| A Study of Abrasion Resistant Cast Fe-B-C Alloy |
| FU Hanguang |
| 清华大学 |
|
Cite this article:
FU Hanguang. A Study of Abrasion Resistant Cast Fe-B-C Alloy. Acta Metall Sin, 2006, 42(5): 545-548 .
|
|
|
Abstract The solidification structures of cast Fe-B-C alloy containing more than 2.0%B and lower than 0.2%C and the structures and properties of alloy after heat treatment were researched by means of optical microscopy (OM), scanning electron microscopy (SEM), X-ray diffraction (XRD), hardness measurements, impact tester and pin abrasion tester. The results show that the solidification structures of cast Fe-B-C alloy are made up of boride (Fe2B), pearlite and ferrite, and boride distributes along grain boundary in network form. After normalizing at 950oC, the part broken network of boride of cast Fe-B-C alloy appears, the matrix all transforms into lath martensite. The hardness of cast Fe-B-C alloy increases obviously and nears to60HRC, its impact toughness and dynamic fracture toughness excel 10J/cm2 and 30MPa.m1/2 respectively. In the condition of dry skimming wear, cast Fe-B-C alloy has excellent abrasion resistance. Its abrasion resistance is more excellent than that of Ni-hard white cast iron, GCr15 and Cr12MoV, nears to that of high chromium white cast iron. Cast Fe-B-C alloy has simple melting process and good casting property, there are no costly nickel and molybdenum elements and low production cost.
|
|
Received: 26 August 2005
|
|
|
[1] Dogan O N, Hawk J A, Rice J. In: Association for Iron and Steel Technology ed., AIST Process Metallurgy. Product Quality and Applications Proceedings, New Orleans, LA, Unite States, 2004: 451 [2] Laird G Ⅱ. AFS Trans, 1991; 99: 339 [3] Carpenter S D, Carpenter D, Pearce J T H. Mater Chem Phys, 2004; 85(1): 32 [4] Maldonado-Ruiz S I, Lopez D, Velasco A, Colas R. Mater Sci Technol, 2004; 20 [5] Fan Q Y, Fu W. Mach Eng, 1999;(4):33 (范庆云,傅伟.机械工程师,1999;(4):33 [6] Zumelzu E, Goyos I, Cabezas C, Opitz O, Parada A.J Mater Process Technol, 2002; 128: 250 [7] Tabrett C P, Sare 1 R, Ghomashchi M R.Int Mater Rev, 1996; 41(2): 59 [8] Ge C L, Ye R C, Zhu S C. J Chin Univ Min Technol, 1997; 7(1): 69 [9] Berns H, Fischer A. Mater Charact, 1997; 39: 499 [10] Martini C, Palombarini G, Poll G, Prandstraller D. Wear, 2004; 256: 608 [11] Pertek A, Kulka M. J Mater Sci, 2003; 38: 269 [12] Zum Gahr K H, George E T. Wear, 1980; 64: 175 [13] Fu H H, Han K S, Song J I. Wear, 2004; 256: 705 [14] Celik H, Kaplan M. Wear, 2004; 257: 606 [15] Banerjee K, Rollett A D. Ironmaking Steelmaking,2003; 30(6): 62 [16] Baker H. Alloy Phase Diagrams. Materials Park, Ohio: ASM International, 1992: 281 [17] Benxi Iron & Steel Co. Boron Steel.Beijing:Metallurgi- cal Industry Press, 1977: 2 (本溪钢铁公司.硼钢.北京:冶金工业出版社,1977:2) [18] Richardson R C D. Wear, 1968; 11: 245n |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|