Abstract Symmetrical push-pull fatigue tests were conducted on as-electrodeposited
polycrystalline copper containing a high density of twins. It was found
that twins have different effects on fatigue hardening behavior of copper
under different plastic strain amplitudes. When plastic strain amplitude
was higher than about 8.14×10 -4, twins will elevate fatigue
saturation stress and extend stress saturation plateau because of the
interactions between twin boundaries and dislocations.
[1] Burgers W G, Meijs J C, Tiedema T J. Acta Metall, 1953;1: 75 [2] Dash S, Brown N. Acta Metall, 1963; 11: 1067 [3] Meyers M A, Murr L E. Acta Metall, 1978; 26: 951 [4] Thompson A W. Metallography, 1972; 1: 366 [5] Mughrabi H. Mater Sci Eng, 1978; 33: 207 [6] Yamakov V, Wolf D, Phillpot S R, Gleiter H. Acta Mater,2002; 50: 5005 [7] Yamakov V, Wolf D, Phillpot S R, Gleiter H. Acta Mater,2003; 51: 4135 [8] Murr L E, Horylev R J, Lin W N. Philos Mag, 1970; 22:515 [9] Llanes L, Laird C. Mater Sci Eng, 1992; A157: 21 [10] Kawazoe H, Yoshida M, Basinski Z S, Niewczas M. ScrMater, 1999; 40: 639