| Radiation Damage Behavior of Carbide in Long Term Aging Treatmented Low Activation Austenitic Fe-Cr-Mn Alloy |
| HU Benfu;HKINOSHITA Hiroshi; SAKAGUCHI Kisiki; TAKAHASHI Heishichiro |
|
Cite this article:
HU Benfu; HKINOSHITA Hiroshi; SAKAGUCHI Kisiki; TAKAHASHI Heishichiro. Radiation Damage Behavior of Carbide in Long Term Aging Treatmented Low Activation Austenitic Fe-Cr-Mn Alloy. Acta Metall Sin, 2006, 42(3): 234-238 .
|
|
|
Abstract In this study ,irradiation damage characteristic of carbide in Long term aging treatment for Fe-Cr-Mn alloy is investigated by electron beam and dual-beam with electron–hilum ion irradiation. The results indicate that the voids were observed inside carbide and along interface of carbide/matrix. Interface migration and interface segregation of Cr. Mn. W. V is first observed. The phase stability and reason of the irradiation damage of aged carbide are discussed with the interaction between point defects and solute elements and radiation-induced synergistic effect of hilum. The radiation damage phase is a form of expression of the unstability of phase.
|
|
Received: 17 March 2005
|
|
|
[1] Holland J R, Mansur L K, Potter D I. Phase Stability During Irradiation. New York: Metallurgical Society of American Institute of Mining, Metallurgical and Petroleum Engineers, 1981: 619 [2] Nolfi F V. Phase Transformations During Irradiation. New York: Applied Science Publishers, 1983 [3] Maziasz P J, McHargue C J. Int Mater Rev, 1987; 32: 190 [4] Jia C C, Lu L, Sun J Y, Hu B F. Trans Met Heat Treat, 2000; 21(1): 12 (贾成厂,鹿 林,孙静远,胡本芙.金属热处理学报, 2000; 21(1):12 [5] Hu B F, Lu L, Sun J Y, Jia C C. Trans Met Heat Treat, 2000; 21(3): 22 (胡本芙,鹿 林,孙静远,贾成厂.金属热处理学报, 2000; 21(3):22 [6] Kato T, Takahashi H, Izumiya M. J Nucl Mater, 1992; 189: 167 [7] Dawson W M, Sale F R. Metall Trans, 1980; 11 A: 1849 [8] Pan J D, Ballufi R W. Acata Metall, 1982; 30: 861 [9] Ashworth M A, Norris D I R, Jones I P. J Nucl Mater, 1992; 189: 289 [10] Nakata K, Katano Y, Masaoka I, Shiraishi K. J Nucl Mater, 1985; 133-134: 575 [11] Okamoto P R, Rehn L E. J Nucl Mater, 1979; 83: 2 [12] Chen F S, Dixit G, Aldykiewicz A J Jr, King A H. Metall Trans, 1990; 21A: 2363 [13] Rabkin E I. Scr Metall Mater, 1994; 30: 1043 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|