| Transformation And Deformation Characteristics Of Ti49.4ni50.6 Superelastic Spring |
| HE Zhirong; ZHANG Yonghong;WANG Yongshan |
| State Key Laboratory for Mechanical Behavior of Materials; Xi'an Jiaotong University |
|
Cite this article:
HE Zhirong; ZHANG Yonghong; WANG Yongshan. Transformation And Deformation Characteristics Of Ti49.4ni50.6 Superelastic Spring. Acta Metall Sin, 2004, 40(1): 46-50 .
|
|
|
Abstract Effects of the annealing and deforming temperatures, thermal cycle, and the stress--strain cycle on the transformation and deformation characteristics of Ti49.4Ni50.6 superelastic (SE) coil spring have been investigated by means of differential scanning calorimetry, tensile test, and stress--strain cycling test. The phase--transformed type of the cold worked plus intermediate temperature annealed TiNi alloy is parent phase B2 rightleftharpoons R phase rightleftharpoons martensite B19'during cooling rightleftharpoons heating cycle. The martensitic transformationtemperatures increase and the R--phase transformationtemperatures decrease with increasing the annealingtemperature. The SE property can be obtained at roomtemperature for the 623---773 K annealing Ti49.4Ni50.6alloy spring, and the rigidity of the SE spring increaseswith increasing the deformed temperature. The SE propertyof Ti49.4Ni50.6alloy spring weakens while theannealed temperature is over 823 K. The smaller the takenshear strain, the higher the strain recovery rate ofTiNi SE spring is during the thermal cycle. The priorcyclic training can enhance the SE stability of TiNi
|
|
Received: 24 December 2002
|
|
|
[1] Miyazaki S, Ohmi Y, Otsuka K, Suzuki Y. J Phys Colloq, 1982; 43(C4) : 255 [2] Sehitoglu H, Jun J, Zhang X, Karaman I, Chumlyakov Y, Maier H J, Gall K. Acta Mater, 2001; 49:3609 [3] Liu Y, Galvin S P. Acta Mater, 1997; 45:4431 [4] Miyazaki S, Imai T, Igo Y, Otsuka K. Metall Trans, 1986; 17A: 115 [5] Huang X, Liu Y. Scr Mater, 2001; 45:153 [6] Vaidynathan R, Bourke M A M, Dunand D C. Metall Mater Trans, 2001; 32A: 777 [7] McKelvey A L, Ritchie R O. Metall Mater Trans, 2001; 32A: 731 [8] Todoroki T. J Jpn Inst Met, 1985; 49:439(轰恒彦.日本金属学会会志, 1985;49:439) [9] Todoroki T, Tamura H. J Jpn Inst Met, 1986; 50:538(轰恒彦,田村裕一.日本金属学会会志,1986;50:538) [10] He Z R, Zhang Y H, Xie N S, Liu C. Chin J Nonferr Met, 1998; 8 (Supp.1) : 218(贺志荣,张永宏,解念锁,刘琛.中国有色金属学报,1998;8(增刊1) :218) [11] He Z R, Zhang Y H. Trans Met Heat Treat, 1999; 20 (3) : 31(贺志荣,张永宏.金属热处理学报,1999;20(3) :31) [12] Otsuka K, Wayman C M. Shape Memory Materials. Cambridge: Cambridge University Press, 1998:49 [13] Otsuka K, Ren X. Mater Sci Eng, 1999; A273-275:89 [14] Miyazaki S, Otsuka K. Metall Trans, 1986; 17A: 53f |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|