| CHAOTIC IDENTIFICATION OF BF IRONMAKING PROCESS I. The Calculation of Saturated Correlative Dimension |
| GAO Chuanhou; LIU Xiangguan |
| Department of Mathematics; Zhejiang University; Hangzhou 310027 |
|
Cite this article:
GAO Chuanhou; LIU Xiangguan. CHAOTIC IDENTIFICATION OF BF IRONMAKING PROCESS I. The Calculation of Saturated Correlative Dimension. Acta Metall Sin, 2004, 40(4): 347-350 .
|
|
|
Abstract As [Si] time series of No.1 BF at Laiwu Iron and Steel Group Co. and No.6 BF at Linfen Iron and Steel Group Co. to be sample space, based on phase space reconstruction technology and G--P algorithm, the saturated
correlative dimensions of chaotic attractor of Laiwu Blast Furnace Ironmaking Process and Linfen Blast Furnace Ironmaking Process are about 3.36 and 3.12, respectively. The existence of saturated correlative dimension with fraction value means there is chaos in both blast furnace ironmaking process.
|
|
Received: 02 April 2003
|
|
|
[1] Lorenz E N. J Atmospheric Sci, 1963; 20: 130 [2] Huang R S. Chaos and its Application. Hubei: Wuhan University Press, 2001: 112(黄润生.混沌及其应用.湖北:武汉大学出版社,2001:112) [3] Packard N H, Grutchfield J P, Farmer J D, Shaw R. S.Phys Rev Lett, 1980; 45(9) : 712 [4] Takens F. Lecture Notes in Mathematics, 1981; 898: 366 [5] Committee of National Natural Science Foundation of China. Automatic Science and Technology-The Research Report on Development Stratagem of Natural Science Subject. Beijing: Science Press, 1995: 132(国家自然科学基金委员会.自动化科学与技术-自然科学学科发展战略调研报告.北京:科学出版社, 1995:132) [6] Rosenstein M T, Collins J J, De Luca C J. Physica D,1994; 73(1) : 82 [7] Jang Y D, Wu Z Q, Chen Y Q, Jiang Y. J University ofScience and Technology Beijing, 2002; 24(3) : 295(江亚东,吴竹清,陈因颀,江月.北京科技大学学报,2002;24(3) :295) [8] Zhong K D, Hu G S. Digital Signal Disposal, Beijing: Ts-inghua University Press, 1988: 117(宗孔德,胡广书.数字信号处理,北京:清华大学出版社,1988:117) [9] Grassberger P, Procaccia I. Physica D, 1983; 9(3) : 189 [10] Liu X G, Liu X Z, Jiang M H, Wu X F, Chen Y M, Zhang X J, Chen T J. Metallurgical Industry Automation, 2002; 26(6) : 15(刘祥官,刘显著,蒋美华,吴晓峰,陈玉明,张晓军,陈铁军.冶金自动化,2002;26(6) :15) [11] Liu X G, Liu F. Optimization and Intelligent Control System of BF Ironmaking Process, Beijing: Metallurgy Industry Press, 2003: 51(刘祥官,刘 芳.高炉炼铁过程优化与智能控制系统,北京:冶金工业出版社,2003:51) |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|