| MEASUREMENT AND REPRESENTATION OF THE INTER--PHASE STRESS FOR DOUBLE-PHASE MATERIAL BY X-RAY METHOD |
| JIANG Chuanhai; CHENG Fanxiong; WU Jiansheng |
| Key Laboratory for High Temperature Materials and Tests of Ministry of Education; School of Materials Science and Engineering; Shanghai Jiaotong University; Shanghai 200030 |
|
Cite this article:
JIANG Chuanhai; CHENG Fanxiong; WU Jiansheng. MEASUREMENT AND REPRESENTATION OF THE INTER--PHASE STRESS FOR DOUBLE-PHASE MATERIAL BY X-RAY METHOD. Acta Metall Sin, 2004, 40(4): 351-354 .
|
|
|
Abstract Based on the theory of X--ray stress measurement, a method of measurement
and representation for the inter--phase stress of double--phase material
was established. The systematic error of the instrument has been effectively reduced by the difference between diffraction angles of two phases. The inter--phase stress of an actual material (SiCp/6061Al composites) was measured, and it was verified
that this method has a high measuring precision.
|
|
Received: 18 April 2003
|
|
|
[1] Noyan I C, Cohen J B. Residual Stress Measurement by Diffraction and Interpretation, Springer-Verlag Press, 1989: 54 [2] Zhang D Q, He J W. Residual Stress Analysis by X-ray Diffraction and Its Functions, Xi'an: Xi'an Jiaotong University Press, 1999: 3(张定铨,何家文.残余应力的X射线分析与作用,西安:西安 交通大学出版社, 1999:3) [3] Ledbetter H M, Austin M W. Mater Sci Eng, 1987; 89:53 [4] Sun Z M, Li J B, Wang Z G, Li W J. Acta Metall Mater,1992; 40(11) : 2961 [5] Sun Z M, Li J B, Wang Z G, Lu S X. Physical Testing andChemical Analysis Part A, Physical Testing, 1992; 28(2) ;38(孙正明,李家宝,王中光,吕毓雄.理化检验物理分册. 1992;28(2) :38) [6] Taya M, Arsenault R J. Metal Matrix Composites Ther-moraechanical Behavior. Pergamon Press, 1989: 23 [7] Jiang C H, Wang D Z, Yao Z K. Acta Metall Sin, 2000; 36: 555(姜传海,王德尊,姚忠凯.金属学报, 2000;36:555) [8] Jiang C H, Wang D Z, Yao C K, J Mater Sci Lett, 1999;18: 901 [9] Yang Y X, Qi X. Analysis by X-ray Diffraction, Shanghai:Shanghai Jiaotong University Press, 1994: 140(杨于兴,漆 玄. X射线衍射分析,上海:上海交通大学出版社, 1994:140) |