Effects of Thermal Exposure on the Tensile and Fatigue Properties of Cast Ti—47Al—2Cr—2Nb--0.15B Alloy |
CUI Yuyou; XIANG Hongfu; JIA Qing; YANG Rui |
Institute of Metal Research; The Chinese Academy of Sciences; Shenyang 110016 |
|
Cite this article:
CUI Yuyou; XIANG Hongfu; JIA Qing; YANG Rui. Effects of Thermal Exposure on the Tensile and Fatigue Properties of Cast Ti—47Al—2Cr—2Nb--0.15B Alloy. Acta Metall Sin, 2005, 41(1): 108-.
|
Abstract The elevated temperature fatigue strength and room temperature tensile
properties and fatigue strength of cast
Ti-47Al-2Cr-2Nb-0.15B(atomic fraction, %)
alloy after thermal exposure were investigated. The microstructural
change of the bulk alloy and the microstructure of
surface layer after 650℃/100 h and 800℃/100 h
exposures were analyzed by means of XRD
and SEM. The room temperature tensile ductility and fatigue
strength decreased slowly with increasing
exposure temperature when it is below 650℃, and then
rapidly decreased above this temperature. Dependence of
fatigue strength for the unexposed alloy
with test temperature exhibits the same trend. The surface layer formed
after 650℃/100 h exposure is an oxygen-enriched layer,
while that after 800℃/100 h exposure is an oxide layer consisting of
TiO2 and Al2O3. Such a change in the nature of
the surface layer corresponds to the onset of rapid
drop in mechanical proerties and fatigue strength of
the alloy with increasing exposure
temperature.
|
Received: 11 February 2004
|
|
[1] Kim Y W. JOM, 1994; 46(7): 30 [2] Kumpfert J, Kim Y W, Dimiduk D M. Mater Sci Eng A,1995;A192-A193:465 [3] Liu C T, Maziasz P J. Intermetallics, 1998; 6: 653 [4] Dowling W E Jr, Donlon W T. Scr Metall, 1992; 27: 1163 [5] Kelly T J, Austin C M, Fink P J, Schaeffer J. Scr Metall,1994; 30: 1105 [6] Lee D S, Stucke M A, Dimiduk D M. Mater Sci Eng A,1995; A192-A193: 824 [7] Planck S K, Rosenberger A H. In: Kim Y W, Dimiduk DM, Loretto M H eds, Gamma Titanium Aluminides 1999.Warrendale (PA): TMS, 1999: 791 [8] Pather R, Mitten W A, Holdway P, Ubhi H S, Wisbey A,Brooks J W. Intermetallics, 2003; 11: 1015 [9] Huang Z W, Voice W, Bowen P. Intermetallics, 2000; 8:417 [10] Beschliesser M, Chatterjee A, Lorich A, Knabl W, KestlerH, Dehm G, Clemens H. Mater Sci Eng A, 2002; A329-331: 124 |