Diffusion-induced Stresses
Cite this article: 

. Diffusion-induced Stresses. Acta Metall Sin, 2006, 42(3): 225-233 .

Download:  PDF(418KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Recent experiments indicate that stresses induced by atomic interdiffusion in solids can not only result in the macro-distortion of materials, but also form some peculiar micro-structures in the materials. Considered that little has been known in a detailed way of the mechanisms of diffusion-induced stresses, the relationship of atomic diffusion and stresses in solids will be elucidated and the concepts of creep-induced diffusion and diffusion-induced stresses are clarified in this paper. Based on the volume growth rate of a flow point, an equation is obtained for the relationship of stresses of flow point and atomic diffusion fluxes and therefore a general theory is constructed to describe the phenomena of diffusion-induced stresses and strains, e.g. the bending of thin diffusion couples and the periodic layer formation during solid state reactions.
Key words:  diffusion couple      interdiffusion growth      periodic-layered structure      diffusion-induced stresses      
Received:  07 June 2005     
ZTFLH:  TG111.6  
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2006/V42/I3/225

[1] Chen Y C, Zhang Y G, Chen C Q. Mater Sci Eng, 2004; A368: 1
[2] Daruka I, Szabo I A, Beke D L, Cserhati Cs, Kodentsov A, van Loo F J J. Acta Mater, 1996; 44: 4981
[3] Szabo I A, Daruka I, Beke D L. Defect Diffus Forum, 1996; 129/130: 127
[4] Greer A L, Karpe N, Bottinger J. J Alloys Compd, 1993; 194: 199
[5] Bastin G F, Rieck G D. Metall Trans, 1974; 5: 1817
[6] Osinski K, Vriend A W, Bastin G F, van Loo F J J. Z Metallkd, 1982; 73: 258
[7] Kodentsov A A, Rijnders M R, van Loo F J J. Acta Mater, 1998; 46: 6521
[8] Philibert J. Defect Diffus Forum, 1996; 129/130: 3
[9] d'Heurle F M, Gas P, Philibert J, Zhang S L. Defect Diffus Forum, 2001; 194/199: 1631
[10] Xia S W. Active Energy and Its Calculation. Beijing: Higher Education Press, 1993 (夏少武.活化能及其计算.北京:高等教育出版社, 1993)
[11] Mehrer H. Defect Diffus Forum, 1996; 129/130: 57
[12] Lin D L. Crystal Defects. Shanghai: Shanghai Jiaotong University Press, 1996 (林栋梁.晶体缺陷.上海:上海交通大学出版社, 1996)
[13] Huang J H. Diffusion in Metals and Alloys. Beijing: Metallurgical Industry Press, 1996 (黄继华.金属及合金中的扩散.北京:冶金工业出版社,1996)
[14] Kraftmakher Y. Defect Diffus Forum, 2001; 194/199: 23
[15] Gutmann A M, Translated by Jin S. Mechanical Chem- istry and Corrosion Protection of Metals. Beijing: Science Press, 1989 (Gutmann A M著,金 石译.金属力学化学与腐蚀防护.北 京:科学出版社,1989)
[16] Oikawa H, Landon T G. In: Evans R W, Wilshire B, eds., Creep of Metals and Alloys, London: The Institute of Metals, 1985
[17] Poirier J P. Creep of Crystals. Cambridge: Cambridge University Press, 1985
[18] Oikawa H, Landon T G. In: Wilshire B, Evans R W, eds., Creep Behaviour of Crystalline Solids, Swansea: Piner- idge Press, 1985
[19] Kraftmakher Y. Phys Rep, 1998; 299: 79
