Freestanding nanowires have ultrahigh elastic strain limits (4%~7%) and yield strengths, it is expected that composites reinforced by nanowires will have exceptional mechanical properties. However, the results obtained so far have been disappointing, primarily because the intrinsic mechanical properties of nanowires have not been successfully exploited in bulk composites. This is thought to be due to the inelastic strain incompatibilities at typical dislocation-piled-up interfaces. Therefore, we proposed a concept of elastic and transformation strain matching to realize the intrinsic mechanical properties of the nanowires. By creating a nanostructured composite consisting of nano Nb embedded in a NiTi matrix, the intrinsic mechanical properties of Nb nanowires, nano ribbons and nano particles are realized. Besides, this breakthrough triggers a new mechanism of stress coupling that induces the nanocomposite showing excellent mechanical properties. Based on the design strategy, we developed an in situ composite that possesses a large quasi-linear elastic strain of over 6%, a low Young's modulus of less than 28 GPa, and a high yield strength of 1.65 GPa.
Fig.1 Two-dimension lattice schematic of the strain match between the nanowire and the dislocation slip matrix(a) matrix before dislocation slip(b) formed Burgers step (red line) after dislocation slip(c) atomic-scale high stress concentration (dotted circle) was generated when the dislocation moves to the interface between the nanowire and the matrix(d) schematic of the strain (ε) distribution when the dislocation slips to the interface, which shows the inelastic shear strain of matrix () approaches 100% around dislocation and elastic strain of matrix () of about 0.2% away the dislocation
Fig.2 Two-dimension lattice schematic of the strain match between the nanowire and the lattice shear matrix(a) matrix before lattice shear(b) matrix after lattice shear(c) interface between the nanowire and the matrix after lattice shear, showing no atomic-scale high stress concentration(d) schematic of the strain distribution when the matrix experiences the stress induced martensitic transformation, which shows the elastic strain of matrix () of about 1% around parent and shear strain of matrix () approaches 7% around martensite. This 7% strain matches the elastic strain of the nanowire () of about 6% (red line)
Fig.3 The macro and micro images of the nanowire Nb/NiTi composite[12] (a) a coil of composite wire with a diameter of 0.5 mm (b) scanning TEM image of the cross section of composite wire (bright regions, cross sections of Nb nanowires; dark regions, NiTi matrix) (c) TEM image of a longitudinal section of composite wire (NW indicates nanowire) (d) macroscopic appearance of a bundle of freestanding Nb nanowires (e, f) SEM images of the freestanding Nb nanowires
Fig.4 The high energy synchrotron XRD of the nanowire Nb/NiTi sample during tensile test and the evolution of the lattice strain with respect to the applied strain of Nb nanowire[12](a) the diffraction peak of the Nb (220) plane perpendicular to the loading direction shifts obviously when the NiTi showing the stress induced martensitic transformation (SIMT—stress-induced martensitic transformation)(b) the diffraction peak of the Nb (220) plane perpendicular to the loading direction shifts slightly when the NiTi showing plastic deformation(c) evolution of the lattice strain with respect to the applied strain for Nb (220) planes
Fig.5 Comparison of the elastic strain limits of Nb nanowires embedded in the matrix deforming by dislocation slip (1), Nb nanowires embedded in the matrix deforming by SIMT (2), and some freestanding nanowires (3)[12]
