| First-Principles Study of IVB and VB transition metal carbides and their surfaces |
| ;; |
| 中科院金属所 |
|
Cite this article:
. First-Principles Study of IVB and VB transition metal carbides and their surfaces. Acta Metall Sin, 2006, 42(5): 554-560 .
|
|
|
Abstract The structure and electronic properties of IVB and VB transition metal carbides and their surfaces are systematically investigated by first-principles method. The some important questions are studied and discussed, such as, the common characteristics and distinctions of the surface ripples on the (001) surfaces of different IVB and VB transition metal carbides, the effects of the surface ripple on the surface energy and the surficial charge distribution, the trends of the cohesive energy and surface energy of these IVB and VB transition metal carbides and their surfaces, and the correlation between the surface energy and the cohesive energy which is the inherent property of the bulk. A new viewpoint is suggested that the cohesive energy of the bulk carbides and the ripple ratio of the (001) surface affect and determine the surface energy of (001) surface of IVB and VB transition metal carbides together.
|
|
Received: 24 August 2005
|
|
|
[1] Toth L E. Transition Metal Carbides and Nitrides. New York: Academic Press, 1971:1 [2] Joansson L I. Surf Sci Rep, 1995; 21: 177 [3] Schwarz K, Crit C R C. Rev Solid State Mater Sci, 1987; 13: 211 [4] Zhang Y F, Li J Q, Zhou L X, Xiang S C. Solid State Commun, 2002; 121: 411 [5] Halglund J, Grimvall G, Jarlborg T, Guillermet A F. Phys Rev, 1991; 43B: 14400 [6] Guillermet A F, Halglund J, Grimvall G. Phys Rev, 1992; 45B: 11557 [7] Guillermet A F, Halglund J, Grimvall G. Phys Rev, 1993; 48B: 11673 [8] Aono M, Hou Y, Souda R, Oshima C, Otani S, Ishizawa Y. Phys Rev Lett, 1983; 50: 1293 [9] Kido Y, Nishimura T, Hoshino Y, Otani S, Souda R. Phys Rev, 2000; 61B: 1748 [10] Tagawa M, Okuzawa M, Kawasaki T, Oshima C, Otani S, Nagashima A. Phys Rev, 2001; 63B: 073407 [11] Tagawa M, Okuzawa M, Kawasaki T, Oshima C, Otani S, Edamoto K, Nagashima A. Surf Sci, 2002; 517: 59 [12] Price D L, Wills J M, Cooper B R. Phys Rev Lett, 1996; 77: 3375 [13] Kobayashi K. Jpn J Appl Phys, 2000; 39: 4311 [14] Hernandez N C, Graciani J, Sanz J F. Surf Sci, 2003; 541: 217 [15] Liu L M, Wang S Q, Ye H Q. J Phys: Condens Matter, 2003; 15: 8103 [16] Liu L M, Wang S Q, Ye H Q. J Phys: Condens Matter, 2004; 16: 5781 [17] Liu L M, Wang S Q, Ye H Q. Surf Sci, 2004; 550: 46 [18] Liu L M, Wang S Q, Ye H Q. Acta Mater, 2004; 52: 3681 [19] Hugosson H W, Eriksson O, Jansson U, Ruban A V, Souvatzis P, Abrikosov I A. Surf Sci, 2004; 557: 243 [20] Vines F, Sousa C, Liu P, Rodriguez J A, Illas F. J Chem Phys, 2005; 122: 174709 [21] Hohenberg P, Kohn W. Phys Rev, 1964; 136B: 864 [22] Kohn W, Sham L J. Phys Rev, 1965; 140A: 1133 [23] Vanderbilt D. Phys Rev, 1990; 41B: 7892 [24] Perdew J P, Chevary J A, Vosko S H, Jackson K A, Pederson M A, Singh D J, Fiolhais C. Phys Rev, 1992; 46B: 6671 [25] Monkhorst H J, Pack J D. Phys Rev, 1976; 13B: 5188 [26] Stampfl C, Freeman J A. Phys Rev, 2001; 63B: 155106 [27] Dudiy S V, Lundqvist B I. Phys Rev, 2001; 64B: 045403 [28] Dunand A, Flack H D, Yvon K. Phys Rev, 1985; 31B: 2299 [29] Arya A, Carter E A. Surf Sci, 2004; 560: 103 [30] Kempter C P, Fries R J. Anal Chem, 1960; 33: 570 [31] Siegel D J, Hector L G Jr, Adams J B. Acta Mater, 2002; 50: 619 [32] Zhukov V P, Gubanov V A, Jepsen O, Christensen N E, Andersen O K. J Phys Chem Solids, 1988; 49: 841 [33] Dodd S P, Cankurtaran M, James B. J Mater Sci, 2003; 38: 1107 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|