[20] Yu Z H, Miao M Q, Jiang Q R, Yang P Z. Fluid Mechanics. The Revised Edition, Beijing: Meteorology Press, 1994 (余志豪,苗曼倩,蒋全荣,杨平章.流体力学.修订版,北京: 气象出版社,1994)
[21] Xu Z L. Elasticity Mechanics. Beijing: People's Education Press, 1979 (徐芝纶.弹性力学.北京:人民教育出版社, 1979)
[22] Poirier J P, translated by Wang G X. Plasticity of Crystalline Materials at High Temperatures. Taibei: Quanhua Science Book Company, 1978 (Poirier J P著,王恭心编译.晶体高温塑性学.台北:全华科 技图书股份有限公司, 1978)
[23] Rapp R A, Ezis A, Yurek G J. Metall Trans, 1973; 4: 1283
[24] Markovski S L, van Dal M J H, Verbeek M J L, Kodentsov A A, van Loo F J J. J Phase Equilib, 1999; 20: 373
[25] Chen Y C, Qi L, Zhang Y G, Chen C Q. Ada Metall Sin, 2005; 41: 235 (陈永翀,其鲁,张永刚,陈昌麒.金属学报,2005;41:235)
[26] Rijnders M R, Kodentsov A A, Cserhati Cs, van den Akker J, van Loo F J J. Defect Diffus Forum, 1996; 129/130: 253
[27] Liu H W. Materials Mechanics. 3rd Ed., Beijing: Higher Education Press, 1992 (刘鸿文.材料力学.第3版,北京:高等教育出版社,1992)
[28] Chen Y C, Zhang Y G, Chen C Q. Mater Sci Eng, 2004; A362: 135
[29] Greer A L. Defect Diffus Forum, 1996; 129/130: 339
[30] Kodentsov A A, van Dal M J H, Cserhati Cs, Gusak A M, van Loo F J J. Defect Diffus Forum, 2001; 194/199: 1491
[1] Chengsong LIU,Fei YE. Mechanism on Modification of MnO-SiO2-Type Oxide by Interfacial Solid-State Reaction During Heat Treatment[J]. 金属学报, 2017, 53(1): 10-18.
[2] Yu GONG, Yongchong CHEN, Dandan LIU, Yanping ZHANG, Csaba CSERHáTI, Attila CSIK. INVESTIGATION OF PERIODIC-LAYERED STRUCTURE DURING SOLID STATE REACTIONS OF Zn/CuxTiy SYSTEMS[J]. 金属学报, 2016, 52(3): 349-354.
[3] WU Changjun, ZHU Chenlu, SU Xuping, LIU Ya, PENG Haoping, WANG Jianhua. THERMODYNAMICAL AND KINETIC INVESTIGA-TION OF FORMATION OF PERIODIC LAYERED STRUCTURE IN TiCu/Zn INTERFACE REACTION[J]. 金属学报, 2014, 50(8): 930-936.
[4] FU Xiaoliang; LI Changrong; LI Mei; ZHANG Weijing. Determination of the Phase Equilibrium of the Ag-Ti Binary System at 980, 1100 and 1200℃[J]. 金属学报, 2005, 41(7): 691-694 .
[5] CHEN Yongchong; QI Lu; ZHANG Yonggang; CHEN Changqi. The analysis of periodic layer formation during solid state reactions[J]. 金属学报, 2005, 41(3): 235-241 .
[6] DING Jinjun;ZHAO Gang;HAO Shiming (Department of Materials Science and Engineering; School of Materials and Metallurgy; Northeastern University;Shenyang 110006). PHASE EQUILIBRIUM RELATIONSHIPS OF α_2(α)/γ IN THE Ti-Al-Cr TERNARY SYSTEM[J]. 金属学报, 1998, 34(2): 171-175.
[7] LIU Xingjun; HAO Shiming; SUN Rongyao; (Northeast University of Technology; Shenyang). ISOTHERMAL SECTION AT 1000 AND 1100℃ OF Fe-Mn-AI SYSTEM PHASE DIAGRAM[J]. 金属学报, 1992, 28(7): 50-54.
[8] QIU Cai'an;JIN Zhanpeng;HUANG Peiyun Central South University of Technology; Changsha. ISOTHERMAL SECTION OF THE W-Ni-Cu SYSTEM AT 1017℃[J]. 金属学报, 1988, 24(5): 403-406.
[9] XU Leying;WANG Wenbin;ZHUANG Yuzhi Institute of Metal Research; Academia Sinica; Shenyang. DIFFUSION REACTIONS BETWEEN Cu AND NbTi[J]. 金属学报, 1988, 24(4): 335-341.
No Suggested Reading articles found!