Fig.6 Tensile stress-strain curves of the nanowire in situ composite with shape memory alloy (NICSMA) composite (εe—elastic limit, σs—yield strength, E—elastic modulus) (a), comparison of strengths and elastic strains of ceramics, metals, polymers and our composite (marked by NICSMA) (b), comparison of the yield strengths and elastic strain limits of different materials (c), comparison of the yield strengths and Young's moduli of different materials (d)[12]
Fig.7 The cyclic tensile stress-strain curve of the nanowire in situ composite with shape memory alloy sample (a), evolution of the diffraction peaks for Nb (220), B2-NiTi (211) and B19'-NiTi (001) planes perpendicular to the loading direction during loading (b), evolution of the lattice strain with respect to the applied strain for Nb (220) plane perpendicular to the loading direction during the first cycle (c), evolution of the lattice strain with respect to the applied strain for Nb (220) plane perpendicular to the loading direction during the second cycle (d)[13]
Fig.8 TEM analyses of two NiTi shape memory alloy composites with 10% and 20% volume fraction Nb nanowire[14] (a, b) SAED patterns of longitudinal view of the two samples(c, d) TEM bright field images of the two samples corresponding to Figs.8a and b(e, f) HAADF images of the two sample(g, h) HRTEM image revealing the interfaces between a Nb nanowire and NiTi matrix
Fig.9 TEM study of lattice strain matching between Nb nanowires and the NiTi matrix[15] (a) bright feld image of a microbeam fabricated by means of focus ion beam milling(b) enlarged view of a Nb nanowire in the beam(c) HRTEM image of the region marked as c in Fig.9b(d) TEM image of the microbeam upon loading to about 3.23% strain(e) enlarged TEM image of the region marked as e in Fig.9d, showing the three martensite plates (marked as M1, M2 and M3) nucleated in the NiTi matrix(f~h) HRTEM images of the regions marked as f, g and h in Fig.9e(i~l) filtered HRTEM images of the regions marked as i in Fig.9c and as j~l in Figs.9f~h
Fig.10 HRTEM image of the region covering martensite plates M1 and M3. The interplanar spacing variation was calculated at an interval of seven (110)Nb planes (a) and distribution of the lattice strain as a function of distance from the start plane (b)[15]
Fig.11 STEM images of a cross-section (a) and a longitudinal-section (b) of a ribbion Nb/NiTi composite, evolution of the d-spacing strain with respect to the applied macroscopic strain for the Nb (220) plane perpendicular to the loading direction (Inset shows the stress-strain curve of the sample at room temperature) (c)[12]
Fig.12 Evolution of d-spacing strain with respect to applied strain for the Nb (110) plane perpendicular to the wire axial direction during tensile loading (Inset is the macroscopic stress-strain curve of the NICSMA composite) (a), evolution of X-ray diffraction intensity of B19′-NiTi <001> planes versus the azimuth angle during tensile loading (b), TEM micrographs of twin morphologies of the martensitic NiTi matrix before and after a tensile deformation cycle to 8.7% (c), comparison of the elastic strain limits of Nb nanowires embedded in the matrix deforming by dislocation slip (1), Nb nanowires embedded in the matrix deforming by detwinning (2), and some freestanding nanowires (3) (d)[16]
Fig.13 The d-spacing strain with respect to applied macroscopic strain for the Nb (110) planes perpendicular to the loading direction in the NiTi-Nb composite (a), comparison of tensile stress-strain curves of the composite wire (red curve) and a commercial superelastic NiTi wire (yellow curve) (b)[17]
Fig.14 The tensile cyclic stress-strain curves of the nanostructured Nb reinforced NiTi shape memory alloy composite wire (strain: 4% and 5%); the tensile cyclic stress-strain curve of a commercial superelastic NiTi shape memory alloy wire[18]
