEL
;
东北大学材料与冶金学院
Cite this article: 

;. CALCULATION ON ELECTROMAGNETIC FORCE IN ELECTROMAGNETIC STIRRING OF CONTINUOUS CASTING OF STEEL. Acta Metall Sin, 2006, 42(5): 540-544 .

Download:  PDF(833KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  A new model and a numerical method are developed to solve the electromagnetic force field produced by the rotating magnetic field in electromagnetic stirring of processing. The model equations are transformed using the characteristics of rotating magnetic field, and the boundary renewal method is applied to boundary conditions. Using the present model, the electromagnetic force fields in different size billets considering the effect of iron core are computed. The three – dimensional distribution of electromagnetic forces are obtained in detail under the condition of variable parameters. The numerical results agree well with the experimental measurement.
Key words:  electromagnetic stirring      electromagnetic force field      calculation model      continuous casting of stee     
Received:  09 September 2005     
ZTFLH:  TF777  
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2006/V42/I5/540

[1] Spizer K H, Dubke M, Schwerdtfeger K. Metall Trans, 1986; 17B: 119
[2] Meyer J L, Szekely J, Ei-Kaddah N. Trans ISIJ, 1987; 27: 25
[3] Natarajan T T, Ei-Kaddah N. ISIJ Int, 1998; 38: 680
[4] Nasar S A, Boldea I. Linear Motion Electric Machines. Hoboken, NJ: John Wiley and Sons, 1976: 215
[5] Ueyama T, Shinkura K, Ueda R. IEEE Trans Magn, 1989; 25: 4153
[6] Gliere A, Masse P. IEEE Trans Magn, 1988; 24: 252
[7] Spizer K H, Schwerdtfeger K. Iron Steelmaker, 1990; 17: 57
[8] Ma Y L, He Y D, Xu G Y, Lu X T. J Baotou Inst Iron Steel, 1997; 16: 193 (麻永林,贺友多,徐光尧,吕湘提.包头钢铁学院学报,1997; 16:193)
[9] Zhou W, Han H Y, Jia B, Zhang Y,Ma Y L, He Y D. J Baotou Inst Iron Steel, 1999; 18: 139 (周伟,韩海鹰,贾斌,张胤,麻永林,贺友多.包头钢 铁学院学报,1999;18:139)
[10] Li G, Li H D. J Univ Sci Technol Beijing, 2004; 26: 95 (李光,李华德.北京科技大学学报,2004;26:95)
[11] Chung S I, Shin Y H ,Yoon J K. Trans ISIJ, 1992; 32: 1287
[12] Kim S,Yoon J K. Ironmaking Steelmaking, 1991; 18: 446
[13] Trindade L B, Vilela A C F,Filho A F F, Vilhena T M B, Soares R B. IEEE Trans Magn, 2002; 38: 3658
[1] ZHANG Lin, GUO Xiao, GAO Jianwen, DENG Anyuan, WANG Engang. Effect of Electromagnetic Stirring on Microstructure and Mechanical Properties of TiB2 Particle-Reinforced Steel[J]. 金属学报, 2020, 56(9): 1239-1246.
[2] REN Zhongming,LEI Zuosheng,LI Chuanjun,XUAN Weidong,ZHONG Yunbo,LI Xi. New Study and Development on Electromagnetic Field Technology in Metallurgical Processes[J]. 金属学报, 2020, 56(4): 583-600.
[3] Guohua WU, Yushi CHEN, Wenjiang DING. Current Research and Future Prospect on Microstructures Controlling of High Performance Magnesium Alloys During Solidification[J]. 金属学报, 2018, 54(5): 637-646.
[4] Zheng LIU,Lina XU,Zhaofu YU,Yangzheng CHEN. RESEARCH ON THE MORPHOLOGY AND FRACTALDIMENSION OF PRIMARY PHASE IN SEMISOLIDA356-La ALUMINUM ALLOY BY ELECTRO-MAGNETIC STIRRING[J]. 金属学报, 2016, 52(6): 698-706.
[5] Zheng LIU,Jiayi ZHANG,Haolin LUO,Keyue DENG. RESEARCH ON MORPHOLOGY EVOLUTION OF PRIMARY PHASE IN SEMISOLID A356 ALLOY UNDER CHAOTIC ADVECTION[J]. 金属学报, 2016, 52(2): 177-183.
[6] LIU Zheng, LIU Xiaomei, ZHU Tao, CHEN Qingchun. EFFECTS OF ELECTROMAGNETIC STIRRING WITH LOW CURRENT FREQUENCY ON RE DISTRIBUTION IN SEMISOLID ALUMINUM ALLOY[J]. 金属学报, 2015, 51(3): 272-280.
[7] SU Zhijian LI Dewei SUN Liwei MARUKAWA Katsukiyo HE Jicheng. NUMERICAL SIMULATION OF SWIRLING FLOW IN IMMERSION NOZZLE INDUCED BY A ROTATING ELECTROMAGNETIC FIELD IN ROUND BILLET CONTINUOUS CASTING OF STEEL[J]. 金属学报, 2010, 46(4): 479-486.
[8] LIU Zheng MAO Weimin ZHAO Zhenduo. SEMI–SOLID A356 ALLOY SLURRY PREPARED BY A NEW PROCESS[J]. 金属学报, 2009, 45(4): 507-512.
[9] YU Haiqi ZHU Miaoyong. 3-D NUMERICAL SIMULATION OF FLOW FIELD AND TEMPERATURE FIELD IN A ROUND BILLET CONTINUOUS CASTING MOLD WITH ELECTROMAGNETIC STIRRING[J]. 金属学报, 2008, 44(12): 1465-1473.
[10] JIN Junze; CAO Zhiqiang; ZHENG Xianshu; ZHANG Shangru(Dalian University of Technology; Dalian 116023)(Manuscript received 1994-06-10; in revised form 1995-03-15). FORMATION OF SEPARATED EUTECTIC PHENOMENON BY ELECTROMAGNETIC STIRRING[J]. 金属学报, 1995, 31(20): 374-378.
[11] YANG Yuansheng; LIU Qingmin; JIAO Yuning; GE Yunlong; HU Zhuangqi(Institute of Metal Research;Chinese Academy of Sciences;Shenyang). FORCE FIELD ANALYSIS ON LIQUID METAL DURING ELECTROMAGNETIC CENTRIFUGAL SOLIDIFICATION[J]. 金属学报, 1994, 30(17): 208-212.
[12] CAO Zhiqiang;ZHANG Liping;REN Zhongming;JIN Junze Dalian University of Technology. INFLUENCE OF ELECTROMAGNETIC STIRRING ON MACRO-SEGREGATION OF GREY CAST IRON[J]. 金属学报, 1992, 28(2): 82-85.
[13] HU Hanqi;ZHENG Riqi University of Science and Technology Beijing professor;Faculty of Casting;University of Science and Technology Beijing;Beijing 100083. INFLUENCE OF ELECTROMAGNETIC STIRRING ON DENDRITIC STRUCTURE AND MECHANICAL PROPERTIES OF LOW SULPHUR STEEL[J]. 金属学报, 1990, 26(4): 83-86.
No Suggested Reading articles found!