Fig.15 Typical microstructure of the TiNi-Ti3Sn composite[19] (a) SEM backscattered electron images of the composite. The inset shows the Ti3Sn (light)-TiNi (dark) lamellar structure at high magnification (b) TEM bright-field image of the composite. The inset shows the button ingot of the composite (c) HRTEM image of the interface between TiNi and Ti3Sn (d, e) display selected-area electron diffraction patterns of the Ti3Sn and TiNi lamellae, respectively, shown in Fig.15b (f) one-dimensional high-energy X-ray diffraction (HE-XRD) pattern of the composite. The inset contains its corresponding two-dimensional HE-XRD pattern
Fig.16 Deformation behavior of the TiNi-Ti3Sn composite[19] (a) the lattice strain evolutions of B19'-TiNi (022) and Ti3Sn (201) planes perpendicular to the loading direction as a function of the applied macroscopic strain. The inset shows an enlarged view of the lattice strain curve of the TiNi in the initial stages of deformation (b) the comparison of the elastic strains of Ti3Sn achieved in our composite with different reinforcements (such as nanowires, laminates, and particles) embedded in conventional metal matrices, which are deformed by dislocation slip
Fig.17 Room-temperature compressive stress-strain curve of the composite (a), comparison of the mechanical properties of our composite with those of other high-performance metal-based lamellar composites in which the soft component is a conventional metal (without the "J-curve" deformation attributes) rather than the biopolymer-like metal ("J-curve" deformation attributes) (b)[19]
Fig.18 Two-way actuated properties of the composite wire[20] (a) output strain-temperature curve of the composite without external load (b) evolution of d-spacing strain with respect to temperature for the Nb (110) plane perpendicular to the wire axial direction
Fig.19 Evolution of high-energy X-ray diffraction peaks for Nb (110) and B19′-NiTi (001) planes through the multiple-step tensile cycles (a), evolution of d-spacing strain with respect to applied strain for the Nb (110) plane perpendicular to the wire axial direction during the multiple-step tensile cycles (b), comparison of the retained tensile and compressive elastic strains of large quantity Nb nanowires in the composite without external load and those of the reported thin films on substrates and embedded nanoinclusions in films (c)[16]
Fig.20 Polarization curves of the oxygen reduction reaction (ORR) of 10 and 5 nm Pt nanofilm under different strain states at a scan rate of 0.3 V/s. The data of 10 nm Pt nanofilm are shown with standard deviation[28]
[1]
Wong E W, Sheehan P E, Lieber C M.Nanobeam mechanics: Elasticity, strength, and toughness of nanorods and nanotubes[J]. Science, 1997, 277: 1971
Podsiadlo P, Kaushik A K, Arruda E M, et al.Ultrastrong and stiff layered polymer nanocomposites[J]. Science, 2007, 318: 80
[7]
Coleman J N, Khan U, Gun'ko Y K. Mechanical reinforcement of polymers using carbon nanotubes[J]. Adv. Mater., 2006, 18: 689
[8]
Thilly L, van Petegem S, Renault P O, et al. A new criterion for elasto-plastic transition in nanomaterials: Application to size and composite effects on Cu-Nb nanocomposite wires[J]. Acta Mater., 2009, 57: 3157
[9]
Vidal V, Thilly L, van Petegem S, et al. Plasticity of nanostructured Cu-Nb-based wires: Strengthening mechanisms revealed by in situ deformation under neutrons[J]. Scr. Mater., 2009, 60: 171
[10]
Ayd?ner C C, Brown D W, Mara N A, et al.In situ x-ray investigation of freestanding nanoscale Cu-Nb multilayers under tensile load[J]. Appl. Phys. Lett., 2009, 94: 031906
[11]
Thilly L, Renault P O, Vidal V, et al.Plasticity of multiscale nanofilamentary Cu/Nb composite wires during in situ neutron diffraction: Codeformation and size effect[J]. Appl. Phys. Lett., 2006, 88: 191906
[12]
Hao S J, Cui L S, Jiang D Q, et al.A transforming metal nanocomposite with large elastic strain, low modulus, and high strength[J]. Science, 2013, 339: 1191
[13]
Wang S, Cui L, Hao S, et al.Locality and rapidity of the ultra-large elastic deformation of Nb nanowires in a NiTi phase-transforming matrix[J]. Sci. Rep., 2014, 4: 6753
[14]
Liu Z Y.Study of structure and functional property of Nb/NiTi composite [D]. Beijing: China University of Petroleum, 2014(刘镇洋. Nb纳米线/NiTi记忆合金复合材料结构与功能特性研究 [D]. 北京: 中国石油大学(北京), 2014)
[15]
Zang K T, Mao S C, Cai J X, et al.Revealing ultralarge and localized elastic lattice strains in Nb nanowires embedded in NiTi matrix[J]. Sci. Rep., 2015, 5: 17530
[16]
Hao S J, Cui L S, Wang H, et al.Retaining large and adjustable elastic strains of kilogram-scale Nb nanowires[J]. ACS Appl. Mater. Interfaces, 2016, 8: 2917
[17]
Hao S J, Cui L S, Guo F M, et al.Achieving large linear elasticity and high strength in bulk nanocompsite via synergistic effect[J]. Sci. Rep., 2015, 5: 8892
[18]
Hao S J, Cui L S, Jiang D Q, et al.Nanostructured Nb reinforced NiTi shape memory alloy composite with high strength and narrow hysteresis[J]. Appl. Phys. Lett., 2013, 102: 231905
[19]
Zhang J S, Cui L S, Jiang D Q, et al.A biopolymer-like metal enabled hybrid material with exceptional mechanical prowess[J]. Sci. Rep., 2015, 5: 8357
[20]
Hao S J, Liu Y N, Ren Y, et al.Achieving superior two-way actuation by the stress-coupling of nanoribbons and nanocrystalline shape memory alloy[J]. ACS Appl. Mater. Interfaces, 2016, 8: 16310
[21]
Hao S J, Cui L S, Wang Y D, et al.The ultrahigh mechanical energy-absorption capability evidenced in a high-strength NbTi-NiTi nanocomposite[J]. Appl. Phys. Lett., 2011, 99: 024102
[22]
Zhang J S, Liu Y N, Ren Y, et al.In situ synchrotron X-ray diffraction study of deformation behavior and load transfer in a Ti2Ni-NiTi composite[J]. Appl. Phys. Lett., 2014, 105: 041910
[23]
Jiang D Q, Hao S J, Zhang J S, et al. In situ synchrotron investigation of the deformation behavior of nanolamellar Ti5Si3-TiNi composite [J]. Scr. Mater., 2014, 78-79: 53
[24]
Zhang J S, Liu Y N, Huan Y, et al.High damping NiTi-Ti3Sn in situ composite with transformation-mediated plasticity[J]. Mater. Des., 2014, 63: 460
[25]
Shao Y, Guo F M, Huan Y, et al.Fabrication, microstructure and mechanical properties of W-NiTi composites[J]. J Alloys Compd., 2017, 695: 1976
[26]
Shao Y, Guo F M, Ren Y, et al.Tensile properties of a novel W-NiTi heavy alloy with transforming matrix[J]. Mater. Sci. Eng., 2017, A683: 103
[27]
Shao Y, Yu K Y, Jiang D Q, et al.High strength W/TiNi micro-laminated composite with transformation-mediated ductility[J]. Mater. Des., 2016, 106: 415
[28]
Du M S, Cui L S, Cao Y, et al.Mechanoelectrochemical catalysis of the effect of elastic strain on a platinum nanofilm for the ORR exerted by a shape memory alloy substrate[J]. J. Am. Chem. Soc., 2015, 137: 7397
[29]
Feng C, Zhao J C, Yang F, et al.Nonvolatile modulation of electronic structure and correlative magnetism of L10-FePt films using significant strain induced by shape memory substrates[J]. Sci. Rep., 2016, 6: 20199
[30]
Feng C, Zhao J C, Yang F, et al.Reversible and nonvolatile modulations of magnetization switching characteristic and domain configuration in L10-FePt films via nonelectrically controlled strain engineering[J]. ACS Appl. Mater. Interfaces, 2016, 8: 7545
[31]
Du M S, Wan Q, Wang Z Q, et al.Elastic strain induced improvement in the photocatalytic activity of semiconducting film exerted by the surface relief of Fe-Ni-Co-Ti alloy substrate[J]. Mater. Lett., 2016, 168: 192
[32]
Du M S, Cui L S, Wan Q.Tensile strain induced narrowed bandgap of TiO2 films: Utilizing the two-way shape memory effect of TiNiNb substrate and in-situ mechanical bending[J]. Mater. Sci. Eng., 2016, B207: 7
[33]
Du M S, Wan Q, Wang Z Q, et al.Elastic strain effects on the photocatalytic TiO2 nanofilm: Utilizing the martensitic surface relief of FeNiCoTi alloy substrate[J]. Chem. Phys. Lett., 2016, 658: 130